Abstract:
研究了Fe-Cr-Mo、Fe-Cr-W合金的时效析出过程,发现在时效初期、两合金系中均有过渡R相析出,过渡R相为菱形点阵,α=0.9075nm,α=74.45°,其成分在Fe-Cr-Mo合金中为Pe-(27.5—34.9)Mo-(0—25.5)Cr,在Fe-Cr-W合金中为Fe-(28.9—33.0)W-(9.36—21.0)Cr(at.-%),时效后期,过渡R相分别向平衡相μ相、Laves相、χ相及σ相转变。
References
[1] | 1 Sinha A K, Buckley R A, Hume-Rothery W. J Iron Steel Inst, London, 1967; 205: 191
|
[2] | 2 刘世程,浜口由和,桑野寿.日本金属学会志,1986;50:1023
|
[3] | 3 Andersson J-O, Lange N. Trita-Mac-0322, Div Phys Metall, Royal Inst Technol, Stockholm Swedem: 1986
|
[4] | 4 刘世程,浜口由和,桑野寿,金属学报,1989;25:B97
|
[5] | 5 Hughes H. Keown S R, J Iron Steel Inst, London; 1968; 206: 275
|
[6] | 6 Goldschmidt H J. The Iron and Steel Inst London, Special Report No.43, 1951: 249
|
[7] | 7 Goldschmidt H J. Trans ASM, 1954; 46: 807
|
[8] | 8 刘世程,浜口由和,桑野寿.大连铁道学院学报,1989;10(2) :71
|
[9] | 9 McMullin J G, Reiter S F, Ebeling D G. Trans ASM, 1954; 46: 799
|
Full-Text
|
|
Contact Us
service@oalib.com QQ:3279437679 
WhatsApp +8615387084133
|
|