SMITH Y E,COLDREN A P,CRYDERMAN R.Toward improved ductility and toughness[M].Tokyo:Climax Molybdenum Company Ltd,1972.119-120.
[5]
GLOVER A G,MCGRAT H J T,WEAT HERLY G C,et al.The influence of cooling rate and composition on weld metal microstructures in a C/Mn and HSLA steel[J].Welding Journal,1977,56 (9):225-231.
[6]
方鸿生.贝氏体相变[M].北京:科学出版社,1999.71-79.
[7]
DIAZ-FUENTES M,IZA-MENDIA A,GUTIERREZ I.Analysis of different acicular ferrite microstructures in low-carbon steels by electron backscattered diffraction[J].Metallurgical and Materials Transactions A,2003,34:1043-1067.
KLAUS HULKA,PASCOAL BORDIGNON,MALCOLM GRAY.Experience with low carbon HSLA steel containing 0.06 to 0.10 percent niobium[R].German:Niobium Products Company GmbH,2003.