金属学报  2009 

B对Fe--Ni基合金显微组织和抗氢性能的影响

, PP. 167-172

Keywords: Fe--Ni基合金,B,η相,氢致塑性损减

Full-Text   Cite this paper   Add to My Lib

Abstract:

利用金相显微镜、扫描电镜观察结合力学性能和抗氢性能测试研究了B对Fe--Ni基合金显微组织和抗氢性能的影响.结果表明B的加入有效地抑制了时效过程中晶界上大量η(Ni3Ti)相的析出,晶界上仅析出少量碳化物,从而显著提高了合金的塑性和抗氢性能.断口观察显示,对于无B合金,在由峰值时效到过时效处理的过程中,由于η相的长大,使合金发生由穿晶到沿晶断裂的转变;热充氢后,H在η/γ界面的积聚,促使合金发生大量沿晶断裂,而含B合金在热充氢后仍以穿晶断裂为主.

References

[1]  Cicco H D, Luppo M I, Gribaudo L M, Garcia J O. Mater Charact, 2004; 52: 85
[2]  Ma L M, Liang G J, Fan C G, Li Y Y. Acta Metall Sin, 1997; 10: 206
[3]  Thompson AW, Brooks J A. Metall Trans, 1975; 6A: 1431
[4]  Brooks J A, Thompson A W. Metall Trans, 1993; 24A: 1983
[5]  Rho B S, Hong H U, Nam S W. Scr Mater, 2000; 43: 167
[6]  Li X Y, Zhang J, Rong L J, Li Y Y. J Mater Sci Eng, 2005; 23: 483
[7]  (李秀艳, 张 建, 戎利建, 李依依. 材料科学与工程学报, 2005; 23: 483)
[8]  Zhang J, Li X Y, Rong L J, Zheng Y N, Zhu S Y. Acta Metall Sin, 2006; 42: 469
[9]  (张 建, 李秀艳, 戎利建, 郑永男, 朱升云. 金属学报, 2006; 42: 469)
[10]  Li X Y, Li Y Y. Hydrogen Damaged of Austenitic Alloy. Beijing: Science Press, 2003: 1
[11]  (李秀艳, 李依依. 奥氏体合金的氢损伤. 北京: 科学出版社, 2003: 1)
[12]  Fujwara M, Uchida H, Ohta S. J Mater Sci Lett, 1994; 13: 557
[13]  Kennedy R L, Cao W D, Thomas W M. Adv Mater Pro, 1996; 149: 33
[14]  Sellamuthu R, Giamei A F. Metall Trans, 1986; 17A: 419
[15]  Wills V A, Mccartney D G. Mater Sci Eng, 1991; A145: 223
[16]  Franzoni U, Marchetti F, Sturless S. Scr Metall, 1985; 19: 511
[17]  Shulga A V. J Alloys Compd, 2007; 486: 155
[18]  Horton J A, Mckamey C G, Miller M K, Cao W D,Kennedy R L. Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS AIME, 1997: 401
[19]  Yao X X. Mater Sci Eng, 1999; A271: 353
[20]  Sourmail T, Okuda T, Taylor J E. Scr Mater, 2004; 50: 1271
[21]  Ducki K J, Hermanczyk M H, Kuc D. Mater Chem Phy, 2003; 81: 490
[22]  Rho B S, Nam S W. Mater Sci Eng, 2000; A291: 54
[23]  Li X Y, Zhang J, Rong L J, Li Y Y. Mater Sci Eng, 2008; A488: 547
[24]  Zhao S Q, Xie X S, Smith G D, Patel S J. Mater Sci Eng, 2003; A355: 96
[25]  He X L, Chu Y Y, Ke J. Acta Metall Sin, 1982; 18: 1
[26]  (贺信莱, 褚幼义, 柯俊. 金属学报, 1982; 18: 1)
[27]  Kurban M, Erb U, Aust K T. Scr Mater, 2006; 54: 1053
[28]  Seto K, Larson D J,Warren P J, Smith G DW. Scr Mater, 1999; 40: 1029
[29]  Wu Y X, Li X Y, Wang Y M. Acta Mater, 2007; 55: 4845

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133