水热法合成的介孔二氧化钛的结构表征及其对水中2,4,6-三溴苯酚的光催化降解活性
DOI: 10.1016/S1872-2067(10)60241-0, PP. 1349-1356
Keywords: 介孔二氧化钛,水热合成,结构表征,光催化活性,2,4,6-三溴苯酚
Abstract:
?以聚丙二醇(PPG)为模板剂,采用水热法制备了可控介孔TiO2纳米晶体.醋酸水溶液为水解抑制剂和催化剂.运用X射线衍射、热重分析、扫描电镜和氮气吸附-脱附等技术对样品进行了表征.详细考察了制备过程、模板剂含量和煅烧温度等参数对样品结构和光催化活性的影响,并将样品用于紫外光下降解水体中典型溴代阻燃剂2,4,6-三溴苯酚的反应中,阐明制备的介孔TiO2结构与光催化活性之间的关系.结果表明,所制样品为具有规则孔道结构、较大的孔径和较高比表面积的介孔TiO2.其中,在400°C煅烧、PPG添加量为20%时所得介孔TiO2的光催化活性最高,反应1h可将100umol/L的2,4,6-三溴苯酚完全降解.
References
[1] | Yuan S, Sheng Q R, Zhang J L, Yamashita H, He D N. Micro-porous Mesoporous Mater, 2008, 110: 501
|
[2] | Zhao D, Huo Q, Feng J, Chmelka B F, Stucky G D. J Am Chem Soc, 1998, 120: 6024
|
[3] | Luan Z, Cheng C, Zhou W, Klinowski J. J Phys Chem, 1995, 99: 1018
|
[4] | Lim M H, Blanford C F, Stein A. J Am Chem Soc, 1997, 119: 4090
|
[5] | Yang H, Coombs N, Ozin G A. Nature, 1997, 386: 692
|
[6] | Antonelli D, M Y J Y. Angew Chem, Int Ed, 1995, 34: 2014
|
[7] | Sertchook H, Elimelech H, Makarov C, Khalfin R, Cohen Y, Shuster M, Babonneau F, Avnir D. J Am Chem Soc, 2007, 129: 98
|
[8] | Hirashima H, Imai H, Balek V. J Non-Cryst Solids, 2001, 285: 96
|
[9] | Liu J K, An T C, Li G Y, Bao N Z, Sheng G Y, Fu J M. Microporous Mesoporous Mater, 2009, 124: 197
|
[10] | Li Y J, Ma M Y, Wang X H, Li Z P. Surf Coat Technol, 2010, 204: 1353
|
[11] | Sing K S W, Everett D H, Haul R A W, Moscou L, Pierotti R A, Rouquerol J, Siemieniewska T. Pure Appl Chem, 1985, 57: 603
|
[12] | an J H, Dou H Q, Xiong Z G, Xu C, Ma J Z, Zhao X S. J Mater Chem, 2010, 20: 4512
|
[13] | n T C, Sun L, Li G Y, Gao Y P, Ying G G. Appl Catal B, 2011, 102: 140
|
[14] | heng Q R, Yuan S, Zhang J L, Chen F. Microporous Mesoporous Mater, 2006, 87:177
|
[15] | ang X C, Yu J C, Ho C M, Hou Y D, Fu X Z. Langmuir, 2005, 21: 2552
|
[16] | u J G, Su Y R, Cheng B. Adv Funct Mater, 2007, 17: 1984
|
[17] | eng T Y, Zhao D, Dai K, Shi W, Hirao K. J Phys Chem B, 2005, 109: 4947
|
[18] | aguchi A, Schuth F. Microporous Mesoporous Mater, 2005, 77: 1
|
[19] | un L, An T C, Wan S G, Li G Y, Bao N Z, Hu X H, Fu J M, Sheng G Y. Sep Purif Technol, 2009, 68: 83
|
[20] | u J G, Yu J C, Leung M K P, Ho W K, Cheng B, Zhao X J, Zhao J C. J Catal, 2003, 217: 69
|
[21] | An T C, Liu J K, Li G Y, Zhang S Q, Zhao H J, Zeng X Y, Sheng G Y, Fu J M. Appl Catal A, 2008, 350: 237
|
[22] | Choi H, Sofranko A C, Dionysiou D D. Adv Funct Mater, 2006, 16: 1067
|
[23] | Yu J G, Zhang L J, Cheng B, Su Y R. J Phys Chem C, 2007, 111: 10582
|
[24] | Fei H L, Liu Y P, Li Y P, Sun P C, Yuan Z Y, Li B H, Ding D T, Chen T H. Microporous Mesoporous Mater, 2007, 102: 318
|
[25] | Drisko G L, Luca V, Sizgek E, Scales N, Caruso R A. Langmuir, 2009, 25: 5286
|
[26] | Kulkarni D G., Murugan A V, Viswanath A K, Gopinath C S. J Nanosci Nanotechnol, 2009, 9: 371
|
[27] | Mohammadi M R, Fray D J, Cordero-Cabrera M C. Sensor Actuat B, 2007, 124: 74
|
[28] | Zhou J F, Zhou M F, Caruso R A. Langmuir, 2006, 22: 3332
|
[29] | Mokaya R, Zhou W Z, Jones W. Chem Commun, 1999: 51
|
[30] | Zhang M L, An T C, Hu X H, Wang C, Sheng G Y, Fu J M. Appl Catal A, 2004, 260: 215
|
[31] | Klug H P, Alexander L E. New York: Wiley, 1974. 618
|
[32] | Ding X J, An T C, Li G Y, Zhang S Q, Chen J X, Yuan J M, Zhao H J, Chen H, Sheng G Y, Fu J M. J Colloid Interf Sci, 2008, 320: 501
|
[33] | Kruk M, Jaroniec M. Chem Mater, 2001, 13: 3169
|
Full-Text
|
|
Contact Us
service@oalib.com QQ:3279437679 
WhatsApp +8615387084133
|
|