全部 标题 作者
关键词 摘要

OALib Journal期刊
ISSN: 2333-9721
费用:99美元

查看量下载量

相关文章

更多...

Crystallographic Polymorphs Changes of the Yttria Stabilized Zirconia under Humidity

DOI: 10.4236/jmmce.2026.146010, PP. 135-144

Keywords: Yttria-Stabilized Zirconia, Abradable Coating, Hydrothermal Aging, Phase Transformation, Rietveld Refinement

Full-Text   Cite this paper   Add to My Lib

Abstract:

One of the major sources of efficiency loss in gas turbine engines is the leakage of high-pressure gases through the clearance between rotating blade tips and the stationary shroud. To minimize this leakage in the high-temperature turbine section, yttria-stabilized zirconia (YSZ)-based abradable coatings are commonly applied by plasma spraying. These coatings provide a self-adjusting sealing system that enables minimal tip clearance during engine operation. In this study, a commercial YSZ-based abradable coating (Metco 2460NS) was exposed to a humid environment at 60?C for 85 weeks, after which a decrease in hardness was observed. The phase composition before and after exposure was characterized by X-ray diffraction (XRD) coupled with Rietveld refinement. The results revealed significant phase evolution during aging, accompanied by a progressive reduction in mechanical bond strength. The observed mechanical performance degradation was associated with phase transformations within the YSZ coating. The stabilization of zirconia by yttrium is primarily attributed to the formation of oxygen vacancies in the crystal lattice. Prolonged exposure to moisture may alter the defect chemistry and promote local yttrium redistribution or depletion, thereby destabilizing the cubic and tetragonal phases and mainly, increasing the fraction of the monoclinic phase. The associated volume expansion of the monoclinic phase can generate localized stresses and microcracking, ultimately compromising coating integrity. These findings suggest that prolonged hydrothermal exposure promotes phase destabilization and contributes to the deterioration of the mechanical performance of YSZ-based abradable coatings.

References

[1]  Davenport, J.R., Mendez-Garcia, L., Purkayastha, S., Hancock, M.E., Stearn, R.J. and Clegg, W.J. (2014) Material Needs for Turbine Sealing at High Temperature. Materials Science and Technology, 30, 1877-1883.
https://doi.org/10.1179/1743284714y.0000000527
[2]  Witz, G., Shklover, V., Steurer, W., Bachegowda, S. and Bossmann, H. (2007) Phase Evolution in Yttria-Stabilized Zirconia Thermal Barrier Coatings Studied by Rietveld Refinement of X-Ray Powder Diffraction Patterns. Journal of the American Ceramic Society, 90, 2935-2940.
https://doi.org/10.1111/j.1551-2916.2007.01785.x
[3]  Zhao, M., Zhang, L.X. and Pan, W. (2012) Properties of Yttria-Stabilized-Zirconia Based Ceramic Composite Abradable Coatings. Key Engineering Materials, 512, 1551-1554.
https://doi.org/10.4028/www.scientific.net/kem.512-515.1551
[4]  Liebert, C.H., Jacobs, R.E., Stecura, S. and Morse, C.R. (1976) Durability of Zirconia Thermal Barrier Ceramic Coatings on Air-Cooled Turbine Blades in Cyclic Jet Engine Operation. Lewis Research Center, 1-16.
https://ntrs.nasa.gov/api/citations/19760025104/downloads/19760025104.pdf
[5]  Bridges, K.J.P. (2018) Degradation Mechanisms in Ceramic Abradable Coatings for Hot Section Turbine Components. UC Irvine Electronic Theses and Dissertations.
https://escholarship.org/uc/item/1366g630
[6]  Oerlikon Metco (2016) An Introduction to Thermal Spray.
https://www.oerlikon.com/ecoma/files/BRO-0005_Thermal_Spray_Brochure_EN.pdf?download=true
[7]  Toksoy, D. and ?n?ral, ?. (2024) Optical Behavior of Zirconia Generations. Cyprus Journal of Medical Sciences, 9, 380-389.
https://doi.org/10.4274/cjms.2024.2024-29
[8]  Rietveld, H.M. (1969) A Profile Refinement Method for Nuclear and Magnetic Structures. Journal of Applied Crystallography, 2, 65-71.
https://doi.org/10.1107/s0021889869006558
[9]  (2017) DSMTS-0014.4—Zirconium Oxide Ceramic Abradable Powders?2017. Oerlikon Metco.
https://jya.cl/wp-content/uploads/2021/05/DSMTS-0014.4_ZrO-poly.pdf
[10]  ASTM International: C633-24 (2024) Standard Test Method for Adhesion or Cohesive Strength of Thermal Spray Coatings.
https://store.astm.org/c0633-24.html
[11]  Powder Cell for Windows (PCW).
https://powdercell-for-windows.software.informer.com/2.4/
[12]  FullProf (Winplotr).
https://fpsuite-doc.readthedocs.io/en/latest/pages/installation/installation.html
[13]  Wu, J.W., Bai, C.N., Wei, W.X., Zheng, X.D., Yan, W., Wei, G.Q., et al. (2026) Unraveling Chloride-Driven Phase-Interface Degradation in Stabilized ZrO2 under Seawater Tribocorrosion. Ceramics International, 52, 32131-32146.
https://doi.org/10.1016/j.ceramint.2026.05.255
[14]  Chevalier, J., Gremillard, L., Virkar, A.V. and Clarke, D.R. (2009) The Tetragonal‐Monoclinic Transformation in Zirconia: Lessons Learned and Future Trends. Journal of the American Ceramic Society, 92, 1901-1920.
https://doi.org/10.1111/j.1551-2916.2009.03278.x

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133