用流态化工艺制备WC-Co粉末
, PP. 144-146
Keywords: WC-Co,流态化,超细晶粒,硬质合金
Abstract:
用偏钨酸铵和硝酸钴原料喷雾干燥制成CoWO4/WO3复合粉末,用流态化反应炉使之在H2和CH4/H2气相中连续还原碳化成WC-Co粉末,着重研究了不同还原碳化工艺及其产物的形成机理.测试结果表明,所制CoWO4/WO3复合粉末呈均匀球形的非晶和微晶混合态,WC-Co粉末的晶粒细小均匀、相纯度高,适于制备超细晶粒的WC-Co硬质合金.