Fe74.5Ni10Si3.5B9C2非晶带的氢致滞后断裂

, PP. 91-94

Keywords: Fe74.5Ni10Si3.5B9C2,非晶合金

Full-Text   Cite this paper   Add to My Lib

Abstract:

Fe74.5Ni10Si3.5B9C2非晶带在恒截荷动态充氢时能发生氢致滞后断裂,测量了不同充氢电流密度i下的氢致滞后断裂归一化门槛应力σHIC/σF,以及进入试样的氢浓度Co,结果表明,当Co≤67.4×10^-4%时,σHIC/σF随lnCO上升成线性下降,即σHIC/σF=1.59-0.35lnCo,当C0>67.4×10^-4%后,σHIC/σF≤0.1,由于实验精度的限制无法测出真实的σFIC/σF值.

References

[1]    Kawashima A,  Hashimoto K, Masumoto T.   Corrosion,1980; 36: 577
[2]    Tong H S, Macur J E. Corrosion, 1982; 38: 464 
[3]    Latanision R M, Compeau C R, Kurkela M. In: Gibala R,Hehemann R F eds., Hydrogen Embrittlement and StressCorrosion Cracking, Metals Park, Ohio: ASM, 1984: 297 
[4]    Ashok S, Stoloff N S, Glicksman M E, Slavin T. Scr Met-all, 1981; 15: 331 
[5]    Flis J, Ashok S, Stoloff N S, Duquette D J. Acta Metall,1987; 35: 2071
[6]    Lin J J, Perng T P. J Mater Sci Lett, 1991; 10:  1443 
[7]    Zuo Y, Latanision R M. Mater Sci Eng, 1992; 159A: 87 
[8]    Lin J J, Perng T P. Metall Mater Trans, 1995; 26A: 197 
[9]    Zu Y. Corros Sci Protect Technique, 1996; 8: 43(左 禹 腐蚀科学与防护技术,1996;96;8:43)
[10]   Eliaz N, Eliezer D. Adv Perform Mater, 1999; 6: 5 
[11]   Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture andEnvironmental Fracture.    Beijing:   Science Press,  2000:120
[12]  (褚武扬,乔利杰,陈奇志,高克玮. 断裂和环境断裂. 北京:科学出版社,2000:120)

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133