核技术  2015 

轧制钨板在氦源高热流作用下的形貌演化

DOI: 10.11889/j.0253-3219.2015.hjs.38.070604, PP. 70604-70604

Keywords: ,,高热流,表面形貌演化

Full-Text   Cite this paper   Add to My Lib

Abstract:

为研究轧制钨在氦粒子流与高热流协同作用下的表面形貌演化过程,利用德国马普等离子体物理研究所的GLADIS设备对轧制钨板进行了氦源高热流加载实验。结果表明,样品温度对损伤形貌影响显著:低温加载时逐渐发生表面起泡及气泡破裂,且较大尺寸气泡集中分布在近取向区域;高温加载时观察到多孔/珊瑚状结构;中温加载时则呈现出两种损伤形貌的混合。研究认为,表面损伤形貌的形成由表面起泡和珊瑚状结构演化两个过程共同控制。样品温度影响氦在钨中的扩散,从而影响两者的相对强弱,得到不同的损伤形貌。研究发现,辐照剂量的增加也会使得损伤形貌最终向多孔/珊瑚状结构转化。

References

[1]  Kaminsky M, Das S K. Kaminsky M, Das S K. Radiation blistering: recent developments[A]. In: IX Summer School and Symposium on the Physics of Ionzed Gases, Dubrovnik, Yugoslavia, 1978.
[2]  Greuner H, Maier H, Balden M, et al. Investigation of W components exposed to high thermal and high H/He fluxes[J]. Journal of Nuclear Materials, 2011, 417(1-3): 495-498
[3]  Li C, Greuner H, Yuan Y, et al. Effects of temperature on surface modification of W exposed to He particles[J]. Journal of Nuclear Materials, 2014, 455(1-3): 201-206
[4]  Greuner H, Boeswirth B, Boscary J, et al. High heat flux facility GLADIS[J]. Journal of Nuclear Materials, 2007, 367-370: 1444-1448
[5]  Berger M J. Stopping-power and range tables for electrons, protons, and helium ions [DB/OL]. :
[6]  Yuan Y, Greuner H, B?swirth B, et al. Melt layer erosion of pure and lanthanum doped tungsten under VDE-like high heat flux loads[J]. Journal of Nuclear Materials, 2013, 438: S229-S232
[7]  陆建, 倪晓武, 贺安之. 激光与材料相互作用物理学[M]. 北京: 机械工业出版社, 1996
[8]  LU Jian, NI Xiaowu, HE Anzhi. Reciprocity between laser and material physics[M]. Beijing: China Machine Press, 1996
[9]  Kaplan A F H. Local absorptivity modulation of a 1μm-laser beam through surface waviness[J]. Applied Surface Science, 2012, 258(24): 9732-9736
[10]  Ongena J, Van Oost G. Energy for future centuries: prospects for fusion power as a future energy source[J]. Fusion Science and Technology, 2010, 57(2T): 3-15
[11]  Pironti A, Walker M. Fusion, tokamaks and plasma control: an introduction and tutorial[J]. Control Systems, IEEE, 2005, 25(5): 30-43
[12]  Pintsuk G. Tungsten as a plasma-facing material[A]. In: Konings R J M. Comprehensive nuclear materials[M]. Oxford: Elsevier Ltd, 2012: 551-581
[13]  Hirai T, Escourbiac F, Carpentier-Chouchana S, et al. ITER full tungsten divertor qualification program and progress[J]. Physica Scripta, 2014, T159: 014006
[14]  Zhou Z B, Yao D M, Cao L, et al. Engineering Studies on the EAST Tungsten Divertor[J]. Plasma Science, IEEE Transactions on, 2014, 42(3): 580-584
[15]  Tokunaga K, Tamura S, Yoshida N, et al. Synergistic effects of high heat loading and helium irradiation of tungsten[J]. Journal of Nuclear Materials, 2004, 329-333: 757-760
[16]  Becquart C S, Domain C. Migration energy of He in W revisited by Ab initio calculations[J]. Physical Review Letters, 2006, 97(19): 196402