7xxx系列Al合金应力腐蚀开裂的研究
, PP. 218-222
Keywords: 高强Al合金,应力腐蚀开裂,综述
Abstract:
综述了7xxx系列Al合金的应力腐蚀开裂机理和影响应力腐蚀开裂行为的因素,讨论了应力腐蚀开裂过程的微观结构变化及其与应力腐蚀开裂敏感性的关系.在不降低合金力学性能的前提下,提高耐应力腐蚀开裂性将使该系合金有广泛的应用前景.
References
[1] | 〔29〕SarkarB ,MarekM ,StarkeEA .Metall.Trans.A ,1981,12:1939
|
[2] | 〔1〕LiXiaomei,StarinkMJ.Mater.Sci.Forum,2000,331-337:1071
|
[3] | 〔2〕LiuJohn,MichaelKulak.Mater.Sci.Forum,2000,331-337:127
|
[4] | 〔3〕FleckP ,CallerosD ,MadsenM ,etal.Mater.Sci.Forum,2000,331-337:649
|
[5] | 〔4〕AsaroRJ,TillerWA .Metall.Trans.,1972,3:1789
|
[6] | 〔5〕GalveleJR .Corros.Sci.,1987,27:1
|
[7] | 〔6〕SieradzkiK ,FriedersdorfFJ.Corros.Sci.,1994,36:669
|
[8] | 〔7〕HollHA .Corrosion,1967,23:173
|
[9] | 〔8〕DeArdoJrAJ,TownsendRD .Metall.Trans.,1970,1:2573
|
[10] | 〔9〕LandkofM ,Gal-OrL .Corrosion,1980,36:241
|
[11] | 〔10〕GestRJ,TroianoAR .Corrosion,1974,30:274
|
[12] | 〔11〕SpeidelMO .Metall.Trans.A ,1975,6:631
|
[13] | 〔12〕PathaniaRS ,TromansD .Metall.Trans.A ,1981,12:607
|
[14] | 〔13〕ScamansGM ,AlaniR ,SwannPR .Corros.Sci.,1976,16:443
|
[15] | 〔14〕AlbrechtJ,ThompsonAW ,BernsteinIM .Metall.Trans.A ,1979,10:1759
|
[16] | 〔15〕AlbrechtJ,BernsteinIM ,ThompsonAW .Metall.Trans.A ,1982,13:811
|
[17] | 〔16〕HardwickDA ,ThompsonAW ,BernsteinIM .Metall.Trans.A ,1983,14:2517
|
[18] | 〔17〕HardwickDA ,ThompsonAW ,BernsteinIM .Corros.Sci.,1988,28:1127
|
[19] | 〔18〕ScamansGM .Metall.Trans.A ,1980,11:846
|
[20] | 〔19〕NajjarD ,MagninT ,WarnerTJ.Mater.Sci.Eng.A ,1997,238:293
|
[21] | 〔20〕ScullyJR ,YoungJrGA ,SmithSW .Mater.Sci.Forum,2000,331-337:1583
|
[22] | 〔21〕ZuhairMGasem,RichardPGangloff.Mater.Sci.Forum,2000,331-337:1479
|
[23] | 〔22〕WeiRP ,PaoPS ,HartRG ,etal.Metall.Trans.A ,1980,11:151
|
[24] | 〔23〕StanzlSE ,MayerHR ,TscheggEK .Mater.Sci.Eng.A ,1991,147:45
|
[25] | 〔24〕LeeSeong-Min,PyunSu-Il,ChunYoung-Gab.Metall.Trans.A ,1991,22:2407
|
[26] | 〔25〕GongBo,LaiZuhan.Proc.ofICAAII,Beijing,1990.657
|
[27] | 〔26〕SedriksAJ ,GreenJAS ,NovakDL .Corrosion,1971,27:198
|
[28] | 〔27〕HFdeJong.Corrosion,1978,34:32
|
[29] | 〔28〕TsaiW -T ,DuhJ-B ,YehJ -J,etal.Corrosion,1990,46:444
|
[30] | 〔30〕BraunR .Corrosion,1997,53:467
|
[31] | 〔31〕NarasimhaRaoBV .Metall.Trans.A ,1981,12:1356
|
[32] | 〔32〕DoigP ,FlewittPEJ,EdingtonJW .Corrosion,1977,33:217
|
[33] | 〔33〕TsengMei-kuang,LiuJun,JinZhen-hong.Proc.ofICAAII ,Beijing,1990.662
|
[34] | 〔34〕WangLaishen.Proc.ofICAAII ,Beijing,1990.687
|
[35] | 〔35〕CinaB .USPatent3856584,1974
|
[36] | 〔36〕ParkJK ,ArdellAJ .Metall.Trans.A ,1984,15:1531
|
[37] | 〔37〕RajanK ,WallaceW ,BeddoesJC .J .Mater.Sci.,1982,17:2817
|
[38] | 〔38〕PapazianJM .Mater.Sci.Eng.,1986,79:97
|
[39] | 〔39〕KannoM ,ArakiI ,CuiQ .Mater.Sci.Technol.,1994,10:599
|
[40] | 〔40〕RajanK ,WallaceW ,BeddoesJC .J .Mater.Sci.,1982,17:2817
|
[41] | 〔41〕TaliankerM ,CinaB .Metall.Trans.A ,1989,20:2087
|
[42] | 〔42〕GongBo,LaiZuhan.Proc.ofICAAII ,Beijing,1990.657
|
[43] | 〔43〕LinZhaoqi,JiangWenhui,YangShenkun,etal.Proc.ofI CAAII ,Beijing,1990.480
|
[44] | 〔44〕WertJA ,PatonNE ,HamiltonCH ,etal.Metall.Trans.A ,1981,12:1267
|
[45] | 〔45〕TsaiTC ,ChuangTH .Mater.Sci.Eng.A ,1997,225:135
|
[46] | 〔46〕ChristodoulouL ,FlowetHM .ActaMetall.,1980,28:481
|
[47] | 〔47〕YoderGR ,PaoPS ,BaylesRA .Scr.Metall.Mater.,1990,24:2285
|
[48] | 〔48〕PaoPS ,GillSJ,BaylesRA .Scr.Metall.Mater.,1991,25:2085
|
[49] | 〔49〕FemminellaOP ,StarinkMJ,GunnSR ,etal.Mater.Sci.Fo rum,2000,331-337:1255
|
[50] | 〔50〕SenatorovaOG ,UksusnikovAN ,LegoshinaSF ,etal.Mater.Sci.Forum,2000,331-337:1249
|
[51] | 〔51〕MilmanYu.V ,LotskoDV ,SirkoOI.Mater.Sci.Forum,2000,331-337:1107
|
[52] | 〔52〕RiddleYancyW ,SandersJrTH .Mater.Sci.Forum,2000,331-337:799
|
[53] | 〔53〕AdlerPN ,DeisaiR .Metall.Trans.A ,1977,8:1185e
|
Full-Text
|
|
Contact Us
service@oalib.com QQ:3279437679 
WhatsApp +8615387084133
|
|