纯Fe在含KCl蒸汽的O2气氛中的高温腐蚀行为
, PP. 20-23
Keywords: Fe,KCl,高温氧化,腐蚀
Abstract:
研究了纯Fe在含有KCl蒸汽的O2中于650℃~850℃的腐蚀行为,结果表明,纯Fe在试验条件下发生了加速腐蚀,并且随温度的提高和KCl蒸气浓度的增大,腐蚀速率均增高.微量的KCl蒸气起加速腐蚀作用,主要是通过与试样表面的氧化膜反应生成Cl2,而Cl2能渗透到基体界面处与基体生成挥发性的Fe的氯化物实现的.〖HT5”H〗中图分类号〖HT5”SS〗〓〓〖
References
[1] | YonghuaShu,FuhuiWang,WeitaoWu.SynergisticeffectofNaClandwatervaporonthecorrosionof1Cr-11Ni-2W -2Mo-Vsteelat500-700°C [J].Oxid.Metals,1999,51(1):463.
|
[2] | MHara,HOkumura,YKitagawa,YSato,YShinata.Effectofpre-oxidationonhotcorrosionofNi-Cr-AlalloyinmoltenNa2SO4-NaCl[J].J.JapanInst.Metals,1995,59(12):1259.
|
[3] | YSato,MHara,YShinata.Effectofasmallamountofhydrogenchlorideonhightemperatureoxidationofpureiron[J].J .JapanInst.Metals,1994,58(6):654.
|
[4] | TakemuraM ,McNallanMJ.Environmentaleffectsonmoltenchloridesacceleratedcorrosioninwasteincinerationsystems[A].CORROSION/95,paperNo.568,(Houston,TX :NACEInternational,1995)
|
[5] | Y .Shinata,YNishi.NaCl-inducedacceleratedoxidationofchromium[J].Oxid.Metals,1986,26(3-4):201.
|
[6] | AbelsJ ,StrehblowH .AsurfaceanalyticalapproachtothehightemperaturechlorinationbehaviourofInconel600at700℃[J].CorrosionScience,1997,39(1):115.
|
[7] | ChangYN ,WeiFI .High-temperaturechlorinecorrosionofmetalsandalloys[J].J .MaterialSci.,1991,26:3693.
|
[8] | YYLee,MJMcnallan.Ignitionofnickelinenvironmentscontainingoxygenandchlorine[J].MetallurgicalTransactionsA ,1987,18A :1099.
|
[9] | OKubaschewski,CBAlock.MetallugicalThermochemistry[M ],5 thEdition,PergamonPress,1979.376.
|
[10] | 李远士,牛焱,吴维.金属材料的高温氯化腐蚀[J],腐蚀科学与防护技术,2000,12(1):P41.
|
[11] | YSato,DJYoung.High-temperaturecorrosionofironat900℃inatmospherescontainingHClandH2O [J].Oxid.Metals,2001,55(3/4):243.
|