材料工程  2013 

义齿树脂基托表面有机-无机杂化膜的制备与研究

DOI: 10.3969/j.issn.1001-4381.2013.10.012, PP. 71-75

Keywords: 杂化膜,义齿树脂基托,吸水性,溶解性,光泽度

Full-Text   Cite this paper   Add to My Lib

Abstract:

本研究设计合成应用于义齿树脂基托表面的有机-无机杂化膜。由缩水甘油醚基丙基三甲氧基硅烷(KH560)和正硅酸乙酯(TEOS)共水解缩合制得杂化硅溶胶;由甲基丙烯酸缩水甘油酯(GMA)、丙烯酸(AA)和甲基丙烯酸甲酯(MMA)三种单体共聚制得聚合物。两者利用KH560和GMA中的环氧基团进行交联,形成具有互穿网络结构的杂化膜。对膜层的硬度、附着性及抗破裂性等进行表征,并对覆膜后的基托树脂的光泽度、吸水性及溶解性进行测试。实验结果表明,杂化膜不仅具有良好的力学性能,而且提高了基托树脂的光泽度,降低了基托树脂的吸水性和溶解性,最终会提高基托综合性能。

References

[1]  RAHAL J S, MESQUITA M F, HENRIQUES G E, et al. Influence of chemical and mechanical polishing on water sorption and solubility of denture base acrylic resins[J]. Braz Dent J, 2004, 15(3):225—230.
[2]  QUIRYNEN M, BOLLEN C M. The influence of surface roughness and surface-free energy on surpra and subgingival plaque formation in man. A review of theliterature[J]. J Clin Periodontol, 1995, 22(1):1—14.
[3]  CURTIS A R, SHORTALL A C, MARQUIS P M, et al. Water uptake and strength characteristics of a nanofilled resin based composite[J]. J Dent, 2008, 36(3):186—193.
[4]  FERRACANE J L. Hygroscopic and hydrolytic effects indental polymer networks[J]. Dent Mater, 2006, 22(3):211—222.
[5]  张利军, 肇研, 罗云烽, 等. 湿热循环对CCF300/QY8911复合材料界面性能的影响[J]. 材料工程, 2012, (2):25-29.ZHANG Li-jun, ZHAO Yan, LUO Yun-feng, et al.On the inter facial properties of CCF300/QT 8911 composite with cyclical hygrothermal treatments[J].Journal of Materials Engineering, 2012, (2):25-29.
[6]  CHAVES C A, MACHADO A L, VERGANI C E, et al. Cytotoxicity of denture base and hard chairside reline materials:a systematic review[J]. J Prosthet Dent, 2012, 107(2):114—127.
[7]  LOPES L G, DA VEIGA J F A, DE SOUZA J B, et al. Influence of pulse-delay curing on sorption and solubility of a composite resin[J]. J Appl Oral Sci, 2009, 17(1):27—31.
[8]  RüTTERMANN S, DLUZHEVSKAYA I, GROSSSTEINBECK C, et al. Impact of replacing Bis-GMA and TEGDMA by other commercially available monomers on the properties of resin-based composites[J]. Dent Mater, 2010, 26(4):353—359.
[9]  POLAT T N, KARACAER O, TEZVERGIL A, et al. Water sorption, solubility and dimensional changes of denture base polymers reinforced with short glass fibers[J]. J Biomater Appl, 2003, 17(4):321—335.
[10]  ARIMA T, MURATA H, HAMADA T. The effect of cross-linking agents on the water sorption and solubility characteristics of denture base resin[J]. J Oral Rehabil, 1996, 23(7):476—480.
[11]  王潇婕, 张玉梅, 孙延, 等. 添加纳米二氧化钛的树脂基托性能测试[J]. 牙体牙髓牙周病学杂志, 2007, 17(4):192—194.WANG Xiao-jie, ZHANG Yu-mei, SUN Yan, et al.Test of function of resin base with added nanometer titania[J].Chinese Journal of Conservative Dentistry, 2007, 17(4):192-194.
[12]  尤宏, 刘琰, 孙德智, 等. LY12 铝合金表面有机-无机杂化膜的防腐性能研究[J]. 材料工程, 2004, (6):7—11.YOU Hong, LIU Yan, SUN De-zhi, et al.Study on corrosion resitance properties of organic-inorganic hybrid coatings on LY12 aluminum alloy[J].Journal of Materials Engineering, 2004, (6):7-11.
[13]  MORALESACOSTA M D, ALVARADO BELTRáN C G, QUEVEDOLóPEZB M A, et al. Adjustable structural, optical and dielectric characteristics in sol-gel PMMA-SiO2 hybrid films[J]. J Non-cryst Solids, 2013, 362:124—135.
[14]  宋东升, 杜启云, 王薇. 有机-无机杂化膜的研究进展[J]. 高分子通报, 2010, (3):12—15. SONG Dong-sheng, DU Qi-yun, WANG Wei.Advances in organic-inorganic hybrid membranes[J].Chinese Polymer Bulletin, 2010, (3):12-15.
[15]  GB/T6739—86, 涂膜硬度铅笔测定法[S].
[16]  ISO2409—2007, 色漆和清漆—划格试验[S].
[17]  沙鹏宇. 亲水性防雾耐磨杂化涂料的设计、制备与性能研究. 长春:吉林大学, 2008.
[18]  YY0270—2003, 牙科学——义齿基托聚合物[S].
[19]  PARK S H, NOH B D, AHN H J, et al. Celluloid strip-finished versus polished composite surface:difference in surface discoloration in microhybrid composites[J]. J Oral Rehabil, 2004, 31(1):62—66.
[20]  刘翠娟. 义齿树脂基托表面粗糙度与细菌黏附和色素沉着关系的研究. 天津:天津医科大学, 2012.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133