铁基非晶涂层在NaCl和H2SO4溶液中的钝化行为
DOI: 10.11900/0412.1961.2014.00272, PP. 49-56
Keywords: 非晶涂层,超音速火焰喷涂,钝化,电化学腐蚀
Abstract:
采用超音速火焰喷涂(HVOF)方法制备了一种FeCrMoMnWBCSi非晶态合金涂层,测试并分析了非晶涂层组织、钝化膜成分及涂层在不同浓度NaCl和H2SO4介质中的钝化行为,并与304不锈钢和ND钢进行对比.结果表明,非晶涂层由于钝化膜中高含量的Cr,Mo及W的氧化物,钝化区间宽,抗钝化膜破裂能力强,孔隙的存在降低其均匀腐蚀抗力.304不锈钢钝化膜破裂电位较低且与NaCl溶液浓度密切相关.304不锈钢和ND钢只有在浓H2SO4溶液中具有较稳定的钝化特征,非晶结构有助于涂层在稀H2SO4溶液中形成更加稳定的钝化膜,厚度较小的涂层(200μm)具有较高的非晶相含量,形成的钝化膜较厚,耐蚀性更加优异.
References
| [1] | Hashimoto K. Corrosion, 2002; 58: 715
|
| [2] | Inoue A, Shinohara Y, Gook J S. Mater Trans JIM, 1995; 36: 1427
|
| [3] | Branagan D J, Swank W D, Haggard D C, Fincke J R. Metall Mater Trans, 2001; 32A: 2615
|
| [4] | Wang Y, Zheng Y G, Ke W, Sun W H, Wang J Q. Mater Corros, 2012; 63: 685
|
| [5] | Liu D Y, Wang C, Zhang H F, Hu Z Q. Acta Metall Sin, 2005; 41: 209 (刘冬艳, 王 成, 张海峰, 胡壮麒. 金属学报, 2005; 41: 209)
|
| [6] | Wang Y, Jiang S L, Zheng Y G, Ke W, Sun W H, Wang J Q. Corros Sci, 2012; 63: 159
|
| [7] | Ni H S, Liu X H, Chang X C, Hou W L, Liu W, Wang J Q. J Alloys Compd, 2009; 46: 163
|
| [8] | Farmer J, Chol J S, Saw C, Haslam J, Day D, Hailey P, Lian T, Rebak R, Perepezko J, Payer J, Branagan D, Beardsley B, Amato A D, Aprigliano L. Metall Mater Trans, 2009; 40A: 1289
|
| [9] | Wang Y, Zheng Y G, Ke W, Sun W H, Hou W L, Chang X C, Wang J Q. Corros Sci, 2011; 53: 3177
|
| [10] | Zhang C, Liu L, Chan K C, Chen Q, Tang C Y. Intermetallics, 2012; 29: 80
|
| [11] | Wang S, Cheng J, Yi S H, Ke L. Trans Nonferrous Met Soc China, 2014; 24: 146
|
| [12] | Chen Q J, Hu L L, Zhou X L, Hua X Z. Rare Met Mater Eng, 2012; 41: 512 (陈庆军, 胡林丽, 周贤良, 华小珍. 稀有金属材料与工程, 2012; 41: 512)
|
| [13] | Wang Y, Jiang S L, Zheng Y G, Ke W, Sun W H, Wang J Q. Corros Sci, 2012; 63: 159
|
| [14] | Guo J H, Wu J W, Ni X J, Li D R, Lian F Z, Lu Z C. Acta Metall Sin, 2007; 43: 780 (郭金花, 吴嘉伟, 倪晓俊, 李德仁, 连法增, 卢志超. 金属学报, 2007; 43: 780)
|
| [15] | Pang S J, Zhang T, Asami K, Inoue A. Corros Sci, 2002; 44: 1847
|
| [16] | Wang S L, Yi S. Intermetallics, 2010; 18: 1950
|
| [17] | Liu X Q, Zheng Y G, Chang X C, Hou W L, Wang J Q, Tang Z, Burgess A. J Alloys Compd, 2009; 484: 300
|
| [18] | Wang A P, Chang X C, Hou W L, Wang J Q. Acta Metall Sin, 2006; 42: 537 (王爱萍, 常新春, 侯万良, 王建强. 金属学报, 2006; 42: 537)
|
| [19] | Cao C N, Zhang J Q. Introduction of Electrochemical Impedance Spectroscopy. Beijing: Science Press, 2002: 118 (曹楚南, 张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 118)
|
| [20] | Pardo A, Merino M C, Otero E, Lo'pez M D, M'hichet A. J Non-cryst Solids, 2006; 352: 3179
|
| [21] | Wang W H. Prog Phys, 2013; 33: 177 (汪卫华. 物理学进展, 2013; 33: 177)
|
| [22] | Scully J R, Payer J H. J Mater Res, 2008; 22: 302
|
| [23] | Wang Z M, Ma Y T, Zhang J, Hou W L, Chang X C, Wang J Q. Electrochim Acta, 2008; 54: 261
|
| [24] | Lloyd A C, Noel J J, McIntyre S, Shoesmith D W. Electrochim Acta, 2004; 49: 3015
|
| [25] | Habazaki H, Kawashima A, Asami K, Hashimoto K. J Electrochem Soc, 1991; 138: 76
|
| [26] | Maurice V, Strehblow H H, Marcus P. J Electrochem Soc, 1999; 146: 524
|
| [27] | Pedraza F, Roman E, Cristobal M J, Hierro M P, Perez F J. Thin Solid Films, 2002; 414: 231
|
Full-Text
|
|
Contact Us
service@oalib.com QQ:3279437679 
WhatsApp +8615387084133
|
|