Dupel P, Bourratx, Pailler R. Structure of pyrocarbon infiltrated by pulse-CVI [J].Carbon, 1995, 33(9):1193-1204.
[2]
Spotz M S, Skamser D J, Johnson D L, et al. Thermal-stability of ceramic materials in microwave-heating[J]. J Am Ceram Soc, 1995, 78(4):1041-1048.
[3]
Lachter A, Trinquecoste M, Delhaes P, et al. Fabrication of carbon/carbon composites by d.c. plasma enhanced CVD of carbon [J].Carbon, 1985, 23(1):111-116.
[4]
Xiao P, Xu Y, Zhang L, et al. New technology for fabrication of C/SiC composites reinforced by continuous carbon tows [J].Mater Sci &Tech, 2001, 17(8):1012-1017.
[5]
Li R Z, Su J M, Cui H, et al. Exploratory applied research of polyaryacetylene on C/C material [A].Int Conf on Carbon[C].2002.60-61.
[6]
Pierson H O, Lieberman M L. The chemical vapor deposition of carbon on carbon fibers [J].Carbon, 1975, 13(3):159-166.
[7]
Pierson Hugh O, Northrop David A. J Compo Mat, 1975,(4):118-137.
[8]
Girard H. The preparation and properties of high density carbon carbon composites [A].Proceeding of the fifth London interna tional carbon and graphite conference [C].1978:483.