甘肃某金矿的浮选尾矿无氰浸金试验研究
|
Abstract:
甘肃某金矿石经多级浮选后,浮选回收率仅能达到80%左右,浮选尾矿中金的含量仍达到1.0 g/t~1.3 g/t,通过对该浮选尾矿进行直接浸出的试验研究,对比了氰化钠与无氰浸金剂Y-CD的浸出效果,并优化了无氰浸金剂Y-CD的浸出试验条件,取得了良好的效果,提高了金的回收率。
In some gold mine in Gansu by multistage flotation, the flotation recovery rate can only reach about 80%, the content of gold flotation tailings still reached 1.0 g/t~1.3 g/t, through the experimental study on the direct leaching of flotation tailings, the leaching effect was compared with sodium cyanide free non-cyanide leaching agent Y-CD, and the optimal conditions of leaching of non non-cyanide leaching Kim agent Y-CD, and achieved good results, improve the recovery rate of gold.
[1] | 徐天允, 徐正春. 金的氰化与冶炼[M]. 沈阳: 沈阳黄金学院, 1985. |
[2] | 黄永泉. 难浸金矿石的提金技术简介(二)——强化氰化和非氰化浸出[J]. 江西地质科技, 1995, 22(3): 141-145. |
[3] | 白成庆. 非氰浸金试剂的应用现状及发展[J]. 矿业快报, 2008(12): 12-17. |
[4] | 邱显扬, 杨永斌, 戴子林. 氰化提金工艺的新进展[J]. 矿冶工程, 1999(3): 7-9. |
[5] | 李俊萌. 难处理金矿石预处理方法研究现状及其发展趋势[J]. 稀有金属, 2003, 27(4): 478-481+490. |
[6] | 伏雪峰. 强化氰化浸出的机理探讨[J]. 有色矿山, 1995(1): 42-47. |
[7] | 孙兆学. 贵金属生产技术实用手册[M]. 北京: 冶金工业出版社, 2011: 931-954. |
[8] | 邱定蕃. 金银工业[M]. 北京: 冶金工业出版社, 1992. |
[9] | 孙戬. 金银冶金[M]. 北京: 冶金工业出版社, 1998: 350-355. |
[10] | 王丽莉. 富氧氰化浸金作用机理及应用[J]. 有色金属(选矿部分), 2000(4): 18-21. |