锂离子电池富锂过渡金属氧化物xLi2MnO3·(1-x)LiMO2(M=Ni,Co或Mn)正极材料
DOI: 10.7536/PC130767, PP. 259-269
Keywords: 锂离子电池,正极材料,过渡金属氧化物,高容量,合成方法
Abstract:
作为下一代高比能锂离子电池正极材料的有力竞争者,富锂过渡金属氧化物xLi2MnO3·(1-x)LiMO2(M=Ni,Co或Mn)相对于传统的锂离子电池正极材料而言,具有比容量高的显著优势(可超过300mAh/g),因此近年来得到了广泛关注。本文对富锂过渡金属氧化物xLi2MnO3·(1-x)LiMO2(M=Ni,Co或Mn)近几年的研究进展进行了总结,对该类材料的晶体结构特征以及首次充放电机理、不同合成方法的发展以及电化学性能的改善进行了评述,并对这类材料今后的发展方向提出了思考。
References
[1] | Nagaura T, Tozawa K. Pro. Batteries Solar Cells, 1990, 9: 209.
|
[2] | 张临超(Zhang L C), 陈春华(Cheng C H). 化学进展(Prog. Chem.), 2011, 23(2/3): 275.
|
[3] | Sun Y K, Myung S T, Bang H J, Park B C, Park S J, Sung N Y. J. Electrochem. Soc., 2007, 154: A937.
|
[4] | Amriou T, Khelifa B, Aourag H, Aouadi S M, Mathieu C. Mater. Chem. Phys., 2005, 92: 499.
|
[5] | Liu H, Yang Y, Zhang J. J. Power Sources, 2007, 173: 556.
|
[6] | Macneil D D, Lu Z H, Dahn J R. J. Power Sources, 2002, 108: 8.
|
[7] | Stoyanova R, Zhecheva E, Alcantara R, Tirado J L, Bromiley G, Bromiley F, Ballaran T B. Solid State Ionics, 2003, 161: 197.
|
[8] | Whittingham M S. Chem. Rev., 2004, 104(10): 4271.
|
[9] | Johnson C S, Kim J S, Leef C, Li N, Vaughey J T, Thackeray M M. Electrochem. Commun., 2004, 6: 1085.
|
[10] | Wu Y, Manthiram A. Electrochem. Solid-State Lett., 2006, 9: A221.
|
[11] | Jarvis K A, Deng Z Q, Allard L F, Manthiram A, Ferreira P, Chem. Mater., 2011, 23: 3614.
|
[12] | Pan C J, Lee Y J, Ammundsen B, Grey C P. Chem. Mater., 2002, 14: 2289.
|
[13] | Bréger J, Jiang M, Dupré N, Meng Y S, Shao-Horn Y, Ceder G, Grey C P. J. Solid State Chem., 2005, 178: 2575.
|
[14] | Yoon W S, Kim N, Yang X Q, McBreen J, Grey C P. J. Power Sources, 2003, 119/121: 649.
|
[15] | Park Y J, Hong Y S, Wu X L, Kim M G, Ryu K S, Chang S H. J. Electrochem. Soc., 2004, 151: A720.
|
[16] | Kim J S, Johnson C S, Vaughey J T, Thackeray M M. Chem. Mater., 2004, 16: 1996.
|
[17] | Croy J R, Kang S H, Balasubramanian M, Thackeray M M. Electrochem. Commun., 2011, 13: 1063.
|
[18] | Saint J A, Doeff M M, Reed J. J. Power Sources, 2007, 172: 189.
|
[19] | Guo X J, Li Y X, Zheng M, Zheng J M, Li J, Gong Z L, Yang Y. J. Power Sources, 2008, 184: 414.
|
[20] | Lu Z H, Beaulieu L Y, Donaberger R A, Thomas C L, Dahn J R. J. Electrochem. Soc., 2002, 149: A778.
|
[21] | Robertson A D, Bruce P G. Chem. Commun., 2002, 2790.
|
[22] | Benedek R, Thackeray M M, Walle A. Chem. Mater., 2008, 20: 5485.
|
[23] | Yoon W S, Grey C P, Balasubramanian M, Yang X Q, Fischer D A, McBreen J. Electrochem. Solid-State Lett., 2004, 7: A53.
|
[24] | Yu D Y W, Yanagida K, Kato Y, Nakamura H. J. Electrochem. Soc., 2009, 156: A417.
|
[25] | Armstrong A R, Robertson A D, Bruce P G. J. Power Sources, 2005, 146: 275.
|
[26] | Zheng J M, Wu X B, Yang Y. Electrochimi. Acta, 2011, 56: 3071.
|
[27] | 王昭(Wang Z), 吴锋(Wu F), 苏岳锋(SuY F), 包丽颖(Bao L Y), 陈来(Chen L), 李宁(Li N), 陈实(Chen S). 物理化学学报(Acta Phys. -Chim. Sin.), 2012, 28(4): 823.
|
[28] | 杜柯(Du K), 周伟瑛(Zhou W Y), 胡国荣(Hu G R). 化学学报(Acta Chimica Sinica), 2010, 68: 1391.
|
[29] | Yu C, Guan X F, Li G S, Zheng J, Li L P. Scr. Mater., 2012, 66: 300.
|
[30] | West W C, Soler J, Ratnakumar B V. J. Power Sources, 2012, 204: 200.
|
[31] | Kim M G, Jo M, Hong Y S, Cho J. Chem. Commun., 2009, 2: 218.
|
[32] | Park S H, Sun Y K. J. Power Sources, 2003, 119: 161.
|
[33] | Jiao L F, Zhang M, Yuan H T, Zhao M, Guo H, Wang W, Di Zhou X, Wang M. J. Power Sources, 2007, 167: 178.
|
[34] | Lian F, Gao M, Qiu W H, Axmann P, Wohlfahrt-Mehrens M. J. Appl. Electrochem., 2012, 42: 409.
|
[35] | Wu Y, Manthiram A. Solid State Ionics, 2009, 180: 50.
|
[36] | Wang Q Y, Liu J, Mueugan A V, Manthiram A. J. Mater. Chem., 2009, 19: 4965.
|
[37] | Liu J, Reeja-Jayan B, Manthiram A. J. Phys. Chem. C, 2010, 114: 9528.
|
[38] | Liu J, Wang Q, Reeja-Jayan B, Manthiram A. Electrochem. Commun., 2010, 12: 750.
|
[39] | Lu Z, MacNeil D D, Dahn J R. Electrochem. Solid-State Lett., 2001, 4: A200.
|
[40] | MacNeil D, Lu Z, Dahn J R. J. Electrochem. Soc., 2002, 149: A1332.
|
[41] | Rougier A, Bravereau P, Delmas C. J. Electrochem. Soc., 1996, 143(4): 1168.
|
[42] | Liu Z L, Yu A S, Lee J Y. J. Power Sources, 1999, 81/82: 416.
|
[43] | Kim G H, Kim J H, Myung S T, Yoon C S, Sun Y K. J. Electrochem. Soc., 2005, 152: A1707.
|
[44] | Lu W, Belharouak I, Vissers D, Amine K. J. Electrochem. Soc., 2006, 153: A2147.
|
[45] | Myung S T, Komaba S, Hosoya K, Miura Y, Hirosaki N, Kumagai N. Chem. Mater., 2005, 17: 2427.
|
[46] | Johnson C S, Li N, Leef C, Thackeray M M. Electrochem. Commun., 2007, 9: 787.
|
[47] | Thackeray M M, Kang S H, Johnson C S, Vaughey J T, Hackney S A. Electrochem. Commun., 2006, 8: 1531.
|
[48] | Ammundsen B, Paulsen J, Davidson I, Liu R S, Shen C H, Chen J M, Jang L Y, Lee J F. J. Electrochem. Soc., 2002, 149 (4): A431.
|
[49] | Park Y J, Wu X L. Solid State Ionics, 2004, 175: 305.
|
[50] | Thackeray M M, Kang S H, Johnson C S, Vaughey J T, Benedek R, Hackney S A. J. Mater. Chem., 2007, 17: 3112.
|
[51] | Lu Z H, Dahn J R. J. Electrochem. Soc., 2002, 149: A815.
|
[52] | Bare?o J, Lei C H, Wen J G, Kang S H, Petrov I, Abraham D P. Adv. Mater., 2010, 22: 1122.
|
[53] | Yoon W S, Iannopollo S, Grey C P, Carlier D, Gorman J, Reed J, Ceder G. Electrochem. Solid-State Lett., 2004, 7 (7): A167.
|
[54] | Yu L Y, Qiu W H, Lian F, Liu W, Kang X L, Huang J Y. Mater. Lett., 2008, 62: 3010.
|
[55] | Lu Z H, Chen Z H, Dahn J R. Chem. Mater., 2003, 15: 3214.
|
[56] | Koyama K, Tanaka I, Nagao M, Kanno R. J. Power Sources, 2009, 189: 798.
|
[57] | Lim J H, Bang H, Lee K S, Amine K, Sun Y K. J. Power Sources, 2009, 189: 571.
|
[58] | Armstrong A R, Holzapfel M, Novák P, Johnson C S, Kang S H, Thackeray M M, Bruce P G. J. Am. Chem. Soc., 2006, 128: 8694.
|
[59] | Kikkawa J, Akita T, Tabuchi M, Shikano M, Tatsumi K, Kohyama M. Electrochem. Solid-State Lett., 2008, 11: A183.
|
[60] | Kubota K, Kaneko T, Hirayama M, Yonemura M, Imanari Y, Nakane K, Kanno R. J. Power Sources, 2012, 216: 249.
|
[61] | Xiao R J, Li H, Chen L Q. Chem. Mater., 2012, 24: 4242.
|
[62] | Gong Z L, Liu H S, Guo X J, Zhang Z R, Yang Y. J. Power Sources, 2004, 136: 139.
|
[63] | Santhanam R, Rambabu B. J. Power Sources, 2010, 195: 4313.
|
[64] | Zheng J M, Wu X B, Yang Y. Electrochim. Acta, 2011, 56: 3071.
|
[65] | Li J, Kl?psch R, Stan M C, Nowak S, Kunze M, Winter M, Passerini S. J. Power Sources, 2011, 196: 4821.
|
[66] | Xiang X D, Li X Q, Li W S. J. Power Sources, 2013, 230: 89.
|
[67] | Yu L Y, Qiu W H, Lian F, Huang J Y, Kang X L. J. Alloys and Compounds, 2009, 471: 317.
|
[68] | Kim G Y, Yi S B, Park Y J, Kim H G. Mater. Res. Bull., 2008, 43: 3543.
|
[69] | Wei X, Zhang S C, He L, Liu G R, Yang P H. Int. J. Electrochem. Sci., 2013, 8: 1885.
|
[70] | Bai Y, Wang F, Wu F, Wu C, Bao L Y. Electrochimica Acta, 2008, 54: 322.
|
[71] | Gao J, Manthiram A. J. Power Sources, 2009, 191: 644.
|
[72] | Zheng J M, Li J, Zhang Z R, Guo X J, Yang Y. Solid State Ionics, 2008, 179: 1794.
|
[73] | Kang S H, Thackeray M M. Electrochem. Commun., 2009, 11: 748.
|
[74] | Wu F, Li N, Su Y F, Lu H Q, Zhang L J, An R, Wang Z, Bao L Y, Chen S. J. Mater. Chem., 2012, 22: 1489.
|
[75] | Gao J, Kim J, Manthiram A. Electrochem. Commun., 2009, 11: 84.
|
[76] | Gao J, Manthiram A. J. Power Sources, 2009, 191: 644.
|
[77] | Wei G Z, Lu X, Ke F S, Huang L, Li J T, Wang Z X, Zhou Z Y, Sun S G. Adv. Mater., 2010, 22: 4364.
|
[78] | Lin J, Mu D B, Jin Y, Wu B R, Ma Y F, Wu F. J. Power Sources, 2013, 230: 76.
|
[79] | Wang D, Belharouak I, Zhou G W, Amine K. Adv. Funct. Mater., 2013, 23: 1070.
|
[80] | 吴锋(Wu F), 陈实(Chen S), 仲云霞(Zhong Y X), 白莹(Bai Y), 吴川(Wu C), 包丽颖(Bao L Y), 吴伯荣(Wu B R). CN102655232A, 2012年.
|
Full-Text
|
|
Contact Us
service@oalib.com QQ:3279437679 
WhatsApp +8615387084133
|
|