RE-Si-Al-O-N (RE=Y或Lu)连接Si3N4陶瓷接头的微观组织与性能
DOI: 10.14062/j.issn.0454-5648.2015.03.05
Abstract:
通过添加稀土Y或Lu,设计Si3N4–Al2O3–RE2O3–SiO2(RE-Si-Al-O-N,RE=Y或Lu)混合粉末焊料,原位形成以RE-Si-Al氧氮玻璃为中间层的氮化硅陶瓷接头。研究了连接过程中陶瓷接头微观组织与性能随连接温度、保温时间、稀土类型的变化,并分析了接头高温氧化行为。结果表明,采用Y-Si-Al-O-N焊料时,保温时间延长有利于接头内组织均匀化、焊缝致密化及焊料与母材间的相互扩散,形成良好连接。接头强度随保温时间延长先升高后降低,保温30min时,接头强度出现峰值(218MPa)。接头经1200℃氧化20h后仍保持原始强度的82%。采用Lu-Si-Al-O-N玻璃连接氮化硅,随连接温度升高,焊缝致密化程度提高,b-sialon相增加,连接强度呈现升高趋势。
References
[1] | BROCHU?M,?PUGH?M?D,?DREW?R?A?L.?Joining?silicon?nitride?ceramic?using?a?composite?powder?as?active?brazing?alloy?[J].?Mater?Sci?Eng?A,?2004,?374:?34–42.
|
[2] | LEMUS-RUIZ?J,?LEóN-PATI?O?C?A,?AGUILAR-REYES?E?A.?Interface?behaviour?during?the?self-joining?of?Si3N4?using?a?Nb-foil?interlayer?[J].?Scr?Mater,?2006,?54?(7):?1339–1343.
|
[3] | CHEN?J,?WEI?P,?MEI?Q,?et?al.?The?wettalility?of?Y-Al-Si-O-Noxynitride?glasses?and?its?application?in?silicon?nitride?joining[J].?J?Eur?Ceram?Soc,?2000,?20:?2685–2689.
|
[4] | Hampshire?S,Pomeroy?M?J.?Effect?of?composition?on?viscosities?of?rare?earth?oxynitride?glasses?[J].?J?Non-Cryst?Solids,?2004,?344:?1–7.
|
[5] | GLASS?S?J,?MAHONEY?F?M,?QUILLAN?B,?et?al.?Refractory?oxynitride?joints?in?silicon?nitride[J].?Acta?Mater,?46(1998):?4425–4438.
|
[6] | 刘春凤,?虞鸿江,?林英魁,?等.?原位形成氧氮玻璃中间层连接Si3N4陶瓷.?硅酸盐学报,?2013,?41(2):?275–280. LIU?Chunfeng,?YU?Hongjiang,?LIN?Yingkui,?et?al.?J?Chin?Ceram?Soc,?2013,?41(2):?275–280.
|
[7] | Gopal?M,?De?Jonghe?L?C,?thomas?G.?Indentation?and?oxidation?studies?on?silicon?nitride?joints?[C]//American?Ceramic?Society's?98th?Annual?Meeting,Indianapolis,?the?United?States,1996:?1–8.
|
[8] | SHELBY?J?E,?KOHLI?J.?Rare-earth?aluminosilicate?glasses?[J].?J?Am?Ceram?Soc,?1990,?73(1):?39–42.
|
[9] | 刘春凤.?稀土添加剂的类型对a-sialon陶瓷组织与性能的影响[D].?哈尔滨:?哈尔滨工业大学,?2007. LIU?Chunfeng.?Effect?of?type?of?rare-earth?on?microstructure?and?properties?of?a-sialon?ceramics?(in?Chinese,?dissertation).?Harbin:?Harbin?Institute?of?Technology,?2007.
|
[10] | ? 周玉.?陶瓷材料学[M].?哈尔滨:?哈尔滨工业大学出版社,?1995.
|
[11] | ZHANG?J,?SUN?Y,?LIU?C?F,?et?al.?Interfacial?microstructure?of?Si3N4/Si3N4?joint?brazed?using?Au-Ni-V?filler?alloy[J].?J?Mater?Sci,?2010,?45:?2188–2193.
|
[12] | GLASS?J,?MAHONEY?F?M,?QUILLAN?B,?et?al.?Refractory?oxynitride?joints?in?silicon?nitride?[J].?Acta?Mater,?1998,?46:?2393–99.
|
[13] | SAINZ?M?A,?MIRANZO?P,?OSENDI?M?I.?Silicon?nitride?joining?using?silica?and?yttria?ceramic?interlayers?[J].?J?Am?Ceram?Soc,?2002,?85(4):?941–46.
|
[14] | XIE?R?J,?MITOMO?M,?HCHEN?Z,?et?al.?Interfacial?microstructure?and?strength?of?partial?transient?liquid-phase?bonding?of?silicon?nitride?with?Ti/Ni?multi-interlayer?[J].?Mater?Sci?Eng?A,?2004,?380(1-2):?394–401.
|
[15] | BROCHU?M,?PUGH?M?D,?DREW?R?A?L.?PTLPB?of?Si3N4?to?FA-129?using?nickel?as?a?core?interlayer?[J].?Int?J?Refract?Met?Hard?Mater,?2004,?22:?95–103.
|
[16] | XIE?R?J,?MITOMO?M,?HUANG?L?P,?et?al.?Joining?of?silicon?nitride?ceramics?for?high-temperature?applications?[J].?J?Mater?Res,?2000,?15(1):?136–141.
|
[17] | ZHOU?F,?CHEN?Z.?Bonding?of?silicon?nitride?ceramic?composites?with?Y2O3-La2O3-Al2O3-SiO2?mixtures?[J].?J?Mater?Res,2002,?17(8):?1969–1972.
|
[18] | BECHER?P?F,?WATERS?S?B,?WESTMORELAND?C?G,?et?al.?Compositional?effects?on?the?properties?of?Si-Al-RE-based?oxynitride?glass?(RE=La,?Nd,?Gd,?Y,?or?Lu)?[J].?J?Am?Ceram?Soc,?2002,?85(4):?897–902.
|
Full-Text
|
|
Contact Us
service@oalib.com QQ:3279437679 
WhatsApp +8615387084133
|
|