金属学报  1999 

镍基单晶高温合金CMSX-2原始树枝状晶中γ相的定向粗化

, PP. 902-908

Keywords: 树枝状晶,γ相,定向粗化,镍基,高温合金

Full-Text   Cite this paper   Add to My Lib

Abstract:

在760-1050℃和750-140MPa范围内,选择不同温度和应力的配合对CMSX-2合金进行持久拉伸至断裂,观察了试件原始树枝状晶区域(枝晶干、枝晶屑及枝晶间)中γ相的定向粗化及合金元素的分布特征.结果表明,γ的定相经程度在枝晶干内最大,在枝晶内次之,在枝晶间最小,在所有这些区域中,试验温度较高者的暄向粗化程度较大;各试件在持久试验后,γ形成元素W,Cr和Co,γ形成元素A1和Ta.

References

[1]  Tien J K, Copley S M Metall Trans, 1971: 2: 543
[2]  Fredholm A, Strudel J L In: Gell M, Kortovich C S, Bricknell R H, Kent W B, Radovich J F eds, Superalloys 1984.Warrendale, Pennsylvania: AIME,1984: 211
[3]  Mackay R A, Nathal M V. Acta Metall Mater, 1990;38:993
[4]  Buffiere J Y, Ignat M. Acta Metall Mater, 1990;43:1791
[5]  Socrate S, Parks D M. Acta Metall Mater, 1993;41: 2185
[6]  Pollock T M, Argon A S Acta Metall Mater, 1994;42: 1859
[7]  Guo X P, Fu H Z, Sun J H. Acta Metall Sin, 1994;30: A321(郭喜平,傅恒志,孙家华. 金属学报,1994;30: A321)
[8]  Peng Z F,Glatzel U;Feller-Kniepmeier M.Acta Metall Sin,1995; 31: A531(彭志方,Glatzel U,Feller-Kniepmeirer M、金属学报,1995;31:A531)
[9]  Nabarro F R N. Metall Mater Trans, 1996 27A: 1147
[10]  Chen W,Immarigeon J P Scr Mater 1998; 39: 167
[11]  Peng Z F, Ren Y Y, Fan B Z,Yan P,Zhao J C, Sun J H.Acta Metall Sin, 1999; 35: 9(彭志方,任遥遥,樊宝珍,燕平.赵京晨.孙家华,金属学报.1999;35:9)
[12]  Nathal M V,Ebert L J Scr Metall,1983;17:1151
[13]  Mackay R A,Ebert L J Metall Trans, 1985;16A: 1969
[14]  Nathal M V. Metall Trans,1987;18A:1961
[15]  Nathal M V,Mackay R A.Miner R V,Metall Trans,1989;20A:133
[16]  Peng Z F,Clatzel U,Link T, Feller-Kniepmeier M ScrMater, 1996; 34:221
[17]  Peng Z F, Yan Y H. Acta Metall Sin, 1997;33: 1147(彭志方,严演辉,金属学报,1997;33:1147)
[18]  Tian S G, Zhou H H Zhang J H, Yang H C, Xu Y B, Hu ZQ. Acta Metall Sin,1998;34:591
[19]  (田素贵,周惠华,张静华,杨洪才,徐永波,胡壮麒,金属学报,1998 34:591)
[20]  Peng Z F, Ren Y Y, Fan B Z Yan P, Zhao J C, Sun J HActa Metall Sin, 1999; 35: 265(彭志方,任遥遥,樊宝珍,燕平,赵京晨,孙家华,金属学报,1999 35:265)
[21]  Thinckauf K, Nembach E Acta Metall Mater, 1991: 39: 3057
[22]  Nathal M V, Ebert L J. Metall Trans, 1985;16A: 1849
[23]  Svetlov I L,Golovko B A Epinshin A I, Abalakin N P ScrMetall Mater, 1992; 26: 1353
[24]  Schmidt R Feller-Kniepmeier M. Scr Metall Mater, 1993;29:1079
[25]  Liu Z Y, Li J G, Fu H Z. Acta Metall Sin, 1995: 31: A329(刘忠元,李建国,傅恒志.金属学报, 1995; 31: A329)
[26]  Schmidt R, Feller-Kniepmeier M Metall Trans, 1992;23A:745
[27]  Qiu Y M,Zhu Y X.Acta Metall Sin,1989;25:A78(邱一鸣,朱耀霄,金属学报,1989;25:A78)
[28]  Wang J A. Yu Y S, Zrnik J, Zitnansky M Mater Sci Technol,1997; 5:5(王纪安,余水泗, Zrnik J, Zitnansky M,材料科学与工艺,1997;5:5)
[29]  Hazotte A,Locaze J. Scr Metall,1989;23:1977
[30]  Glatzel U. Microstructure and Internal Strains of Unde-formed and Creep Deformed Samples of a Nickel-Base Su-peralloy. Verlag Dr Koster, Berlin. 1994: 8
[31]  Nathal M V,Mackay R A, Garlick R G. Mater Sci Eng. 1985;75:195

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133