油气田CO2/H2S共存条件下的腐蚀研究进展与选材原则

, PP. 401-405

Keywords: CO2/H2S腐蚀,腐蚀机理,选材原则

Full-Text   Cite this paper   Add to My Lib

Abstract:

综述了CO2/H2S共存条件下的腐蚀机理、其影响因素和国内外CO2/H2S腐蚀的研究现状与趋势,提出了CO2/H2S共存时的选材要求及原则,展望了对CO2/H2S腐蚀的研究重点和抗CO2/H2S腐蚀钢的研发方向.

References

[1]  Pots B F M,John R C,Rippon I J,et al.Improvements on de waardmilliams corrosion prediction and applications to corrosion management[J].Corrosion/2002.Houston:NACE,2002,Paper No.02235.
[2]  Omar I H,Gunaltun Y M,Kvarekval J,et al.H2S corrosion of carbon steel under simulated kashagan field conditions[J].Corrosion/2005.Houston:NACE,2005,Paper No.05300.
[3]  NACE MR01752001,Sulfide stress cracking resistant metallic materials for oilfield equipment[S].[37]NACE TM01772005,Laboratory testing of metals for resistance to sulphide stress cracking and stress corrosion cracking in H2S environments[S].
[4]  NACE TM02842003,Evaluation of pipeline and pressure vessel steels for resistance to hydrogen induced cracking[S].
[5]  EFC Publications No.16,Guidelines on materials requirements for carbon and low alloy steels for H2Scontaining environments in oil and gas production[S].
[6]  EFC Publications No.17,Corrosion resistant alloys for oil and gas production:Guidelines on general requirements and test methods for H2S service[S].
[7]  ISO 151561:2001,Petroleum and natural gas industriesMaterials for use in H2Scontaining environments in oil and gas productionPart1:General principles for selection of crackingresistant materials[S].
[8]  ISO 151562:2003,Petroleum and natural gas industriesMaterials for use in H2Scontaining environments in oil and gas productionPart2:Crackingresistant carbon and low alloy steels,and the use of irons[S].
[9]  ISO 151563:2003,Petroleum and natural gas industriesMaterials for use in H2Scontaining environments in oil and gas productionPart3:Crackingresistant CRAs(corrosionresistant alloys)and other alloys[S].
[10]  张忠铧,郭金宝,蔡海燕,等.经济型抗CO2、H2S腐蚀油套管的开发[J].试验与研究,2004,33(5):18.
[11]  植田昌克,Ueda M.合金元素和显微结构对CO2/H2S环境中腐蚀产物稳定性的影响[J].石油与天然气化工,2005,34(1):43.
[12]  Klein L J,Thompson R M,Moore D E.9CrlMo and 13Cr tubules for sour service[J].Corrosion/1990.Houston:NACE,1990,Paper No.52.
[13]  Kermanin B J,Martin J,Esaklul K,et al.Materials design strategy:Effects of H2S/CO2 corrosion on materials selection[J].Corrosion/2006.Houston:NACE,2006,Paper No.06121.
[14]  Kimura M,Sakata K,Shimamoto K,et al.SCC performance of martensitic stainless steel OCTG in packer fluid[J].Corrosion/2006.Houston:NACE,2006,Paper No.06137.
[15]  BBolmer P W.Polarization of iron in H2S NaHS buffer[J].Corrosion,1965,21(3):69.
[16]  白白真权,李鹤林,刘道新,等.模拟油田H2S/CO2环境中N80钢的腐蚀及影响因素研究[J].材料保护,2003,36(4):32.
[17]  PPots B F M,John R C.Improvement on De WaardMilliams corrosion prediction and application to corrosion management[J].Corrosion/2002.Houston:NACE,2002,Paper No.02235.
[18]  AAgrawal A K,Durr C,Koch G H.Sulfide films and corrosion rates of AISI1018 carbon steel in saline solutions in the presence of H2S and CO2 at temperature up to 175°F[J].Corrosion/2004.Houston:NACE,2004,Paper No.04383.
[19]  KKvarekval J,Nyborg R,Seiersten M.Corrosion product films on carbon steel in semisour CO2/H2S environments[J].Corrosion/2002.Houston:NACE,2002,Paper No.02296.
[20]  HHausler R H,Stegman D W,Tjandroso D.Parametric study on the effect of H2S,condensate,metallurgy,and flowrate[J].Corrosion/1990.Houston:NACE,1990,Paper No.6.
[21]  SSmith S N,Pacheco J L.Prediction of corrosion in slightly sour environments[J].Corrosiou/2002.Houston:NACE,2002,Paper No.02241.
[22]  姜姜放,戴海黔,曹小燕,等.油套管在CO2和H2S共存时的腐蚀机理研究[J].石油与天然气化工,2005,34(3):213.[9]Dugstad A.Mechanism of protective film formation during CO2 corrosion of carbon steel[J].Corrosion/1998[C].Houston:NACE,1998,Paper No.31.
[23]  Hunnik E W J V,Pots B F M,Hendriksen E L J A,et al.The formation of protective FeCO3 corrosion product layers in CO2 corrosion[J].Corrosion/1996.Houston:NACE,1996,Paper No.6.
[24]  Nyborg R.Initiation and growth of mesa corrosion attack during CO2 corrosion of carbon steel[J].Corrosion/1998.Houston:NACE,1998,Paper No.48.
[25]  Kvarekval J,Nyborg R,Choi H,et al.Formation of multilayer iron sulfide films during high temperature CO2/H2S corrosion of carbon steel[J].Corrosion/2003.Houston:NACE,2003,Paper No.03339.
[26]  Ueda M.Effect of alloying elements and microstructure on stability of corrosion product in CO2 and/or H2S environments[J].Chemical Engineering of Oil and Gas,2005,34(1):43.
[27]  Smith J S,Miller J D A.Nature of sulfides and their corrosive effect on ferrous metals[J].A Review,British Corrosion Journal,1975,10(3):136.
[28]  Morse J W,Millero F J,Cornwell J C,et al.The chemistry of the hydrogen sulfide and iron sulfide systems in natural waters[J].Earth-Science Reviews,1987,24(1):1.
[29]  Sun W,Nesic S,Papavinasam S.Kinetics of iron sulfide and mixed iron sulfide/carbonate scale precipitation in CO2/H2S corrosion[J].Corrosion/2006.Houston:NACE,2006,Paper No.06644 
[30]  白真权,任呈强,刘道新.N80钢在CO2/H2S高温高压环境中的腐蚀行为[J].石油机械,2004,32(12):16.[18]李萍.90℃时油管钢P110的CO2/H2S腐蚀行为[J].全面腐蚀控制,2006,20(2):23. [19]Brown B,Parakala S R,Nesic S.CO2 corrosion in the presence of trace amounts of H2S[J].Corrosion/2004.Houston:NACE,2004,Paper No.04736.
[31]  《油气田腐蚀与防护技术手册》编委会.油气田腐蚀与防护技术手册(下册)[M].北京:石油工业出版社,1999.471.
[32]  Ramanarayanan T A,Smith S N.Corrosion of iron in gaseous environments and in gas-saturated aqueous environments[J].Corrosion,1990,46(1):66.
[33]  张清,李全安,文九巴,等.CO2分压对油管钢CO2/H2S腐蚀的影响[J].钢铁研究学报,2004,16(4):72.
[34]  周计明.油管钢在含CO2/H2S高温高压水介质中的腐蚀行为及防护技术的作用[D].西安:西北工业大学,2002.28.
[35]  MoraMendoza J L,ChaconNava J G,ZavalaOlivares G,et al.Influence of turbulent flow on the localized corrosion processes of mild steel with inhibited aqueous CO2 systems[J].Corrosion,2002,58(7):608.
[36]  Abayarathna D,Naraghi A,Wang S H.The effect of surface films on corrosion of carbon steel in a CO2-H2S-H2O System[J].Corrosion/2005.Houston:NACE,2005,Paper No.05624.
[37]  Ikeda A,Ueda M,Mukai S,et al.Influence of environmental factors on corrosion in CO2 source well[J].Corrosion/1985.Houston:NACE,paper No 29.
[38]  李国敏.碳钢在含硫化氢及高压二氧化碳饱和的NaCl溶液中的腐蚀行为[J].中国腐蚀与防护学报,2000,20(4):204.
[39]  张学元,邸超,雷良才.二氧化碳腐蚀与控制[M].北京:化学工业出版社,2000.15.
[40]  Dugstad A,Lunde L.Parametric study of CO2 corrosion of carbon steel[J].Corrosion/1994.Houston:NACE,1994,Paper No.94014.
[41]  Bich N N,Goerz K.Caroline pipeline failure:Findings on corrosion mechanisms in wet sour gas systems containing significant CO2[J].Corrosion/1996.Houston:NACE,1996,Paper No.26.
[42]  Hoffmeister H.Modeling the effect of chloride content on H2S corrosion by coupling of phase and polarization behavior[J].Corrosion/2007.Houston:NACE,2007,Paper No.07501.
[43]  Vitale D D.Effect of hydrogen sulfide partial pressure,pH and chloride content on the SSC resistance of martensitic stainless steels and martensitic precipitation hardening stainless steels[J].Corrosion/1999.Houston,1999,Paper No.584.
[44]  Salih S A,Mazhar A A,Mahanny H.The effect of sour gases and some anions on the corrosion behavior of carbon steel[J].Portugaliae Electrochimica Acta,2004,22(3):205.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133