材料工程  2015 

球磨制备轴承珠表面自润滑涂层及其摩擦性能

DOI: 10.11868/j.issn.1001-4381.2015.09.004, PP. 19-24

Keywords: 轴承珠,二硫化钼,行星式球磨,摩擦

Full-Text   Cite this paper   Add to My Lib

Abstract:

通过将MoS2粉末和轴承珠放入真空球磨罐中进行球磨的方法在轴承珠表面制备自润滑涂层。固定球磨转速为200r/min,研究不同球磨时间对轴承珠表面制备涂层的影响。采用配有能谱的扫描电子显微镜对球磨不同时间所制备涂层的形貌及元素分布进行观察。结果表明随球磨时间的延长,涂层表面形貌变化不大,涂层厚度先增加后减小,Mo的分布先均匀后分散,球磨5h后涂层的厚度及元素的均匀性最佳。制备涂层的摩擦测试结果表明球磨1h和5h所制备的涂层具有明显的润滑效果,而球磨10h的润滑效果不明显。球磨5h所制备的涂层具有最佳的润滑效果。

References

[1]  CAO Y X, DU L Z, HUANG C B, et al.Wear behavior of sintered hexagonal boron nitride under atmosphere and water vapor ambiences[J]. Applied Surface Science, 2011, 257(23): 10195-10200.
[2]  ZHU S Y, BI Q L, YANG J, et al. Influence of Cr content on tribological properties of Ni3Al matrix high temperature self-lubricating composites[J]. Tribology International, 2011, 44(10): 1182-1187.
[3]  潘国梁, 乔红斌, 郭强. 复合型固体润滑膜的滚动/滑动复合干磨损特性[J]. 哈尔滨工业大学学报, 2006, 38(增刊): 298-302. PAN Guo-liang, QIAO Hong-bin, GUO Qiang. Dry rolling/sliding wear characteristics of solid lubricating composite films[J]. Journal of Harbin Institute of Technology,2006,38(Suppl):298-302.
[4]  乔红斌, 郭强, 潘国梁,等. 粉末涂料固体润滑膜滚动/滑动复合干摩擦磨损特性研究[J]. 润滑与密封, 2006,(3): 47-49. QIAO Hong-bin, GUO Qiang, PAN Guo-liang,et al. Friction and wear characteristics of the polymer powder coatings for solid lubrication under the dry rolling/sliding condition[J]. Lubrication Engineering, 2006,(3): 47-49.
[5]  陈建敏,冶银平,党鸿辛.粘结固体润滑膜及其应用[J].摩擦学报,1994,14(2):180-189. CHEN Jian-min, YE Yin-ping, DANG Hong-xin. Developing situation and application of bonded solid lubricant films[J]. Tribology, 1994, 14(2): 180-189.
[6]  严晓华, 陈国需. 固体润滑技术的研究现状及展望[J]. 能源研究与信息, 2005, 21(2): 69-73. YAN Xiao-hua, CHEN Guo-xu. Current development and future prospects on solid lubricating techniques[J].Energy Research and Information, 2005, 21(2): 69-73.
[7]  罗军,王运动,蔡振兵,等.粘结MoS2固体润滑涂层的转动微动磨损特性[J].机械工程学报,2012,48(17):100-105. LUO Jun,WANG Yun-dong,CAI Zhen-bing,et al.Rotational fretting wear characteristics of bonded molybdenum disulfide solid lubrication coating[J].Journal of Mechanical Engineering,2012,48(17):100-105.
[8]  王小静,邵红红,王季.射频磁控溅射法制备MoS2/SiC双层薄膜[J].机械工程材料,2012,36(2):68-71. WANG Xiao-jing,SHAO Hong-hong,WANG Ji.MoS2/SiC double films prepared by radio frequency magnetron sputtering[J]. Materials for Mechanical Engineering,2012,36(2):68-71.
[9]  YANG J, LUO J B, PANG S Q. Effect of Ti or TiN codeposition on the performance of MoS2 based composite coatings[J]. Thin Solid Films, 2004, 461(2): 288-293.
[10]  高名传,童向阳,汪洪生.热喷涂法制备钼系涂层的研究进展[J].中国钼业,2014,38(6):41-47. GAO Ming-chuan,TONG Xiang-yang,WANG Hong-sheng.Research progress of Mo-based coatings fabricated by thermal spray technology[J].China Molybdenum Industry,2014,38(6):41-47.
[11]  WEI R H, YANG H B, DU K, et al.Preparation of type-ⅡMoS2 film by chemical bath deposition onto Si coated with electrolessly Ni[J]. Materials Science and Engineering: B, 2007, 138(3): 259-262.
[12]  SPALVINS T. Coatings for wear and lubrication[J]. Thin Solid Films,1978,53:285-300.
[13]  赵学敏,汪刘应,张虎,等.固体润滑涂层研究工艺的研究进展[J].材料导报,2013,27(22):68-71. ZHAO Xue-min,WANG Liu-ying,ZHANG Hu,et al.Research progress on the preparation of solid lubricating coatings[J].Materials Review,2013,27(22):68-71.
[14]  刘政军,冯丽峰,成明华,等.材料表面改性技术原理分析[J].现代焊接,2008,(8):21-25. LIU Zheng-jun,FENG Li-feng,CHENG Ming-hua,et al.Brief analysis of the principle of material surface modification technology[J].Modern Welding Technology,2008,(8):21-25.
[15]  YOSHIDA H,LU Y,NAKAYAMA H,et al. Fabrication of TiO2 film by mechanical coating technique and its photocatalytic activity[J]. Journal of Alloys and Compounds,2009,475(1-2):383-386.
[16]  HAO L, LU Y, SATO H, et al.Fabrication of zinc coatings on alumina balls from zinc powder by mechanical coating technique and the process analysis[J]. Powder Technology,2012,228:377-384.
[17]  HAO L, LU Y,HIROSHI A, et al.The influence of the processing parameters on the formation of iron thin films on alumina balls by mechanical coating technique[J]. Journal of Materials Processing Technology,2012,212(5):1169-1176.
[18]  LU Y, YOSHIDA H, NAKAYAMA H, et al. Formation of TiO2/Ti composite photocatalyst film by 2-step mechanical coating technique[J]. Materials Science Forum,2011,675-677:1229-1232.
[19]  ROSENKRANZ S, BREITUNG-FAES S, KWADE A.Experimental investigations and modeling of the ball motion in planetary ball mills[J]. Powder Technology,2011, 212(1): 224-230.
[20]  ERDEM A S, ERGüN S L.The effect of ball size on breakage rate parameter in a pilot scale ball mill[J]. Minerals Engineering, 2009, 22(7-8): 660-664.
[21]  GU L, CAO G J, WANG L Q, et al. Synthesis and characterization of a self-lubricating film on bearing balls[J]. Advanced Materials Research, 2011,154-155: 367-370.
[22]  韦习成, 赵源. FeS层的减磨耐磨机理[J]. 润滑与密封, 1994,(2): 12-17. WEI Xi-cheng, ZHAO Yuan. Anti-friction and wear resistance mechanism of FeS layer[J]. Lubrication Engineering, 1994,(2): 12-17.
[23]  赵军军, 张平, 韩文政. 离子渗硫技术在装甲车辆中的应用[J]. 装甲兵工程学院学报, 2003, 17(1): 10-14. ZHAO Jun-jun, ZHANG Ping, HAN Wen-zheng. The application of ion sulphidizing process to armored vehicle[J]. Journal of Armored Force Engineering Institute, 2003, 17(1): 10-14.
[24]  王海斗, 徐滨士, 刘家浚,等. 两步法制备固体润滑FeS薄膜的摩擦磨损性能研究[J].摩擦学学报, 2005, 25(4):304-306. WANG Hai-dou, XU Bin-shi, LIU Jia-jun,et al. Study on the tribological properties of FeS solid lubrication films prepared by two-step method[J]. Tribology, 2005, 25(4):304-306.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133