材料工程  2008 

铬、铝、硅对铁基高温合金抗氧化性能的影响

, PP. 73-77

Keywords: 耐热钢,铁基高温合金,氧化膜,抗氧化性

Full-Text   Cite this paper   Add to My Lib

Abstract:

采用正交设计的实验方法探讨了铬、铝、硅元素含量对铁基高温合金抗氧化性的影响规律.为获得稳定的抗氧化能力,上述各元素的含量应分别高于17%Cr,4%Al,1.5%Si.结果表明当三元素同原子比时对铁基高温合金抗氧化性的影响次序为Si最大,Al次之,Cr最小.结构平坦、组织致密、颗粒细小均匀的氧化膜抗氧化性较好,反之较差.当氧化膜由Cr2O3,Al2O3,SiO2,Fe(Ni)Cr2O4多种氧化物组成复合氧化膜时于1250℃表现为强抗氧化性,当缺少Al2O3或SiO2时表现为弱抗氧化性.

References

[1]  CHO BOKLAE,CHOI EUNSEO,CHUNG SUKMIN,et al.A novel Cr2O3 thin film on stainless steel with high sorption resistance[J].Surface Science,1999,439(1-3):L799-L802.
[2]  GREEFF A P,LOUW C W,SWART H C.The oxidation of industrial FeCrMo steel[J].Corrosion Science,2000,42:1725-1740.
[3]  刘含莲,滕新营,王执福,等.Fe-CrNi-N高温耐热钢的抗氧化性研究[J].铸造技术,2001,(6):55-57.
[4]  PEREZ F J,CRISTOBAL M J,HIERRO M P,et al.The influence of implanted silicon on the cyclic oxidation behaviour of two different stainless steels[J].Surface and Coatings Technology,1999,120-121:442-447.
[5]  HSU Hung-wen,TSAI Wen-ta.High temperature corrosion behavior of siliconized 310 stainless steel[J].Materials Chemistry and Physics,2000,64:147-155.
[6]  HUNTZ A M,BAGUE V,BEAUPLE G,et al.Effect of silicon on the oxidation resistance of 9% Cr steels[J].Applied Surface Science,2003,207:255-275.
[7]  LOUDJANI M K,PIVIN J C,HUNTZ A M,et al.High temperature corrosion of Fe-Ni-Cr,Fe-Cr-Al and Fe-Ni-Cr-Al alloys in controlled H2/H2O/CH4 atmospheres[J].Corrosion Science,1988,28:1075-1088.
[8]  PRESCOTT R.The formation of aluminium oxide scales on hightemperature alloys[J].Oxidation Metallurgy,1992,38:233-254.
[9]  WOLFF I M,IORIO L E,RUMPF T,et al.Oxidation and corrosion behaviour of Fe-Cr and Fe-Cr-Al alloys with minor alloying additions[J].Materials Science and Engineering A,1998,241:264-276.
[10]  NIU Y,WANG S,GAO F,et al.Ultra-thin aluminum oxide as a thermal oxidation barrier on metal films[J].Thin Solid Films,2002,415:219-223.
[11]  SHARAFI S,FARHANG M R.Effect of aluminizing on surface microstructure of an HH309 stainless steel[J].Surface and Coatings Technology,2006,200:5048-5051.
[12]  中国腐蚀与防护学会.金属腐蚀手册[M].上海:上海科学技术出版社,1987.22-23.