-  2020 

Vacuum refinning cooper blister to remove antimony

Keywords: vacuum refining, blister copper, antimony, evaporation of metals, induction vacuum furnace

Full-Text   Cite this paper   Add to My Lib

Abstract:

Sa?etak A research on kinetics of antimony evaporation from molten copper blister was made in a vacuum induction melting (VIM) furnace at temperatures of 1 473 and 1 523 K, and operating pressures of 8 - 133 Pa. The evaporation rate of Sb was found to be first order with respect to your content in the melt. The overall mass transfer coefficient of antimony evaporation from cooper blister are from 1,82×10-5 ms-1 to 3,43×10-5 ms-1 at 1 473 K (8 Pa) - 1 523 K (133 Pa)