材料工程  2013 

X80管线钢埋弧焊接头冲击韧性及其断口形貌分析

DOI: 10.3969/j.issn.1001-4381.2013.06.010, PP. 50-54

Keywords: X80管线钢,焊接接头,冲击韧性,韧脆转变温度,断口形貌

Full-Text   Cite this paper   Add to My Lib

Abstract:

对X80管线钢埋弧焊焊接接头进行了-80~20℃温度范围的夏比冲击实验。测试了其冲击吸收功和脆性断面率,用扫描电镜观察了其断口形貌,分析了焊接接头断裂形式和断口形貌,讨论了焊接接头的韧脆转变温度和冲击断裂的力学行为。结果表明,室温时断口为韧窝状分布,焊接接头的韧脆转变温度为-28℃;断口形貌由韧性断裂向脆性断裂转变,断口主要表现为解理断裂。

References

[1]  SUNG H K, SHIN S Y, CHA W, et al. Effects of acicular ferrite on charpy impact properties in heat affected zones of oxide-containing API X80 line pipe steels [J]. Materials Science and Engineering: A, 2011, 528 (9): 3350-3357.
[2]  周民, 杜林秀, 刘相华, 等. 不同温度下X100管线钢的冲击韧性[J]. 塑性工程学报, 2010, 17 (5): 108-113.ZHOU Min, DU Lin-xiu, LIU Xiang-hua, et al. Impact toughness of X100 pipeline steels at different temperature [J]. Journal of Plasticity Engineering, 2010, 17 (5): 108-113.
[3]  张小立, 庄传晶, 吉玲康, 等. 高钢级管线钢的特征参量及其与强韧性的关系[J]. 材料工程, 2006, (8): 3-7.ZHANG Xiao-li, ZHUANG Chuan-jing, JI Ling-kang, et al. Characteristic parameters of high grade pipeline steels and its relationship with toughness [J]. Journal of Materials Engineering, 2006, (8): 3-7.
[4]  衣海龙, 杜林秀, 王国栋, 等. X80管线钢的组织与性能研究[J]. 东北大学学报:自然科学版, 2008, 29 (2): 213-216. YI Hai-long, DU Lin-xiu, WANG Guo-dong, et al. Microstructure and mechanical properties of pipeline steel X80 [J]. Journal of Northeastern University:Natural Science, 2008, 29 (2): 213-216.
[5]  HWANG B, LEE S, KIM Y M, et al. Analysis of abnormal fracture occur ring during drop-weight tear test of high-toughness line-pipeline steel [J]. Materials Science and Engineering: A, 2004, 368 (1): 18-27.
[6]  YANG X B, ZHUANG Z, YOU X C, et al. Dynamic fracture study by an experiment/simulation method for rich gas transmission X80 steel pipelines [J]. Engineering Fracture Mechanics, 2008, 75 (18): 5018-5028.
[7]  KIM Y M, LIM S K, KIM N J. Effect of microstructure on the yield ratio and low temperature toughness of line pipe steels [J]. ISIJ International, 2002, 42 (12): 1571-1577.
[8]  SANG Y S, BYOUNGCHUL H, SUNGBAK L, et al. Correlation of microstructure and charpy impact properties in API X70 and X80 pipeline steels [J]. Materials Science and Engineering: A, 2007, 458 (1): 281-289.
[9]  胥聪敏. X80钢在霍尔果斯水饱和土壤中的短期腐蚀行为研究[J]. 材料工程, 2011, (3): 78-81.XU Cong-min. Study on short-term corrosion behavior of X80 pipeline steel in Huo’erguosi soil with saturated water [J]. Journal of Materials Engineering, 2011, (3): 78-81.
[10]  SANTOS T F A, HERMENEGILDO T F C, AFONSO C R M, et al. Fracture toughness of ISO 3183 X80M (API 5L X80) steel friction stir welds [J]. Engineering Fracture Mechanics, 2010, 77 (15): 2937-2945.
[11]  李红英, 魏冬冬, 林 武, 等. X80管线钢冲击韧性研究[J]. 材料热处理学报, 2010, 31 (11): 73-78. LI Hong-ying, WEI Dong-dong, LIN Wu, et al. Research on impact toughness of X80 pipeline steel [J]. Transactions of Materials and Heat Treatment, 2010, 31 (11): 73-78.
[12]  张莉莉, 张骁勇, 高惠临, 等. 一种高铌X80管线钢的组织性能分析[J]. 材料工程, 2009, (5): 1-5. ZHANG Li-li, ZHANG Xiao-yong, GAO Hui-lin, et al. Microstructure and mechanical properties of a high Nb-microalloyed X80 pipeline steel [J]. Journal of Materials Engineering, 2009, (5): 1-5.