碳化硅/石墨复合陶瓷密封材料的显微结构与性能

DOI: 10.14062/j.issn.0454-5648.2015.12.02

Full-Text   Cite this paper   Add to My Lib

Abstract:

以碳化硅微粉为原料、石墨为固体润滑添加剂,采用无压烧结技术制备碳化硅/石墨复合陶瓷密封材料,研究了石墨添加量对复合陶瓷密封材料烧结性能、显微结构、力学性能和摩擦性能的影响。结果表明,加入的石墨能以片状颗粒形态均匀分布在碳化硅陶瓷基体中;随着石墨添加量增加,复合陶瓷密封材料的体积密度、抗弯强度、弹性模量、断裂韧性、硬度均逐渐降低,但干、湿静摩擦系数则随之减小;当石墨添加量达到20%(质量分数)时,复合陶瓷的相对密度仅为90.6%,弯曲强度降至189MPa,弹性模量降至295GPa,断裂韧性为1.82MPa·m1/2,Vickers硬度为19.2GPa,而干、湿摩擦系数则分别减小到0.14和0.10。综合考虑复合陶瓷的力学性能和摩擦性能,石墨添加量控制在10%~15%之间为宜。

References

[1]  张玲洁. 颗粒、晶须强韧化碳化硅陶瓷及在密封环中的应用[D]. 杭州: 浙江大学, 2012.ZHANG Lingjie. Particle and whisker strengthening and toughing andapplication in sealing ring of SiC ceramic (in Chinese, dissertation).Hangzhou: Zhejiang University, 2012.
[2]  黄永银. 低摩擦碳化硅复合陶瓷的制备及机理[D]. 杭州: 浙江大学, 2012.HUANG Yongyin. The preparation and mechanism of low-friction SiCcomposite ceramic (in Chinese, dissertation). Hangzhou: ZhejiangUniversity, 2012.
[3]  顾永泉. 机械密封实用技术[M]. 北京: 机械工业出版社, 2001:85–109.
[4]  王静, 张玉军, 龚红宇. 无压烧结碳化硅研究进展[J]. 陶瓷,2008(4): 17–50.WANG Jing, ZHANG Yujun, GONG Hongyu. Ceramics(in Chinese),2008(4): 17–50.
[5]  郭兴忠, 朱潇怡, 张玲洁, 等. 无压烧结制备纳米复合碳化硅陶瓷[J]. 硅酸盐学报, 2010, 38(2): 258–264.GUO Xingzhong, ZHU Xiaoyi, ZHANG Lingjie, et al. J Chin CeramSoc, 2010, 38(2): 258–264.
[6]  郭兴忠, 杨辉, 王建武. SiC/YAG复合粉体的烧结特性与力学性能[J]. 稀有金属材料与工程, 2004, 33(3): 58–60.GUO Xingzhong, YANG Hui, WANG Jianwu. Rare Met Mater Eng(inChinese), 2004, 33(3): 58–60.
[7]  SAINI I, SHARMA A, ROZRA J, et al. Modification of structural,thermal, and electrical properties of PVA by addition of silicon carbidenanocrystals [J]. J Appl Polym Sci, 2015, 132(34): 42464–42471.
[8]  GUO X Z, YANG H, ZHU X Y, et al. Preparation and properties ofnano-SiC-based ceramic composites containing nano-TiN [J]. ScrMater, 2013, 68: 281–284.
[9]  KRENKEL W, HEIDENREICH B, RENZ R. C/C-SiC composites foradvanced friction systems [J]. Adv Eng Mater, 2002, 4(7): 427–436.
[10]  张亚妮, 徐永东, 楼建军, 等. 碳/碳化硅复合材料摩擦磨损性能分析[J]. 航空材料学报, 2005, 25(2): 49–54.ZHANG Yani, XU Yongdong, LOU Jianjun, et al. J Aeronaut Mater,2005, 25(2): 49–54.
[11]  GUO X Z, CAI X B, ZHANG J L, et al. Sintering, properties andmicrostructure of low friction SiC ceramic seals containing graphitefluoride [J]. Adv Appl Ceram, 2013, 112(6): 341–344.
[12]  YANG H, ZHANG J L, GUO X Z, et al. Pressureless sintering ofsilicon carbide ceramics containing zirconium diboride [J]. Ceram Int,2011, 37: 2031–2035.
[13]  ZHANG J L, YANG H, GUO X Z, et al. Preparation and properties ofsilicon carbide ceramics enhanced by TiN nanoparticles and SiCwhiskers [J]. Scr Mater, 2011, 65: 186–189.
[14]  KRENKEL W, BERND F, C/C-SiC composites for space applicationsand advanced friction systems [J]. Mater Sci Eng A, 2005, 412(1/2):177 –181.
[15]  SATO S, SERIZAWA, H ARAKI H, et al. Temperature dependence ofinternal friction and elastic modulus of SiC/SiC composites [J]. J AlloyCompd, 2003, 355(1 /2): 142–147.