LENZ J, KESSEL S. Thermal stresses in metal-ceramic specimens for the ISO crack initiation test (three-point flexure bond test) [J]. Dental Materials, 1998, 14(4): 277-280.
[3]
CASCONE P J, NABATRAN D. Determination of thermal expansion compatibility limits for porcelain-metal systems [J]. Journal of Dental Research, 1982, 61(9): 330-333.
[4]
TOPARLI M, SASAKI S. Finite element analysis of the temperature and thermal stress in a post restored tooth [J]. Journal of Oral Rehabilitation, 2003, 30(9): 921-926.
PROOS K A, SWAIN M V, IRONSIDE J, et al. Finite element analysis studies of a metal-ceramic crown on a first premolar tooth [J]. The International Journal of Prosthodontics, 2002, 15(6): 521-527.
[8]
TRIA M G, HENRIQUES G E P, NBILO M A A, et al. The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminum-vanadium alloy [J]. Dental Materials, 2003, 19(8): 790-796.
[9]
MARKLUND S, BERGMAN B, HEDLUND S O, et al. An intraindividual clinical comparison of two metal-ceramic systems: a 5-year prospective study [J]. The International Journal of Prosthodontics, 2003, 16(1): 70-73.
[10]
HUSSAINI I A, WAZZAN K A. Effect of surface treatment on bond strength of low-fusing porcelain to commercially pure titanium [J]. The Journal of Prosthetic Dentistry, 2005, 94(4): 350-356