金属学报  2013 

稀土Ce添加对Fe83Ga17合金微结构和磁致伸缩性能的影响

DOI: 10.3724/SP.J.1037.2012.00498, PP. 87-91

Keywords: Fe-Ga合金')",&searchField=keyword">href="#">,Fe-Ga合金,磁致伸缩,稀土Ce添加,微结构

Full-Text   Cite this paper   Add to My Lib

Abstract:

为了改善Fe-Ga合金的磁致伸缩性能,采用真空非自耗电弧炉制备了Fe83Ga17Cex(x=0.0,0.2,0.4,0.6,0.8,1.0)合金,用X射线衍射仪(XRD)和扫描电镜及能谱仪(SEM/EDS)分析了合金的微结构,用电阻应变法测量了合金的磁致伸缩性能.结果表明Fe83Ga17合金由单一的bcc结构A2相组成.而添加稀土Ce后,除x=0.2合金外,Fe83Ga17Cex合金主要由bcc结构的A2相和CeFe2第二相组成.此外,Fe83Ga17合金的微观组织是晶粒粗大的等轴晶,而Fe83Ga17Ce0.8合金的微观组织是晶粒细小的柱状晶.与Fe83Ga17对照合金相比,除x=0.2合金的磁致伸缩系数略小于对照合金外,其他添加稀土Ce后的合金样品磁致伸缩系数均明显增加.添加稀土Ce后,Fe83Ga17Cex合金的磁致伸缩系数随稀土Ce含量的增加呈现出先增加后减小的变化趋势,x=0.8合金的磁致伸缩系数最大,在557kA/m外加磁场下,磁致伸缩系数达到356×10-6.

References

[1]  Na S M, Flatau A B.Scr Mater, 2012; 66: 307
[2]  Li J H, Gao X X, Xie J X, Yuan C, Zhu J, Yu R B.Intermetallics, 2012; 26: 66
[3]  Fang M L, Zhu J, Li J H, Gao X X.Intermetallics, 2011; 19: 1804
[4]  Zhou Y, Wang B W, Li S Y, Wang Z H, Huang W M, Cao S Y, Huang W P. J Magn Magn Mater, 2010; 322: 2104
[5]  Reddy K S M, Estrine E C, Lim D H, Smyrl W H, Stadler B J H. Electrochem Commun, 2012; 18: 127
[6]  Bormio--Nunes C, Turtelli R S, Mueller H, Grossinger R,Sassik H, Tirelli M A.J Magn Magn Mater, 2005; 290--291: 820
[7]  Hu Y, Ding Y T, Zhang Y L, Wang G B, Zhou Z G.Trans Nonferrous Met Soc Chia, 2012; 22: 2146
[8]  Kirchmayr H R, Poldy C A.J Magn Magn Mater, 1978; 8: 1
[9]  Wang B W, Cao S Y, Huang W M.Magnetostrictive Material and Devices.Beijing: Metallurgical Industry Press, 2008: 14(王博文, 曹淑英, 黄文美. 磁致伸缩材料与器件. 北京:冶金工业出版社, 2008: 14)
[10]  Gu M, Zhou J K, Li J G.J Alloys Compd, 2007; 441: 81
[11]  Basumatary H, Palit M, Chelvane J A, Pandian S, Raja M M,Chandrasekaran V.Scr Mater, 2008; 59: 878
[12]  Xu S F, Zhang H P, Wang W Q, Guo S H, Zhu W, Zhang Y H, Wang X L,Zhao D L, Chen J L, Wu G H.J Alloys Compd, 2009; 469: 203
[13]  Zhu J, Peng F L, Fang M L, Li J H, Gao X X, Yu R H.Chin Phys,2011; 20B: 057504
[14]  Cui Z Q.Metallography and Heat Treatment. Beijing: MachineryIndustry Press, 2000: 52(崔忠圻. 金属学与热处理. 北京: 机械工业出版社, 2000: 52)
[15]  Li Y X, Liu H Y, Li S T, Meng F B, Lu Z M, Qu J P, Chen J L, Wu G H,Tang C.J Alloys Compd, 2006; 408--412: 127
[16]  Callen E, ed. Gardner F S,Proc Metallic Magnetoacoustic Materiala Workshop, Boston, MA, 1969: 75
[17]  Koon N C, Schindler A I, Carter F L.Phys Lett, 1971; 37A: 413
[18]  Lograsso T A, Ross A R, Schlagel D L, Clark A E, Wun--Fogle M. J Alloys Compd, 2003; 350: 95
[19]  Takahashi T, Hashimoto K, Okazaki T, Furuya Y, Kubota T, Saito C. Scr Mater, 2009; 60: 847
[20]  Li C, Liu J H, Wang Z B, Jiang C B.J Magn Magn Mater,2012; 324: 1177
[21]  Hatchard T D, George A E, Farrell S P, Steinitz M O, Adams C P,Cormier M, Dunlap R A.J Alloys Compd, 2010; 494: 420
[22]  Gong Y, Jiang C B, Xu H B.Acta Metall Sin, 2006; 42: 830(龚彦, 蒋成保, 徐惠彬. 金属学报, 2006; 42: 830)
[23]  Zhang J J, Ma T Y, Yan M.Physica, 2010; 405B: 3129
[24]  Gaudet J M, Hatchard T D, Farrell S P, Dunlap R A.J Magn Magn Mater,2008; 320: 821
[25]  Mellors N J, Zhao X, Simmons L M, Quinn C J, Kilcoyne S H.J Magn Magn Mater, 2012; 324: 3817
[26]  Sun L, Zhang M C, Gao X X, Qiao Y, Zhu J.J Alloys Compd,2008; 463: 6
[27]  Li J H, Gao X X, Zhu J, Li J, Zhang M C.J Univ Sci Technol Beijing, 2009; 31: 1281(李纪恒, 高学绪, 朱洁, 李洁, 张茂才. 北京科技大学学报, 2009; 31: 1281)
[28]  Jiang L P, Zhang G R, Yang J D, Hao H B, Wu S X, Zhao Z Q. J Rare Earths, 2010; 28: 409
[29]  Yu Q G, Jiang L P, Zhang G R, Hao H B, Wu S X, Zhao Z Q. Chin Rare Earths, 2010; 31(4): 21(于全功, 江丽萍, 张光睿, 郝宏波, 吴双霞, 赵增祺. 稀土, 2010; 31(4): 21)

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133