镍基合金740H的组织结构与析出相分析

DOI: 10.13334/j.0258-8013.pcsee.2015.17.019, PP. 4439-4444

Keywords: 镍基高温合金,740,740H,时效,组织结构,析出相

Full-Text   Cite this paper   Add to My Lib

Abstract:

分析了镍基合金740H在不同状态下的组织结构和析出相的种类及其对室温硬度和冲击韧性的影响。供货态镍基合金740H晶内含TiN和(Nb,Ti)C颗粒,晶界分布一些M23C6颗粒;经800℃×16h标准热处理后,晶内析出细小γ'颗粒,晶界析出少量碳化物;硬度明显提高,冲击韧性显著降低,分别为304HB和37.5J/cm2。时效后,γ'相尺寸呈逐步增大趋势且与基体保持共格关系,晶界碳化物数量明显增多。750℃下时效300~3000h过程中硬度和韧性的变化范围分别为323~331HB和25~35J/cm2,时效态740H韧性的稳定性高于740合金。

References

[1]  Rösler J,Götting M,Del Genovese D,et al.Wrought Ni-base superalloys for steam turbine applications beyond 700 ℃[J].Advanced Engineering Materials,2003,5(7):469-483.
[2]  Saunders S R J,Monteiro M,Rizzo F,et al.The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour:A review[J].Progress in Materials Science,2008,53(5):775-837.
[3]  Maile K.Use of advanced alloy 617 mod for critical components of the future 700 ℃ coal fired power plant[C]//2009 Symposium on Advanced Power Plant Heat Resistant Steels and Alloys.Shanghai,China,2009.
[4]  Klöwer J,Husemann R U,Bader M,et al.Development of nickel based on alloy 617 for components in 700 ℃ power plants[J]. Procedia Engineering,2013,55(4):226-231.
[5]  Gariboldi E,Cabibbo M,Spigarelli S,et al.Investigation on precipitation phenomena of Ni-22Cr-12Co-9Mo alloy aged and crept at high temperature[J].International Journal of Pressure Vessels and Piping,2008,85(1-2):63-71.
[6]  Guo Y,Wang B H,Hou S F.Aging precipitation behavior and mechanical properties of Inconel 617 superalloy[J].Acta Metallurgica Sinica(English Letters),2013,26(3):307-312.
[7]  郭岩,周荣灿,侯淑芳,等.617合金760 ℃时效组织结构及力学性能分析[J].中国电机工程学报,2010,30(26):86-89. Guo Yan,Zhou Rongcan,Hou Shufang,et al.Analysis of microstructure and mechanical properties of alloy 617 aged at 760 ℃[J].Proceedings of the CSEE,2010,30(26):86-89(in Chinese).
[8]  郭宏钢,王岩,李阳.617 B镍基高温合金铸态组织热变形行为研究[J].热加工工艺,2013,42(24):51-53. Guo Honggang,Wang Yan,Li Yang.Research on hot deformation behavior of as-cast structure of 617 B nickel-base superalloy[J].Hot Working Technology,2013,42(24):51-53(in Chinese).
[9]  江勇,赵双群,李维银.改进型Inconel 740镍基合金在模拟煤灰和烟气环境中的腐蚀行为[J].机械工程材料,2008,32(12):29-32,43. Jiang Yong,Zhao Shuangqun,Li Weiyin.Corrosion behavior of modified Ni based alloy Inconel 740 in simulated coal-ash/flue-gas environments[J].Materials for Mechanical Engineering,2008,32(12):29-32,43(in Chinese).
[10]  符锐,林福生,赵双群,等.Inconel 740 H主要强化元素对热力学平衡相析出行为的影响[J].动力工程学报,2013,33(5):405-412. Fu Rui,Lin Fusheng,Zhao Shuangqun,et al.Influence of strengthening elements on precipitation of thermodynamic equilibrium phases in Inconel alloy 740 H[J].Journal of Chinese Society of Power Engineering,2013,33(5):405-412(in Chinese).
[11]  Wu Q.Microstructural characterization of advanced boiler materials for ultra supercritical coal power plants[C]//Proceedings to the Fourth International Conference on Advances in Materials Technology for Fossil Power Plants.Materials Park,OH:ASM-International,2005.
[12]  Patel S J.Introduction to Inconel Alloy 740:an alloy designed for superheater tubing in coal-fired ultra supercritical boilers[J].Acta Metallurgica Sinica(English Letters),2005,18(4):479-488.
[13]  Evans N D,Maziasz P J,Swindeman R W,et al.Microstructure and phase stability in INCONEL alloy 740 during creep[J].Scripta Materialia,2004,51(6):503-507.
[14]  Zhao S Q,Xie X S,Smith G D,et al.Research and improvement on structure stability and corrosion resistance of nickel-base superalloy INCONEL alloy 740[J].Materials and Design,2006,27(10):1120-1127.
[15]  赵双群,谢锡善.一种新型镍基高温合金长期时效后的组织和性能[J].金属学报,2003,39(4):399-404. Zhao Shuangqun,Xie Xishan.Properties and microstructure after long-term aging at different temperatures for a new nickel base superalloy[J].Acta Metallurgica Sinica,2003,39(4):399-404(in Chinese).
[16]  张红军,周荣灿,侯淑芳,等.先进超超临界机组用Inconel 740合金的组织稳定性研究[J].中国电机工程学报,2011,31(8):108-113. Zhang Hongjun,Zhou Rongcan,Hou Shufang,et al.Study on microstructure stability of Inconel 740 for advanced ultra supercritical unit[J].Proceedings of the CSEE,2011,31(8):108-113(in Chinese).
[17]  赵双群,谢锡善.超超临界锅炉过热器管材的高温组织稳定性及其改进研究[J].材料导报,2004,18(8):131-133. Zhao Shuangqun,Xie Xishan.High temperature structure stability and its improvement on superheater tube material for ultra-supercritical boilers[J].Materials Review,2004,18(8):131-133(in Chinese).
[18]  谢锡善,赵双群,董建新,等.超超临界电站用 Inconel 740镍基合金的组织稳定性及其改型研究[J].动力工程学报,2011,31(8):638-643. Xie Xishan,Zhao Shuangqun,Dong Jianxin,et al.Structural stability and improvement of Inconel alloy 740 for ultra supercritical power plants[J].Journal of Chinese Society of Power Engineering,2011,31(8):638-643(in Chinese).
[19]  赵双群,张麦仓,董建新,等.新型高温合金700 ℃时效组织及力学性能[J].稀有金属材料与工程,2003,32(12):991-994. Zhao Shuangqun,Zhang Maicang,Dong Jianxin,et al.Mechanical properties and structure of new superalloys after prolonged aging at 700 ℃[J].Rare Metal Materials and Engineering,2003,32(12):991-994(in Chinese).
[20]  赵双群,谢锡善,董建新.Inconel 740合金在空气和含有水蒸气的空气中的氧化研究[J].动力工程学报,2011,31(10):797-802.Zhao Shuangqun,Xie Xishan,Dong Jianxin.Oxidation resistance of Inconel 740 in static air or air-steam mixture[J].Journal of Chinese Society of Power Engineering,2011,31(10):797-802(in Chinese).

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133