等离子喷涂制备TiC+(Al2O3/TiC)+Al2O3自愈合涂层

Full-Text   Cite this paper   Add to My Lib

Abstract:

采用大气等离子喷涂方法在马氏体钢基体上制备TiC+(Al2O3/TiC)+Al2O3复合涂层。对涂层的抗热冲击性能、热氧化处理前后截面形貌及成分进行了分析,利用电化学方法测量涂层的耐腐蚀性能。结果表明,这种复合涂层在高温下具有良好的自愈合能力及抗热冲击性能,涂层样品在800、700、600℃和500℃下的抗热冲击次数分别达到了157、125、95次和83次;在600℃经过30h热氧化处理之后,涂层的耐腐蚀性能提高了近1个数量级,孔隙率下降了90%以上。能谱分析表明,涂层中TiC在高温下的氧化产物填充并愈合了涂层中的裂纹与孔隙,起到了自愈合的作用。

References

[1]  ? MOSKALEWICZ T, SMEACETTO F, FILEMONOWICZ A C. Microstructure, properties and oxidation behavior of the glass–ceramic based coating on near-α titanium alloy [J]. Surf Coat Technol, 2009, 203(16): 2249–2253.
[2]  ? NAKAMICHI M, NAKAMURA H, HAYASHI K, et al. Impact of ceramic coating deposition on the tritium permeation in the Japanese ITER-TBM [J]. J Nucl Mater, 2009, 386(30): 692–695.
[3]  ? VILA R, HODGSON E R. TIEMF effect in ceramic coated cables [J]. J Nucl Mater, 2009, 386(30): 1041–1044.
[4]  ? TORREY J D, BORDIA R K. Mechanical properties of polymer-derived ceramic composite coatings on steel [J]. J Eur Ceram Soc, 2008, 28(1): 253–257.
[5]  ? MURTAZA G, HUSSAIN S S, SADIQ M, et al. Plasma focus assisted carburizing of aluminium [J]. Thin Solid Film, 2009, 517(24): 6777– 6783.
[6]  ? MATSUMOTO M, TAKAYAMA H, YOKOE D, et al. Thermal cycle behavior of plasma sprayed La2O3, Y2O3 stabilized ZrO2 coatings [J]. Scr Mater, 2006, 54(12): 2035–2039.
[7]  ? GADOW R, KERN F, KILLINGER A. Manufacturing technologies for nanocomposite ceramic structural materials and coatings [J]. Mater Sci Eng B, 2008, 148(1): 58–64.
[8]  ? KHAN A N, LU J. Thermal cyclic behavior of air plasma sprayed thermal barrier coating sprayed on stainless steel substrates [J]. Surf Coat Technol, 2007, 201(8): 4653–4658.
[9]  ? GIOLLI C, SCRIVANI A, RIZZI G, et al. Failure mechanism for thermal fatigue of thermal barrier coating systems [J]. J Therm Spray Technol, 2009, 18(2): 223–230.
[10]  ? GUO H F, AN M Z. Effect of surfactants on surface morphology of ceramic coatings fabricated on magnesium alloys by micro-arc oxidation [J]. Thin Solid Films, 2006, 500(2): 186–189.
[11]  ? SALMAN S, KOSE R, URTEKIN L, et al. An investigation of different ceramic coating thermal properties [J]. Mater Des, 2006, 27(7): 585–590.
[12]  ? RAO K P, RAM G D, STUCKER B E. Improvement in corrosion resistance of friction stir welded aluminum alloys with micro arc oxidation coatings [J]. Scr Mater, 2008, 58(11): 998–1001.
[13]  ? QUINTO D T. Mechanical property and structure relationships in hard coatings for cutting tools [J]. J Vac Sci Technol A: Vac Surf Films, 2009, 6(2): 2149–2157.
[14]  ? FU Q J, LI H J, ZHANG Z Z, et al. SiC nanowire-toughened MoSi2– SiC coating to protect carbon/carbon composites against oxidation [J]. Corros Sci, 2010, 52(5): 1879–1882.
[15]  ? CHANDRA S, FAUCHAIS P. Formation of solid splats during thermal spray deposition [J]. J Therm Spray Technol, 2009, 18(2): 148–180.
[16]  ? ASHIDA A, FUJITA A, SHIM Y, et al. ZnO thin films epitaxially grown by electrochemical deposition method with constant current [J]. Thin Solid Films, 2008, 517(4): 1461–1464.
[17]  ? CHECMANOWSKI J G, SZCZYGIE B. High temperature oxidation resistance of FeCrAl alloys covered with ceramic SiO2–Al2O3 coatings deposited by sol–gel method [J]. Corros Sci, 2008, 50(12): 3581–3589.

Full-Text