含Si–O–C界面层的C/Si–C–N复合材料的抗氧化性能

Full-Text   Cite this paper   Add to My Lib

Abstract:

为了研究利用Si–O–C界面层来提高碳纤维增强陶瓷基复合材料的抗氧化性能,利用化学气相浸渗和聚合物浸渗裂解工艺制备了以Si–O–C为界面的碳纤维增强Si–C–N陶瓷基复合材料(C/Si–O–C/Si–C–N)和无界面层的碳纤维增强Si–C–N陶瓷基复合材料(C/Si–C–N)。研究了C/Si–O–C/Si–C–N和C/Si–C–N在600、900℃和1200℃空气环境中的氧化行为。结果表明采用Si–O–C界面层后可提高复合材料的抗氧化性能;Si–O–C界面层较高的氧化抗力是碳纤维增强Si–C–N复合材料抗氧化性能提高的主要原因。

References

[1]  References:
[2]  ? ARGIRUSIS C, DAMJANOVI? T, BORCHARDT G. Yttrium silicate coating system for oxidation protection of C/C–Si–SiC composites: Electrophoretic deposition and oxygen self-diffusion measurements [J]. J Eur Ceram Soc, 2007, 27(2–3): 1303–1306.
[3]  ? YAN Z Q, XIONG X, XIAO P, et al. A multilayer coating of dense SiC alternated with porous Si–Mo for the oxidation protection of carbon/carbon silicon carbide composites [J]. Carbon, 2008, 46(1): 149– 153.
[4]  ? YAN Z Q, XIONG X, XIAO P, et al. Si–Mo–SiO2 oxidation protective coatings prepared by slurry painting for C/C–SiC composites [J]. Surf Coat Technol, 2008, 202(19): 4734–4740.
[5]  ? LI J, LUO R Y, LIN C, et al. Oxidation resistance of a gradient self-healing coating for carbon/carbon composites [J]. Carbon, 2007, 45(13): 2471–2478.
[6]  ? ZHOU G H, WANG S W, HUANG X X, et al. Improvement of oxidation resistance of unidirectional Cf/SiO2 composites by the addition of SiCp [J]. Ceram Int, 2008, 34(2): 331–335.
[7]  ? TONG C Q, CHENG L F, YIN X W, et al. Oxidation behavior of 2D C/SiC composite modified by SiB4 particles in inter-bundle pores [J]. Compos Sci Technol, 2008, 68(3–4): 602–607.
[8]  ? LUO R Y, YANG Z, LI L F. Effect of additives on mechanical properties of oxidation resistant carbon/carbon composite fabricated by rapid CVD method [J]. Carbon, 2000, 38(15): 2109–2115.
[9]  ? LABRUQUèRE S, BLANCHARD H, PAILLER R, et al. Enhancement of the oxidation resistance of interfacial area in C/C composites. Part II: Oxidation resistance of B–C, Si–B–C and Si–C coated carbon preforms densified with carbon [J]. J Eur Ceram Soc, 2002, 22(7): 1011–1021.
[10]  ? MA Q, CHEN Z, ZHENG W, et al. Effects of pyrolysis processes on microstructure and mechanical properties of Cf/Si–O–C composites fabricated by preceramic polymer pyrolysis [J]. Ceram Int, 2005, 31: 305–314.
[11]  ? WANG S, CHEN Z, MA Q, et al. Effect of fiber surface state on mechanical properties of Cf/Si–O–C composites [J]. Mater Sci Eng A, 2005, 407(1–2): 245–249.
[12]  ? MANOCHA L M, MANOCHA S M. Studies on solution-derived ceramic coatings for oxidation protection of carbon-carbon composites [J]. Carbon, 1995, 33(4): 435–440.
[13]  ? SAHA A, RAJ R. Crystallization maps for SiCO amorphous ceramics [J]. J Am Ceram Soc, 2007, 90(2): 578–583.
[14]  ? KOLá? F, MACHOVI? V, SVíTILOVá J, et al. Structural characterization and thermal oxidation resistance of silicon oxycarbides produced by polysiloxane pyrolysis [J]. Mater Chem Phys, 2004, 86(1): 88–98.
[15]  ? MOYSAN C, RIEDEL R, HARSHE R, et al. Mechanical characterization of a polysiloxane-derived SiOC glass [J]. J Eur Ceram Soc, 2007, 27(1): 397–403.
[16]  ? ROUXEL T, SORARU G D. Creep viscosity and stress relaxation of gel-derived silicon oxycarbide glasses [J]. J Am Ceram Soc, 2001, 84(5): 1052–1058.
[17]  ? LU G F, QIAO S R, ZHANG C Y, et al. Oxidation behaviors and mechanisms of C/Si–C–N with a mullite interlayer [J]. Adv Comp Mater, 2011, 20: 179–195.
[18]  ? LU G F, QIAO S R, ZHANG C Y, et al. Oxidation protection of C/Si–C–N composite by a mullite interphase [J]. Compos Part A, 2008, 39: 1467–1470.
[19]  ? PANTANO C G, SINGH A K, ZHANG H. Silicon oxycarbide glasses [J]. J Sol–Gel Sci Technol, 1999, 14: 7–25.
[20]  ? ZHAO J X, DING K H, WEI J X. Research on thermophysical properties and anti-thermal-vibration properties of C/C composites [J]. Acta Mater Compos Sinica, 1987, 4(4): 45–50.
[21]  ? JEDRZEJOWSKI P, CIZEK J, AMASSIAN A, et al. Mechanical and optical properties of hard SiCN coatings prepared by PECVD [J]. Thin Solid Films, 2004, 447–448: 201–207.
[22]  ? CAMUS G, GUILLAUMAT L, BASTE S. Development of damage in a 2D woven C/SiC composite under mechanical loading: I. mechanical characterization [J]. Compos Sci Technol, 1996, 56: 1363–1372.
[23]  ? SHIMOO T, OKAMURA K, YAMANALA T. Oxidation behavior of Si–C–O fibers (Nicalon) in alumina [J]. J Mater Sci, 2001, 36(17): 4137– 4143.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133