CRITCHLOW G W,BREWIS D M.Review of surface pretreatment for titanium alloys[J].Int J Adhes Adhes,1995,15;161-172.
[3]
MILLER P D,RICHARD JEFFERYS A.Method of coating titanium articles and product thereof[P].United States Patent,2,864,732,1958.
[4]
徐修成.航空用钛合金的胶接[J].粘合剂,1988,(4):32-34.
[5]
FILBEY J A,WIGHTMAN J P.Factors affecting the surability of Ti-6A1-4V/epoxy bonds[J].Adhes,1989,28(1):1-22.
[6]
YOKIMORI M,BAINBRIDGE I.Method of anodizing titanium to promote adhesion[P].United States Patent:3,959,091,1976-05-25.
[7]
焦洁清.钛合金胶接前表面制备方法初探[J].航空工艺技术,1989,22:25-28.
[8]
ZWILLING V,DARQUE-CERETTI E,BOUTRY-FORVEILLE A,et al.Structure and physicochemistry of anodic oxide films on titanium and TA6V alloy[J].Surf Interface Anal,1999,27:629 -637.
[9]
INGRAM C,RAMANI K.The effect of sodium hydroxide anodization on the durability of poly(etherketonetherketoneke-tone)adhesive bonding of titanium[J].Int J Adhesion and Adhesive,1997,17:39-45.
[10]
MATZ C.Optimization of the durability of structural titanium adhesive joints[J].Int J Adhes Adhes,1988,8(1):17-24.
[11]
王晓蔚,徐修成.钛合金胶接及表面处理[J].航空制造工程,1996,(2):17-19.
[12]
BROAD R,FRENCH,SAUER J.CLP new,effective,ecological surface pretreatment for highly durable adhesively bonded metal joints[J].Int J Adhes Adhes,1999,19(2-3):193-198.
[13]
INGRAM C,RAMANI K.The effect of sodium hydroxide anodization on the durability of poly(etherketonetherketoneketone)adhesive bonding of titanium[J].Int J Adhes Adhesives,1997,17(1):39-45.
[14]
MOLITOR P,YOUNG T.Adhesives bonding of a titanium alloyto a glass fibre reinforced composite material[J].Int J Adhes Adhes,2002,22(2):101-107.
[15]
MOLITOR P,YOUNG T.Investigations into the use of excimer laser irradiation as a titanium alloy surface treatment in a metal to composite adhesive bond[J].Int J Adhes Adhes,2003,24:127-134.
[16]
ARNOLD J R,SANDERS C D,BELLEVOU D L,et al.Proceedings of the 29th international SAMPE technical conference[C].Covina,Calif:Society for the Advancement of Material and Process Engineering,1997.345.
[17]
FILBEY J A,WIGHTMAN J P.Metal alkoxide primers in titanium/epoxy bonding[J].Adhesion,1989,28:23-39.
[18]
王晓蔚,徐修成.改善钛合金胶接表面的底胶[J].宇航材料工艺,1996,(5):11-15.
[19]
CLEARFIELD H M,COTE G O,OLVER K A,et al.Surface analysis of Ti-6A1-4V adhesive bonding systems[J].Surface and Interface Analysis,1988,(11):347-352.
[20]
NATAN M,VENABLES J D.The stability of anodized titanium surfaces in hot water[J].The Journal of Adhesion,1983,15(2):125-136.
[21]
CLEARFIELD H M,SHAFFER D K,VANDOREN S L,et al.Surface preparation of Ti-6Al-4V for high-temperature adhesive bonding[J].Adhes,1989,29(1-4):81-102.
[22]
MAHOON A.Durability of structural adhesives[M].London:Applied Science Publishers,1983.255.
[23]
MOLITOR P,BARRON V,YOUNG T.Surface treatment of titanium for adhesive bonding to polymer composites:a review[J].Int J Adhes Adhes,2001,21:129-136.
[24]
LOCKE M C,JOSEPH MARCEAN A,HARRIMAN K M.Chromic acidfluoride anodizing surface treatment for titanium[P].United States Patent.4,473,446,1984-09-25.
LEAHY W,YOUNG T,BUGGY M,et al.A study of environmentally friendly titanium pretreatments for adhesive bonding to a thermoplastic composite[J].Materialwissenschaft and Werkstofftechnik,2003,34:415-420.
[30]
RAMANI K,WILLIAM J W,KUMAR G.Silicon sputtering as a surface treatment to titanium alloy for bonding with PEKEKK[J].Int J Adhes Adhes,1998,(18):401-412.