埋地钢质管道的外壁应力腐蚀开裂

DOI: 10.11903/1002.6495.2014.118, PP. 207-210

Keywords: 埋地管道,外壁应力腐蚀开裂,SCC,完整性管理

Full-Text   Cite this paper   Add to My Lib

Abstract:

介绍了SCC裂纹的典型特点、形成条件、检测和预防方法。旨在引起对SCC裂纹的重视,加强在检测过程中对SCC裂纹的识别,为管道完整性管理中识别SCC高敏感区的工作提供理论依据。同时列举了一些控制SCC发生的方法。

References

[1]  David L, Culbertson. Use of intelligent pigs to detect stress corrosion cracking in gas pipelines [A]. Corrosion/96 [C]. Houston, Texas: NACE, 1996, 35
[2]  Xie J, Yazdanfar K, Ikeda K. Unusual corrosion and stress corrosion cracking on a pipeline [A]. Corrosion/2013 [C]. Houston, Texas: NACE, 2013, 2120
[3]  Beavers J A, Johnson J T, Sutherby R L. Materials factors influencing the initiation of near-neutral pH SCC on underground pipelines [A]. 4 th International Pipeline Conference Proceedings [C]. New York: ASME, 2000, 47
[4]  Surkov Y P. Corrosion crack initiation in gas pipelines [J]. Phys. Met. Metall., 1994, 78(1): 102
[5]  Beavers J A, Durr C L, Shademan S S. Mechanistic studies of near-neutral pH SCC on underground pipelines [A]. Proceedings of the 37 th International Symposium on Materials for Resource Recovery and Transport [C]. Montreal: CIM, 1998, 51
[6]  Jack T R, Erno B, Krist K, et al. Generation of near-neutral pH and high pH SCC environment on buried pipelines [A]. Corrosion/2000 [C]. Houston, Texas: NACE, 2000, 362
[7]  ASME B31. 8S-2001, Managing system integrity of gas pipelines [S]
[8]  NACE SP0204-2008, Stress corrosion cracking (SCC) direct assessment methodology [S]
[9]  Parkins R N. A review of stress corrosion cracking of high pressure gas pipelines [A]. Corrosion/2000 [C]. Houston, Texas: NACE, 2000, 363

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133