全部 标题 作者
关键词 摘要

OALib Journal期刊
ISSN: 2333-9721
费用:99美元

查看量下载量

相关文章

更多...
材料工程  2007 

MgF2/N2/空气气氛中密封熔炼AZ91D镁合金实验研究

Keywords: 镁合金,密封炉,MgF2,表面膜

Full-Text   Cite this paper   Add to My Lib

Abstract:

在预先装入固态MgF2的密封熔炼炉中,研究了熔炼温度和炉内空气含量对AZ91D镁合金保护效果的影响,并对表面膜形貌、成分和成分分布进行了研究。结果表明保护效果随熔炼温度和气氛中空气含量增加而逐渐变差;当气氛中空气体积分数为25%,实验温度<750℃时,AZ91D镁合金很好被保护;当熔炼温度为650℃,气氛中空气体积分数<30%时,AZ91D镁合金很好被保护。所有表面膜由MgF2和MgO组成,表面膜厚度随熔炼温度和气氛中空气含量的增加而增加,表面膜中MgF2的数量也随熔炼温度和气氛中空气含量的增加而显著增加;膜表面平整度随气氛中空气含量的增加而变差,熔炼温度增加对膜平整度影响不大。固态MgF2在熔炼温度下蒸气压较高,其蒸气与空气中氧气一起参与AZ91D镁合金表面膜的形成。

References

[1]  中国机械工程学会铸造专业学会.铸造手册:铸造非铁合金[M].北京:机械工业出版社,1993.15-35.
[2]  BLANDIN J J.Ignition resistance of various magnesium alloys[A].Magnesium Technology 2004[C].USA:TMS,2004.197-202.
[3]  ZHANG Z.Effect of inhibitor gas on mould-magnesium reactions in investment casting[A].Magnesium Technology 2004[C].USA:TMS,2004.137-142.
[4]  JOHN F,SWINTON K.Environmental challenges facing the magnesium industry-SF6 replacement[A].60th Annual World Magnesium Conference[C].Germany:International Magnesium Association,2003.10-16.
[5]  BACH F W.New protective system for magnesium casting[J].Foundry Trade Journal,2005,3622:60-62.
[6]  LYON P,ROGERS D,KING J F,et al.Magnesium melt protection at magnesium electron using HFC-134a[A].TMS Annual Meeting,Magnesium Technology[C].USA:TMS,2003.11-14.
[7]  Progress report-U S magnesium industry making strides towards climate protection goal[J].JOM,2004,11:31-35.
[8]  BARTOS S C.EPA's voluntary partnership with the magnesium industry for climate protection[A].TMS Annual Meeting[C].USA:TMS,2000.83-86.
[9]  BROCHOT.Method for protecting a nonferrous liquid metal,in particular,liquid magnesium against oxidation and ignition[P].France Patent:FR2775209,1988-06-29.
[10]  NIE Shu-hong.Effects of residual F content in a sealed melting furnace on experimental results of cover gas research for magnesium alloys[J].Material Science and Engineering A,2006,422:346-351.
[11]  NIE Shu-hong,XIONG Shou-mei.Study on the protecting effect of HFC134a on AZ91D magnesium alloy in a sealed melting furnace[A].Magnesium Technology 2006[C].USA:TMS,2006.19-24.
[12]  聂书红,熊守美.密封熔炼炉0.01%vol.HFC134a氮气中保温时间对AZ91D镁合金保护的影响[J].铸造,2006,55(2):112-115.
[13]  CASHIONS S P,RICKETTS N J,HAYES P C.The mechanism of protection of molten magnesium by cover gas mixtures containing sulphur hexafluoride[J].Journal of Light Metals,2002,2(1):43-47.
[14]  PETTERSEN G,OVRELID E,TRANELL G,et al.Characterization of the surface films formed on molten magnesium in different protective atmospheres[J].Materials Science and Engineering,2002,A332:285-294.
[15]  聂书红,熊守美,柳百成.熔态Mg在air/SF6保护气氛中形成的表面膜特征[J].材料工程,2005,(6):3-6.
[16]  聂书红,熊守美.熔态AZ91D镁合金在air/SF6保护气氛中形成的表面膜特征[J].材料保护,2005,(8):1-3.
[17]  巴林.纯物质热化学数据手册[M].北京:科学出版社,2003.1185-1896.