HATTA H,GOTO K,IKEGAKI S,et al.Tensile strength and fi-ber/matrix interfacial properties of2D-and3D-carbon/carbon compos-ites[J].J Eur Ceram Soc,2005,25(4):535-542. [2]XU Y D,CHENG L F,ZHANG L T,et al.Mechanical properties of3D fiber reinforced C/SiC composites[J].Mater Sci Eng A,2001,300(1-2):196-202. [3]MURTHY P L N,NEMETH N N,BREWER D N,et al.Probabilistic analysis of a SiC/SiC ceramic matrix composite turbine vane[J].Compos B:Eng,2008,39(4):694-703. [4]GOUJARD S,VANDENBULCKE L,TAWIL H.Oxidation behavior of2D and3D carbon/carbon thermostructural materials protected by CVD polylayer coatings[J].Thin Solid Films,1994,252(2):120-130. [5]JIAO G S,LI H J,LI K Z,et al.Multi-composition oxidation resistant coating for SiC-coated carbon/carbon composites at high temperature[J].Mater Sci Eng,A,2008,486(1-2):556-561. [6]CHENG L F,XU Y D,ZHANG L T,et al.Oxidation behavior of three dimensional C/SiC composites in air and combustion gas environments[J].Carbon,2000,38(15):2103-2108. [7]WU S J,CHENG L F,ZHANG L T,et al.Comparison of oxidation behaviors of3D C/PyC/SiC and SiC/PyC/SiC composites in an O2-Ar atmosphere[J].Mater Sci Eng B,2006,130(1-3):215-219. [8]WU S J,CHENG L F,YANG W B,et al.Oxidation Protective Multi-layer CVD SiC coatings modified by a graphitic B-C interlayer for3D C/SiC composite[J].Appl Compos Mater,2006,13(6):397-406. [9]SCHULTE-FISCHEDICK J,SCHMIDT J,TAMME R,et al.Oxidation behaviour of C/C-SiC coated with SiC-B4C-SiC-cordierite oxidation protection system[J].Mater Sci Eng A,2004,386(1-2):428-434. [10]QUEMARD L,REBILLET F,GUETTE A,et al.Self-healing mecha-nisms of a SiC fiber reinforced multi-layered ceramic matrix compos-ite in high pressure steam environments[J].J Eur Ceram Soc,2007,27(4):2085-2094. [11]QUEMARD L,REBILLET F,GUETTE A,et al.Degradation mecha-nisms of a SiC fiber reinforced self-sealing matrix composite in simu-lated combustor environments[J].J Eur Ceram Soc,2007,27(1):377-388. [12]FARIZY G,CHERMANT J L,SANGLEBOEUF J C,et al.SiCf-SiBC composites:microstructural investigations of the as received material and creep tested composites under an oxidative environment[J].J Mi-crosc,2003,210(2):176-186. [13]VIRICELLE J P,GOURSAT P,BAHLOUL-HOURLIER D.Oxidation behaviour of a multi-layered ceramic-matrix composite(SiC)f/C/(SiBC)m[J].Compos Sci Technol,2001,61(4):607-614. [14]MOSS T S,LACKEY W J,MORE K L.Chemical vapor deposition of B13C2from BCl3-CH4-H2-argon mixtures[J].J Am Ceram Soc,1998,81(12):3077-3086. [15]BERJONNEAU J,CHOLLON G,LANGLAIS F.Deposition process of amorphous boron carbide from CH4/BCl3/H2precursor[J].J Elec-trochem Soc,2006,153(12):C795-C800. [16]GUO Q G,SONG J R,LIU L,et al.Relationship between oxidation resistance and structure of B4C-SiC/C composites with self-healing properties[J].Carbon,1999,37(1):33-40. [17]ANDERSSON S K,THOMAS M E.Infrared properties of CVDβ-SiC[J].Infrared Phys Technol,1998,39(4):223-234. [18]WERHEIT H,AU T,SCHMECHEL R,et al.IR-active phonons and structure elements of isotope-enriched boron carbide[J].J Solid State Chem,2000,154(1):79-86. [19]MARTINET C,DEVINE R A B.Analysis of the vibrational mode spectra of amorphous SiO2films[J].J Appl Phys,1995,77(9):4343-4348.