纳米CaF2对自润滑陶瓷材料力学性能的影响

DOI: 10.7521/j.issn.0454-5648.2014.09.08

Full-Text   Cite this paper   Add to My Lib

Abstract:

采用真空热压烧结工艺制备一种添加纳米固体润滑剂CaF2的新型自润滑陶瓷材料,其力学性能显著高于添加微米CaF2的自润滑陶瓷材料,并且断裂韧性高于不含CaF2的复合陶瓷材料。结果表明烧结后纳米CaF2主要位于基体晶粒内部,形成晶内型纳米结构。相比于添加微米CaF2,添加纳米CaF2时复合陶瓷材料的弹性模量增加了34%,这是材料硬度改善的主要原因。纳米CaF2诱发的穿晶断裂有助于提高复合陶瓷材料的断裂韧性和抗弯强度,裂纹偏转是添加纳米CaF2的复合陶瓷材料的主要增韧机制。

References

[1]   KONG L, BI Q, NIU M, et al. ZrO2(Y2O3)-MoS2-CaF2 self-lubricating composite coupled with different ceramics from 20 to 1000℃[J]. Tribol Int, 2013, 64: 53-62.
[2]   DENG J, CAO T, DING Z, et al. Tribological behaviors of hot-pressed Al2O3/TiC ceramic composites with the additions of CaF2 solid lubricants [J]. J Eur Ceram Soc, 2006, 26(8): 1317-1323.
[3]   DENG J, CAN T, SUN J. Microstructure and mechanical properties of hot-pressed Al2O3/TiC ceramic composites with the additions of solid lubricants [J]. Ceram Int, 2005, 31(2): 249-256.
[4]   QI Y, ZHANG Y, HU L. High-temperature self-lubricated properties of Al2O3/Mo laminated composites [J]. Wear, 2012, 280:1-4.
[5]   FANGY, ZHANGY, SONGJ, etal.Designandfabricationoflaminated-gradedzirconiaself-lubricatingcomposites [J].MaterDes, 2013, 49:421-425.
[6]   QI Y, ZHANG Y, FANG Y, et al. Design and preparation of high-performance alumina functional graded self-lubricated ceramic composites [J]. Compos Part B: Eng, 2013, 47:145-149.
[7]   XU C. Preparation and performance of an advanced multiphase composite ceramic material [J]. J Eur Ceram Soc, 2005, 25(5):605-611.
[8]   LIU B, HUANG C, LU X, et al. In situ growth of TiC whiskers in Al2O3 matrix for ceramic machine tools [J]. Ceram Int, 2007, 33(8): 1475-1480.
[9]   MUKHOPADHYAY A, CHAKRAVARTY D, BASU B. Spark plasma-sintered WC-ZrO2-Co nanocomposites with high fracture toughness and strength [J]. J Am Ceram Soc, 2010, 93(6): 1754-1763.
[10]   KELLY J R, DENRY I. Stabilized zirconia as a structural ceramic: an overview [J]. Dent Mater, 2008, 24(3): 289-298.
[11]   NIIHARA K. New design concept of structural ceramics-ceramic nanocomposites [J]. J Ceram Soc Japan, 1991, 99(10): 974-982.
[12]   AWAJI H, MATSUNAGA T, CHOI S. Relation between strength, fracture toughness, and critical frontal process zone size of ceramics [J]. J Jpn I Met, 2006, 70(1): 59-66.
[13]   ZHANG F C, LUO H H, ROBERTS S G. Mechanical properties and microstructure of Al2O3/mullite composite [J]. J Mater Sci, 2007, 42(16): 6798-6802.
[14]   XU Y, ZANGVIL A, KERBER A. SiC nanoparticle-reinforced Al2O3 matrix composites: Role of intra-and intergranular particles [J]. J Eur Ceram Soc, 1997, 17(7): 921-928.
[15]   GAO L, JIN X, KAWAOKA H, et al. Microstructure and mechanical properties of SiC-mullite nanocomposite prepared by spark plasma sintering [J]. Mater. Sci. Eng A, 2002, 334(1): 262-266.
[16]   JIANG D, VAN B O, VLEUGELS J. ZrO2-WC nanocomposites with superior properties [J]. J Eur Ceram Soc, 2007, 27(2): 1247-1251.
[17]   GREEN D J. Critical microstructures for microcracking in Al2O3-ZrO2 composites [J]. J Am Ceram Soc, 1982, 65(12): 610-614.
[18]   ZOU B, HUANG C, CHEN M, et al. Study of the mechanical properties, toughening and strengthening mechanisms of Si3N4/Si3N4w/TiN nanocomposite ceramic tool materials [J]. Acta Mater, 2007, 55(12): 4193-4202.
[19]   张永胜, 胡丽天, 陈建敏, 等. Y-TZP/A12O3/Mo纳米复合材料的制备及其力学性能[J]. 硅酸盐学报, 2009, 37(8): 1398-1401.
[20]     ZHANG Yongsheng, HU Litian, CHEN Jianmin, et al. J Chin Ceram Soc. 2009, 37(8): 1398-1401.
[21]   ZHANG Y S, HU L T, CHEN J M, et al. Lubrication behavior of Y-TZP/Al2O3/Mo nanocomposites at high temperature[J]. Wear, 2010, 268(9): 1091-1094.
[22]   张永胜,陈建敏,胡丽天.纳米复相陶瓷及其摩擦学研究进展[J].摩擦学学报,2006, 26(3): 284-288.
[23]     ZHANG Yongsheng, CHEN Jianmin, HU Litian. Tribology (in Chinese), 2006,26(3): 284-288.
[24]   HU T, ZHANG Y, HU L. Mechanical and wear characteristic of Y-TZP/Al2O3 nanocomposites [J]. Ind Lubr Tribol, 2014, 66(2): 209-214.
[25]   KARCH J, BIRRINGER R, GLEITER H. Ceramics ductile at low temperature [J]. Nature, 1987, 330: 556-558.
[26]   JIANG X, ZHAO J, JIANG X. Correlation between hardness and elastic moduli of the covalent crystals [J]. Comput Mater Sci, 2011, 50(7): 2287-2290.
[27]   刘于昌,黄晓巍.液相烧结氧化铝陶瓷及其烧结动力学分析[J].硅酸盐学报,2006, 34(6): 647-652.
[28]     LIU Yuchang,HUANG Xiaowei. J Chin Ceram Soc. 2006, 34(6): 647-652.
[29]   WANG Y, CHAN Y C, GUI Z L, et al. Application of Weibull distribution analysis to the dielectric failure of multilayer ceramic capacitors [J]. Mate Sci Eng B, 1997, 47(3): 197-203.
[30]   CHOKSHI A H, ROSEN A, KARCH J, et al. On the validity of the Hall-Petch relationship in nanocrystalline materials [J]. Scr Metall, 1989, 23(10): 1679-1683.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133