OALib Journal期刊
ISSN: 2333-9721
费用:99美元
|
|
|
可见光响应型Bi2WO6光催化剂
, PP. 2124-2131
Keywords: Bi2WO6,光催化,纳米结构,超结构,异质结构,掺杂
Abstract:
Bi2WO6作为一种新型半导体光催化剂,具有较窄的带隙宽度和特殊的层状结构,因而显示出良好的可见光催化性能。本文综述了围绕提高Bi2WO6的光催化活性和实用性而开展的相关研究成果,包括纳米结构Bi2WO6材料;分级超结构Bi2WO6材料;Bi2WO6光催化剂的系列修饰改性,如金属氧化物复合、碳烯和金属单质的表面沉积,以及金属离子和非金属离子的掺杂等。此外,还从回收角度综述了Bi2WO6的固定化技术。最后对Bi2WO6光催化剂的发展趋势进行了展望,强调对Bi2WO6进行带隙调控,并加强对其异质结构界面状态的研究,通过理论计算可深入理解光催化机制,以从制备入手指导现有催化剂的改良和设计新型光催化剂。
References
[1] | Chen X B, Mao S S. Chem. Rev., 2007, 107: 2891-2959
|
[2] | Tang J W, Zou Z G, Ye J H. Angew. Chem. Int. Ed., 2004, 43: 4463-4466
|
[3] | Zhu H Y, Chen X, Zheng Z F, Ke X B, Jaatinen E, Zhao J C, Guo C, Xie T F, Wang D J. Chem. Commun., 2009, 7524-7526
|
[4] | Wang D F, Kako T, Ye J H. J. Am. Chem. Soc., 2008, 130: 2724-2725
|
[5] | McDowell N A, Knight K S, Lightfoot P. Chem. Eur. J., 2006, 12: 1493-1499
|
[6] | Tang J W, Zhou Z G, Ye J H. Catal. Lett., 2004, 92: 53-56
|
[7] | Xiao Q, Zhang J, Xiao C, Tan X K. Catal. Comm., 2008, 9: 1247-1253
|
[8] | Kudo A, Hijii S. Chem. Lett., 1999, 1103-1104
|
[9] | Zhang C, Zhu Y F. Chem. Mater., 2005, 17: 3537-3545
|
[10] | Zhang G K, Lü F, Li M, Yang J L, Zhang X Y, Huang B B. J. Phys. Chem. Solids, 2010, 71: 579-582
|
[11] | Saison T, Chemin N, Chanéac C, Durupthy O, R uaux V, Mariey L, Maugé F, Beaunier P, Jolivet J P. J. Phys. Chem. C, 2011, 115: 5657-5666
|
[12] | Zhang G Q, Chang N, Han D Q, Zhou A Q, Xu X H. Mater. Lett., 2010, 64: 2135-2137
|
[13] | Zhou Y, Tian Z P, Zhao Z Y, Liu Q, Kou J H, Chen X Y, Gao J, Yan S C, Zou Z G. Appl. Mater. inter., 2011, 3: 3594-3601
|
[14] | Xu C X, Wei X, Guo Y M, Wu H Q, Ren Z H, Xu G, Shen G, Han G H. Mater. Res. Bull., 2009, 44: 1635-1641
|
[15] | Li Y Y, Liu J P, Huang X T. Nanoscale Res. Lett., 2008, 3: 365-371
|
[16] | Li Y Y, Liu J P, Huang X T, Li G Y. Cryst. Growth Des., 2007, 7: 1350-1355
|
[17] | Ma D K, Huang S M, Chen W X, Hu S W, Shi F F, Fan K L. J. Phys. Chem. C, 2009, 113: 4369-4374
|
[18] | Korte K E, Skrabalak S E, Xia Y N. J. Mater. Chem., 2008, 18: 437-441
|
[19] | Zhang J, Bang J H, Tang C C, Kamat P V. ACS Nano., 2010, 4: 387-395
|
[20] | Gui M S, Zhang W D. Nanotechnology, 2011, art. nn. 22: 265601
|
[21] | Murcia L S, Hidalgo M C, Navío J A, Colón G. J. Hazard. Mater., 2011, 185: 1425-1434
|
[22] | Xu Q C, Wellia D V, Ng Y H, Amal R, Tan T T Y. J. Phys. Chem. C, 2011, 115: 7419-7428
|
[23] | Cui Z K, Zeng D W, Tang T T, Liu J, Xie C S. Catal. Comm., 2010, 11: 1054-1057
|
[24] | Chen Y L, Cao X X, Kuang J D, Chen Z, Chen J L, Lin B Z. Catal. Comm., 2010, 12: 247-250
|
[25] | Gao E P, Wang W Z, Shang M, Xu J H. Phys. Chem. Chem. Phys., 2011, 13: 2887-2893
|
[26] | Xu J H, Wang W Z, Gao E P, Ren J, Wang L. Catal. Comm., 2011, 12: 834-838
|
[27] | Ren J, Wang W Z, Sun S M, Zhang L, Chang J. Appl. Catal. B, 2009, 92: 50-55
|
[28] | Zhang L S, Wong K H, Yip H Y, Hu C, Yu J C, Chan C Y, Wong P K. Environ. Sci. Technol., 2010, 44: 1392-1398
|
[29] | Fu H B, Zhang S C, Xu T G, Zhu Y F, Chen J M. Environ. Sci. Technol., 2008, 42: 2085-2091
|
[30] | Zhang L, Wang W Z, Shang M, Sun S M, Xu J H. J. Hazard. Mater., 2009, 172: 1193-1197
|
[31] | Xu J H, Wang W Z, Shang M, Sun S M, Ren J, Zhang L. Appl. Catal. B, 2010, 257: 227-232
|
[32] | Kamat P V. Chem. Rev., 1993, 93: 267-300
|
[33] | Wang R, Hashimoto K, Fujishima K, Chikuni M, Kojima E, Kitamura A, Shimohigoshi M, Watanabe T. Nature, 1997, 388: 431-432
|
[34] | Fu H B, Zhang L W, Yao W Q, Zhu Y F. Appl. Catal. B, 2006, 66: 100-110
|
[35] | Tang J W, Zou Z G, Ye J H. Catal. Lett., 2004, 92: 53-56
|
[36] | Mclaren A, Valdes-Solis T, Li G Q, Tsang S C. J. Am. Chem. Soc., 2009, 131: 12540-12541
|
[37] | Shang M, Wang W Z, Sun S M, Zhou L, Zhang L. J. Phys. Chem. C, 2008, 112: 10407–10411
|
[38] | Xu C X, Wei X, Ren Z H, Wang Y, Xu G, Shen G, Han G R. Mater. Lett., 2009, 63: 2194–2197
|
[39] | Wu L, Bi J H, Li Z H, Wang X X, Fu X Z. Catal. Today, 2008, 131: 15–20
|
[40] | Shang M, Wang W Z, Xu H L. Cryst. Growth Des., 2009, 9: 991-996
|
[41] | Zhang G Y, Feng Y, Wu Q S, Xu Y Y, Gao D Z. Mater. Res. Bull., 2012, 47: 1919-1924
|
[42] | Zhang L S, Wang W Z, Chen Z G, Zhou L, Xu H L, Zhu W. J. Mater. Chem., 2007, 17: 2526-2532
|
[43] | Wang W Z, Poudel B, Ma Y, Ren Z F. J. Phys. Chem. B, 2006, 110: 25702-25706
|
[44] | Wu J, Duan F, Zheng Y, Xie Y. J. Phys. Chem. C, 2007, 111: 12866-12871
|
[45] | Li Y Y, Liu J P, Huang X T. Nanoscale Res. Lett., 2008, 3: 365-371
|
[46] | Zhang L S, Wang W Z, Zhou L, Xu H L. Small, 2007, 9: 1618-1625
|
[47] | Liu S W, Yu J G. J Solid State Chem., 2008, 181: 1048-1055
|
[48] | Zhang LW, Baumanis C, Robbern L, Kandiel T, Bahnemann D. Small, 2011, 7: 2714-2720
|
[49] | Cao X F, Zhang L, Chen X T, Xue Z L. Cryst. Eng. Comm., 2011, 13: 306-311
|
[50] | Huang Y, Wu J H, Huang M L, Lin J M, Huang Y F, Huang Y. Sci. China Chem., 2011, 54: 211-216
|
[51] | Chen Z, Qian L W, Zhu J, Yuan Y P, Qian X F. Cryst. Eng. Comm., 2010, 12: 2100-2106
|
[52] | Robert D. Catal. Today, 2007, 122: 20-26
|
[53] | Ge M, Li Y F, Liu L, Zhou Z, Chen W. J. Phys. Chem. C, 2011, 115: 5220-5225
|
[54] | Zhou Y, Vuille E, Heel A, Patzke G R. Z. Anorg. Allg. Chem., 2009, 635: 1848-1855
|
[55] | Zhu S B, Xu T G, Fu H B, Zhao J C, Zhu Y F. Environ. Sci. Technol., 2007, 41: 6234-6239
|
[56] | Li Y Y, Liu J P, Huang X T, Yu J G. Dalton Trans., 2010, 39: 3420-3425
|
[57] | Sonawane R S, Dongare M K. J. Mol. Catal. A: Chem., 2006, 243: 68-76
|
[58] | Zhang L S, Wong K H, Chen Z G, Yu J C, Zhao J C, Hu C, Chan C Y, Wong P K. Appl. Catal., 2009, 363: 221-229
|
[59] | Duan F, Zheng Y, Chen M Q. Appl. Surf. Sci., 2011, 257: 1972-1978
|
[60] | Shi R, Huang G L, Lin J, Zhu Y F. J. Phys. Chem. C, 2009, 113: 19633-19638
|
[61] | Shang M, Wang W Z, Zhang L, Xu H L. Mater. Chem. Phys., 2010, 120: 155-159
|
[62] | Zhang Z J, Wang W Z, Gao E P, Shang M, Xu J H. J. Hazard. Mater., 2011, 196: 255-262
|
[63] | Shang M, Wang W Z, Zhang L, Sun S M, Wang L, Zhou L. J. Phys. Chem. C, 2009, 113: 14727-14731
|
Full-Text
|
|
Contact Us
service@oalib.com QQ:3279437679 
WhatsApp +8615387084133
|
|