LLeckie H P,Uhlig H H.Environmental factors affecting the crit-ical potential for pitting in 18-8 stainless steel[J].J Elec-trochem Soc,1966,113:1262.
[2]
PPistorius P C,Burstein G T.Growth of corrosion pits on stain-less steel in chloride solution containing dilute sulphate[J].Cor-ros.Sci.,1992,33:1885.
[3]
RRefaey S A M,Abd El-Rehim S S,Taha F,et al.Inhibition oflocalized corrosion of mild steel by PO43-,CrO42-,MoO42-,andNO2-anions[J].Applied Surface Science,2000,158:190.
FFujioka E,Nishihara H,Aramaki K.The inhibition of pit nucle-ation and growth on the passive surface of iron in a borate buffersolution containing Cl-by oxidizing inhibitors[J].Corros.Sci.,1996,38:1915.
[7]
CCheng Y F,Wilmott M,Luo J L.The role of chloride ions inpitting of carbon steel studied by the statistical anslysis of elec-trochemical noise[J].Applied Surface Science,1999,152:161.
[8]
VVirtanen S,Surber B,Nylund P.Influence of MoO42-anion inthe electrolyte on passivity breakdown of iron[J].Corros.Sci.,2001,43:1165.y