340MPa级BH钢的Snoek-K■─Kster阻尼
, PP. 831-835
Keywords: 内耗,SKK峰,钢,烘烤硬化
Abstract:
研究了两种成分的340MPa级烘烤硬化(BH)钢的Snoek—(SKK)阻尼发现用通常范围的频率测量内耗时,BH钢的SKK峰激活能(H)明显偏大;用1.7Hz的较高频率测量时,二者中含C量较高(0.024%)钢的Q-1-T曲线呈双中温峰
References
[1] | 1 Magalas L B.J Phys, 1996; 4: 163
|
[2] | 2 Kster W L, et al. Arch Eisenh ttenw, 1954; 25: 569
|
[3] | 3 T S.Trans AIME,1948;176:448
|
[4] | 4戢景文,赵增琪,贺礼端,耿殿奇物理学报,1985;3:1620(Ji J W, Zhao Z Q, He L D, Geng D Q. Acta Metall Sin, 1985; 34: 1620)
|
[5] | 5戢景文,赖祖涵,吴玉琴,张国福,李广义.金属学报,1991; 27:A408(Ji J W,Lai Z H,Wu Y Q,Zhang G F,Li G Y.Acta Metall Sin,1991;27:A408)
|
[6] | 6Petarra D P, Bechers P N. Acto Metall, 1967; 15: 791
|
[7] | 7 Ino H, Sugeno T. Acta Metall, 1967;15:1197
|
[8] | 8戢景文,魏全金,张国福,赖祖涵,陈廷国.金属学报.1902;28:A207(Ji J W, Wei Q J, Zhang G F, Lai Z H, Chen T G. Acta Metall Sin, 1992; 28: A207)
|