材料工程  2011 

2A50锻铝三点弯曲试验与高分辨率CT成像分析

, PP. 13-16

Keywords: 疲劳裂纹,三点弯曲试验,高分辨率CT,可视化,危险度因子

Full-Text   Cite this paper   Add to My Lib

Abstract:

采用高频疲劳试验机对2A50锻铝缺口试样进行了三点弯曲试验,获得了含裂纹的CT检测试样。对疲劳试样进行了高分辨率CT三维重建,分析了裂纹CT图像的损伤特点;引入了参考平面,将不同层的裂纹CT图像映射到参考平面定义了截面损伤危险度因子。CT分析结果表明裂纹扩展过程中不同部位的疲劳损伤不均匀,三维可视化结果直观显示了裂纹的三维形态;截面损伤危险度因子约为0.34,缺陷面积为最严重损伤截面面积的2.1倍,截面损伤危险度因子与疲劳周次呈单调递增关系,可用于度量工件的损伤状态。

References

[1]  ZHANG H,TODA H,QU P C,et al.Three-dimensional fatigue crack growth behavior in an aluminum alloy investigated with in situ high-resolution synchrotron X-ray microtomography[J].Acta Materialia,2009,57(11):3287-3300.
[2]  MOLENT L,JONES R,BARTER S,et al.Recent developments in fatigue crack growth assessment[J].International Journal of Fatigue,2006,28(12):1759-1768.
[3]  SIEGL J,NEDBAL I,KUNZ J.Fatigue crack growth history in damage tolerance design of aircraft structures[J].International Journal of Fatigue,2009,31(6):1062-1067.
[4]  刘新灵,张卫方,陶春虎.疲劳损伤定量分析与失效评估研究进展[J].失效分析与预防,2006,1(1):35-39.
[5]  王红,左华付,何训,等.某航空发动机第三级涡轮叶片失效分析[J].失效分析与预防,2007,2(1):24-28.
[6]  张朝宗.工业CT技术与原理[M].北京:科学出版社,2009.
[7]  KHOR K H,BUFFIèRE J Y,LUDWIG W,et al.High resolution X-ray tomography of micromechanisms of fatigue crack closure[J].Scripta Materialia,2006,55(1):47-50.
[8]  FERRIé E,BUFFIèRE J Y,LUDWIG W.3D characterisation of the nucleation of a short fatigue crack at a pore in a cast Al alloy using high resolution synchrotron microtomography[J].International Journal of Fatigue,2005,27(10-12):1215-1220.
[9]  QIAN L,TODA H,UESUGI K,et al.Three-dimensional visualization of ductile fracture in an Al-Si alloy by high resolution synchrotron X-ray microtomography[J].Materials Science Engineering A,2008,483-484(15):293-296.
[10]  OHGAKI T,TODA H,S1NCLAIR I,et al.Quantitative assessment of liquid Ga penetration into an aluminium alloy by high-resolution X-ray tomography[J].Materials Science and Engineering A,2006,427(1-2):1-6.
[11]  GERMANEAU A,DOUMALIN P,DUPRé J C.Comparison between X-ray micro-computed tomography and optical scanning tomography for full 3D strain measurement by digital volume correlation[J].NDT & E International,2008,41 (6):407-415.
[12]  LIMODIN N,RéTHORé J,BUFFIèRE J Y,et al.Crack closure and stress intensity factor measurements in nodular graphite cast iron using three-dimensional correlation of laboratory X-ray microtomography images[J].Acta Materialia,2009,57 (14):4090-4101.
[13]  TODA H,YAMAMOTO S,KOBAYASHI M,et al.Direct measurement procedure for three-dimensional local crack driving force using synchrotron X-ray microtomography[J].Acta Materialia,2008,56(20):6027-6039.
[14]  LI P,LEE P D,MAIJER D M,et al.Quantification of the interaction within defect populations on fatigue behavior in an aluminum alloy[J].Acta Materialia,2009,57(12):3539-3548.
[15]  QU P,TODA H,ZHANG H,et al.Local crack driving force analysis of a fatigue crack by a microstructural tracking method[J].Scripta Materialia,2009,61(5):489-492.
[16]  段黎明,周渝庆.基于工业CT图像的材料疲劳寿命预测[J].重庆大学学报,2008,31(8):831-835.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133