电解液的浓度和温度对铝空气电池负极性能的影响

, PP. 149-152

Keywords: 极化,电化学阻抗,恒流,Cl-浓度,温度

Full-Text   Cite this paper   Add to My Lib

Abstract:

通过测量极化曲线、电化学阻抗谱和恒流极化曲线,研究了氯离子浓度和溶液温度对铝空气电池负极腐蚀性能和放电性能的影响.结果表明当氯化钠溶液浓度为3.5%时,铝合金腐蚀速率最快,随着氯化钠溶液浓度升高,铝合金恒流极化稳定电位负移,极化减小.溶液温度升高,加快了铝合金的腐蚀.当溶液温度为50℃时,由于铝合金表面有腐蚀产物层的生成,腐蚀速度略有降低.当溶液温度为40℃时,铝合金表现出最低的恒流极化稳定电位.

References

[1]  Han B, Liang G C. Neutral electrolyte aluminum airbattery with open configuration[J]. Rare Met., 2006, 25(6): 360.
[2]  汪振道, 王晓黎, 田芸. 海水铝-空气燃料电池[J]. 电源技术,1997, 21(3): 106.
[3]  Doche M L, Novel C F, Durand R, et al. Characterization of different grades of aluminum anodes for aluminum/air batteries[J].J. Power Sources, 1997, 65(1-2): 197.
[4]  Nestoridi M, Pletcher D, Wood R J K, et al. The study of aluminium anodes for high power density Al/air batteries with brine electrolytes[J]. J. Power Sources., 2008, 178(1): 445.
[5]  EI Shayeb H A, Abd EI Wahab F M, EI Abedin S Z. Role of indium ions on the activation of aluminium[J]. J. Appl.Electrochem., 1999, 29(5): 601.
[6]  EI Shayeb H A, Abd EI Wahab F M, EI Abedin S Z. Electrochemical behaviour of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions containing stannous ions[J]. Corros. Sci., 2001,43(4): 655.
[7]  EI Shayeb H A, Abd EI Wahab F M, EI Abedin S Z. Effect of gallium ions on the electrochemical behaviour of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions[J]. Corros. Sci., 2001,43(4): 643.
[8]  Tang Y G, Lu L B, Roesky H W, et al. The effect of zinc on the aluminum anode of the aluminum-air battery[J]. J. Power Sources,2004, 138(1-2): 313.
[9]  Ezuber H, El-Houd A, El-Shawesh F. A study on the corrosion behavior of aluminum alloys in seawater[J]. Mater. Des., 2008,29(4): 801.
[10]  Mazhar A A, Arab S T, Noor E A. The role of chloride ions and pH in the corrosion and pitting of Al-Si alloys[J]. J. Appl. Electrochem., 2001, 31(10): 1131.
[11]  Nestoridi M, Pletcher D, Wharton J A, et al. Further studies of the anodic dissolution in sodium chloride electrolyte of aluminium alloys containing tin and gallium[J]. J. Power Sources,2009, 193(2): 895.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133