- 2015
液浸聚光太阳电池散热光稳定剂/二甲基硅油共混物复合材料的性能
|
Abstract:
采用在二甲基硅油内添加2-羟基-4-甲氧基二苯甲酮(UV-9)和受阻胺类光稳定剂GW-783的方法制备了光稳定剂/二甲基硅油共混物复合材料, 研究了其用作聚光太阳电池散热介质的性能.通过加速寿命试验的方法, 考察了复合材料的耐候性、 黏度和光谱透过性, 确定了工作过程中光稳定剂在复合材料中的质量分数范围, 检测和分析了聚光太阳电池试验前后的性能.试验证明光稳定剂/二甲基硅油共混物复合材料能够有效抑制老化作用的影响, 且聚光太阳电池与复合材料之间不会影响彼此的特性, 这保证了聚光光伏(CPV)系统长期运行下电力输出的稳定, 其中UV-9-GW-783/二甲基硅油复合材料的性能最佳. The light stabilizer/di-methyl silicon oil blend composites were prepared by adding hydroxy-4-methoxy-benzophenone (UV-9) and a hindered amine light stabilizer named GW-783 into di-methyl silicon oil and the composites applied as heat transfer medium for concentrator solar cells were studied. By accelerated life test, the weather resistance of the composites, viscosity and spectral transmittance were investigated and the mass fraction range of light stabilizer in composites during working process were defined. And the performance of concentrator soalr cells before and after test was also detected and analyzed. The results show that the aging effect on light stabilizer/di-methyl silicon oil blend composites can be inhibited efficiently and there are no interaction between concentrator solar cells and composites. Hence, the power performance of concentrator solar cells can be kept stable when concentrating photovoltaic (CPV) system is running for a long time. The most effect composite is UV-9-GW-783/di-methyl silicon oil. 国家自然科学基金(51478297)
[1] | Zhu L, Wang Y P, Fang Z L, et al. An effective heat dissipation method for densely packed solar cells under high concentrations [J]. Solar Energy Materials and Solar Cells, 2010, 4(12): 133-140. |
[2] | Subarna M, Kairavi V, Pushpito G. Performance of a silicon photovoltaic module under enhanced illumination and selective filtration of incoming radiation with simu-ltaneous cooling[J]. Solar Energy, 2010, 84(2): 1439-1444. |
[3] | Huang W R.Silicon oil and their secondary products [M].Beijing: Chemical Industry Press, 2004: 81-82 (in Chinese). 黄文润.硅油及二次加工产品[M].北京: 化学工业出版社, 2004: 81-82. |
[4] | Richard G J, Wataru A, Julian C.Silicon containing polymers [M].Berlin: Kluwer Academic Publishers, 2010: 330-331. |
[5] | Ugumori T, Ikeya M.Efficiency increase of solar cells operated in dielectric liquid [J].Japanese Journal of Applied Physics, 1981, 20(5): 77-80. |
[6] | Xin G C, Wang Y P, Sun Y, et al. Experimental study of liquid-immersion Ⅲ-V multi-junction solar cells with di-methyl silicon oil under high concentrations [J]. Energy Conversion and Management, 2015, 2(2): 25-31. |
[7] | Kerschaver E V, Beaucarne G. Back-contact solar cells: A review[J].Progress in Photovoltaic: Research and Applications,2006, 14(2): 107-123. |
[8] | Martin A G, Keith E, Yoshihiro H, et al. Solar cell efficiency tables (version 45) [J].Progress in Photovoltaic: Researchand Applications, 2015, 19(2): 89-92. |
[9] | Shaltout M A M, El-Nicklawy M, Hassan A F, et al.The temperature dependence of the spectral and efficiency behavior of Si solar cell under low concentrator solar cell [J].Renewable Energy, 2000, 12(5): 445-448. |
[10] | Royne A, Dey C J, Mills D R.Cooling of photovoltaic cells under concentrated illumination: A critical review [J].Solar Energy Materials and Solar Cells, 2005, 4(86): 451-483. |
[11] | Liu L, Zhu L, Wang Y P, et al.Heat dissipation performance of silicon solar cells by direct dielectric liquid immersion under intensified illuminations [J]. Solar Energy, 2011, 85(3): 922-930. |
[12] | Wang Y P, Fang Z L, Zhu L, et al. The performance of silicon solar cells operated in liquids [J]. Applied Energy, 2009, 86(9): 1037-1042. |
[13] | Han X Y, Wang Y P, Zhu L, et al. Mechanism study of the electrical performance change of silicon concentrator solar cells immersed in de-ionized water [J]. Energy Conversion and Management, 2012, 12(5): 97-105. |
[14] | Han X Y, Wang Y P, Zhu L, et al.Reliability assessment of silicone coated silicon concentrator solar cells by accelerated aging tests for immersing in de-ionized water [J]. Solar Energy, 2013, 25(7): 24-31. |
[15] | Victoria M, Askins S, Sala G, et al. Durability of dielectric fluids for concentrating photovoltaic systems [J]. Solar Energy Materials and Solar Cells, 2013, 3(19): 74-80. |
[16] | Zhu L, Wang Y P, Zhang Z Y, et al.Study the wether-resistance of dimethypoly-siloxane used in liquid-immersing CPV receivers [J].Acta Energiae Solaris Sinca, 2010, 31(4): 191-196 (in Chinese). 朱丽, 王一平, 张志英, 等.二甲基硅油的耐候性研究[J]. 太阳能学报, 2010, 31(4): 191-196. |
[17] | Fang Q H, Song B, Gao Y, et al. Stress softening and dynamic properties of nano-graphite/natural rubber composites [J]. Acta Materiae Compositae Sinica, 2015, 31(6): 1446-1451 (in Chinese). 方庆红, 宋博, 高雨, 等.纳米石墨/天然橡胶复合材料的应力软化与动态性能[J]. 复合材料学报, 2015, 31(6): 1446-1451. |
[18] | Zhou Y W, Ning L P, Wang Y G, et al. Effect of xylanase solution on material properties of betula alnoides/HDPE wood plastic composites[J].Acta Materiae Compositae Sinica, 2014, 31(2): 338-342 (in Chinese). 周亚巍, 宁莉萍, 王燕高, 等. 木聚糖酶处理对西南桦木/HDPE复合材料性能的影响 [J], 复合材料学报, 2014, 31(2): 338-342. |
[19] | International Electrotechnical Commission. IEC-62108 International standard concentrator pho-tovoltaic (CPV) modules and assemblies design qualification and type approval [S]. Hong Kong, China: Hong Kong Polytechnic Universi-ty, 2007. |
[20] | Shin-Etsu Silicone Company. Silicone fluid KF-96 performance test results[EB/OL]. (2008-02-12) [2014-12-29].http://www.silicone.jp/. |
[21] | Yachigo S. Synergistic and stabilization of polymers: Handbook of polymer degradation [M]. New York: Dekker, 1992: 305-306. |
[22] | Victoria M, Domingguez C. High concentrator CPV module based on a single reflective stage immersed in an optical fluid[J]. Progress in Photovoltaics, 2014, 5(13): 121-129. |
[23] | Zhao Z J. Performance study of linear liquid-immersed solar receiver in medium CPV systems [D].Tianjin: Tianjin University, 2011 (in Chinese). 赵正简. 中倍聚光条件下线性液浸接收器的性能研究[D].天津: 天津大学, 2011. |
[24] | Yang K, Zuo C.A novel multi-layer manifold microchannel cooling system for concentrating photovoltaic cells [J]. Energy Conversion and Management, 2015, 89(4): 214-221. |