Han E H, Wang J Q, Wu X Q, Ke W. Acta Metall Sin, 2010; 46: 1379 (韩恩厚, 王俭秋, 吴欣强, 柯 伟. 金属学报, 2010; 46: 1379)
[2]
Joseph A, Rai S K, Jayakumar T, Murugan N. Int J Pressure Vessels Piping, 2006; 82: 700
[3]
Seifert H P, Ritter S, Shoji T. J Nucl Mater, 2008; 378: 197
[4]
Wang H T, Wang G Z, Xuan F Z, Tu S T. Eng Failure Analysis, 2013; 28: 134
[5]
Peng Q J, Xue H, Hou J, Sakaguchi K, Takeda Y, Kuniya J, Shoji T. Corros Sci, 2011; 53: 4309
[6]
Hou J, Peng Q J, Kuniya J, Shoji T, Wang J Q, Han E H, Ke W. J Mater Sci, 2010; 397: 109
[7]
Li G F, Congleton J. Corros Sci, 2000; 42: 1005
[8]
Meng F J, Wang J Q, Han E H, Shoji T, Ke W. Acta Metall Sin, 2011; 47: 839 (孟凡江, 王俭秋, 韩恩厚, 庄子哲雄, 柯 伟. 金属学报, 2011; 47: 839)
[9]
Bowerman B S, Czajkowski C J, Roberts T C, Neal C. Mater Charact, 1999; 43: 347
[10]
Li G F, Li G J, Fang K W, Peng J, Yang W. Acta Metall Sin, 2011; 47: 797 (李光福, 李冠军, 方可伟, 彭 君, 杨 武. 金属学报, 2011; 47: 797)
[11]
Wang H T, Wang G Z, Xuan F Z, Liu F Z, Tu S T. Mater Sci Eng, 2013; A568: 108
[12]
Choi K J, Kim J J, Lee B H, Bahn C B, Kim J H. J Nucl Mater, 2013; 441: 493
[13]
Hou J, Peng Q J, Lu Z P, Shoji T, Wang J Q, Han E H, Ke W. Corros Sci, 2010; 52: 3949
[14]
Hanninen H, Brederholm A, Toivonen A. 15th Int Conf on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors, Colorado Springs: TMS, 2011: 197
[15]
Sathirathinda N, Gubner R, Pan J, Kivisakk U. Electrochem Solid-State Lett, 2008; 11: C41
[16]
Kasper J S. Acta Metall, 1954; 2: 456
[17]
Michalska J, Sozanska M. Mater Charact, 2006; 56: 355
[18]
Popov A A, Bannikova A S, Belikov S V. Phys Met Metall, 2009; 108: 586
[19]
Chun E J, Baba H, Nishimoto K, Saida K. Mater Charact, 2013; 86: 152
[20]
Escriba D M, Materna-Morris E, Plaut R L, Padilha A F. Mater Charact, 2009; 60: 1214
[21]
Martin D S, Rivera Diaz del Castillo P E J, Peekstok E van del Zwaag S. Mater Charact, 2007; 58: 455
[22]
Lai J K L, Meshukat M. Met Sci, 1978; 9: 416
[23]
Falata L, Svoboda M, Vyrostkova A, Petryshynets I, Sopko M. Mater Charact, 2012; 72: 15
[24]
Naffakh H, Shamanian M, Ashrafizadeh F. J Mater Process Technol, 2009; 209: 3628
[25]
Nelson T W, Lippold J C, Mills M J. Sci Technol Weld Joining, 1998; 77: 249
[26]
Rowe M D, Nelson T W, Lippold J C. Sci Technol Weld Joining, 1999; 78: 31
[27]
Srinivasan P B, Muthupandi V, Dietzel W, Sivan V. Mater Des, 2006; 27: 182
[28]
Hou J, Peng Q J, Shoji T, Wang J Q, Ke W, Han E H. Acta Metall Sin, 2010; 46: 1258 (侯 娟, 彭群家, 庄子哲雄, 王俭秋, 柯 伟, 韩恩厚. 金属学报, 2010; 46: 1258)
[29]
Asami K, Sakai T. Trans Iron Steel Inst Jpn, 1981; 21: B269
[30]
Nelson T W, Lippold J C, Mills M J. Sci Technol Weld Joining, 1999; 78: 329
[31]
Nelson T W, Lippold J C, Mills M J. Sci Technol Weld Joining, 2000; 79: 267
[32]
Hou J, Peng Q J, Takeda Y, Kuniya J, Shoji T, Wang J Q, Han E H, Ke W. J Mater Sci, 2010; 45: 5332
[33]
Wang H T. PhD Dissertation, East China University of Science and Technology, Shanghai, 2013 (王海涛. 华东理工大学博士学位论文, 上海, 2013)
[34]
Naffakh H, Shamanian M, Ashrafizadeh F. J Mater Process Technol, 2009; 209: 3628
[35]
Gertsman V Y, Tangri K, Valiev R Z. Acta Metall Mater, 1994; 42: 1785
[36]
Gertsman V Y, Bruemmer S M. Acta Mater, 2001; 49: 1589
[37]
Lehockey E M, Brennenstuhl A M, Thompson I. Corros Sci, 2004; 46: 2383
[38]
Pan Y, Adams B L, Olson T, Panayotou N. Acta Mater, 1996; 44: 4685
[39]
Lee H T, Wu J L. Corros Sci, 2009; 51: 733
[40]
Qiao D, Zhang W, Pan T Y, Crooker P, David S, Feng Z. Sci Technol Weld Joining, 2013; 92: 624