Nesterenko V F, Meyers M A, Wright T W. Shear Localization and Recrystallization in High-Strain, High-Strain-Rate Deformation of Tantalum [J]. Materials Science & Engineering A: Structural Materials: Properties, Microstructure and Processing, 1997, A229: 23-41.
[2]
Meyers M A, Nesterenko V F. High-Strain, High-Strain-Rate Deformation of Tantalum [J]. Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 1995, 26A: 2493-2501.
[3]
Tang T G, Hu H B, Wang D S, et al. Shear Fracture of HR-2 Steel Tube under Shock Loading [J]. Chinese Journal of High Pressure Physics, 2002, 16(1): 75-79. (in Chinese)
Li X M. An Investigation on the Deformation, Damage and Spall of Cylindrical Steel Tube Loaded by Sliding-Implosion [D]. Hefei: University of Science and Technology of China, 2003. (in Chinese)
[6]
李雪梅. 内爆加载下钢圆管的变形、损伤及层裂研究 [D]. 合肥: 中国科学技术大学, 2003.
[7]
Li Y C, Li D H, Wei Z G, et al. Research on the Deformation, Damage and Fracture Rules of Circular Tubes under Inside-Explosive Loading [J]. Acta Mechanica Sinica, 1999, 31(4): 442-449. (in Chinese)