Si-B-C陶瓷涂敷2DC/SiC复合材料的抗氧化性能

, PP. 100-106

Keywords: C/SiC,Si-B-C陶瓷,涂层,氧化,形貌,自愈合

Full-Text   Cite this paper   Add to My Lib

Abstract:

利用化学气相沉积(CVD)法制备了Si-B-C陶瓷涂敷改性的2DC/SiC复合材料,研究了其在700~1200℃氧化10h性能和结构的演变规律以及自愈合机制,同时获得了Si-B-C涂层在不同温度氧化后的形貌、组分和物相转变规律。结果表明:涂敷在复合材料表面的Si-B-C陶瓷随温度的升高氧化加快,但氧化程度较低,不深于7μm;随温度的升高,氧化形成的硅硼玻璃黏度降低,挥发增强;当温度达到1200℃时,硅硼玻璃析出SiO2晶体;Si-B-C陶瓷涂敷改性的C/SiC具有优良的抗氧化性能,随氧化温度的升高,复合材料失重率增加,但在1200℃氧化10h后失重率仅为0.47%;此外材料在1000℃氧化后的强度保持率最高,达到91.6%,Si-B-C陶瓷氧化形成的硅硼玻璃可以有效封填裂纹,这是材料具有优良抗氧化性能的主要机制。

References

[1]  张立同, 成来飞. 连续纤维增韧陶瓷基复合材料可持续发展战略探讨 [J]. 复合材料学报, 2007, 24(2): 1-6.
[2]  Zhang Litong, Cheng Laifei. Discussion on strategies of sustainable development of continuous fiber reinforced ceramic matrix composites [J]. Acta Materiae Compositae Sinica, 2007, 24(2): 1-6.
[3]  Naslain R. Design, preparation and properties of non-oxidation CMCs for application in engines and nuclear reactors: An overview [J]. Composites Science and Technology, 2004, 62(2): 155-170.
[4]  Viricelle J P, Goursat P, Bahloul-Hourlier D. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiCBC)m [J]. Composites Science and Technology, 2001, 61(4): 607-614.
[5]  Xu Y D, Zhang L T, Cheng L F, et al. Microstructure and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration [J]. Carbon, 1998, 36(7/8): 1051-1056.
[6]  Yin X W, Cheng L F, Zhang L T, et al. Microstructure and oxidation resistance of carbon/silicon carbide composites infiltrated with chromium silicide [J]. Materials Science and Engineering A, 2000, 290(1/2):89-94.
[7]  曹 素, 刘永胜, 左新章, 等. 涂敷含硼硅玻璃SiC涂层的C/SiC复合材料空气氧化行为 [J]. 复合材料学报, 2011, 28(2): 142-148.
[8]  Cao Su, Liu Yongsheng, Zuo Xinzhang, et al. Oxidation behaviors of C/SiC composites coated with SiC coatings containing borosilicate glass [J]. Acta Materiae Compositae Sinica, 2011, 28(2): 142-148.
[9]  Cheng L F, Xu Y D, Zhang L T, et al. Effect of glass sealing on the oxidation behavior of three dimensional C/SiC composites in air [J]. Carbon, 2001, 39(8): 1127-1133.
[10]  Liu Y S, Cheng L F, Zhang L T, et al. Oxidation protection of multilayer CVD SiC/B/SiC coatings for 3D C/SiC composite [J]. Materials Science and Engineering A, 2007, 466(1/2): 172-177.
[11]  Wu S J, Cheng L F, Yang W B, et al. Oxidation protective multilayer CVD SiC coatings modified by a graphitic B-C interlayer for 3D C/SiC composite [J]. Applied Composite Materials, 2006, 13(6): 397-406.
[12]  Goujard S, Vandenbulcke L, Tawil H. The oxidation behaviour of two-and three-dimensional C/SiC thermostructurai materials protected by chemical-vapour-deposition polylayers coatings [J]. J Mater Sci, 1994, 29:6212-6220.
[13]  Goujard S, Vandenbulcke L. Oxidation tests of carbonaceous composite materials protected by Si-B-C CVD coatings [J]. Thin Solid Films, 1994, 245(1/2): 86-97.
[14]  Goujard S, Vandenbulcke L, Tawil H. Oxidation behavior of 2D and 3D carbon/carbon thermostructural materials protected by CVD polylayer coatings [J]. Thin Solid Films, 1994, 252(2): 120-130.
[15]  Rizzo H F. Oxidation of boron at temperatures between 400℃ and 1300℃ in air [C]//Proceedings of conference on Boron. New York: Plenum Press, 1960: 175-189.
[16]  Naslain R. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors [J]. Composites Science and Technology, 2004, 64(2): 155-170.
[17]  Liu Y S, Zhang L T, Cheng L F, et al. Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites [J]. Corrosion Science, 2009, 51(4): 820-826.
[18]  Yang W B, Zhang L T, Cheng L F, et al. Oxidation behavior of C/SiC composite with CVD SiC-B4C coating in a wet oxygen environment [J]. Appl Compos Mater, 2009, 16(2): 83-92.
[19]  Li S W, Feng Z D, Liu Y S, et al. Microstructural evolution of coating-modified 3D C/SiC composites after annealing in wet oxygen at different temperatures [J]. Corrosion Science, 2010, 52(9): 2837-2845.
[20]  Zuo X Z, Zhang L T, Liu Y S, et al. Effect of deposition temperature on dynamics and mechanism of deposition for Si-B-C ceramic from BCl3/SiCH3Cl3/H2 precursor [J]. J Mater Sci Technol, 2012, 28(9): 793-798.
[21]  张伟华, 成来飞, 张立同, 等. C/SiC复合材料表Si-C-B自愈合涂层的制备与抗氧化行为 [J]. 无机材料学报, 2008, 23(4): 774-778.
[22]  Zhang Weihua, Cheng Laifei, Zhang Litong, et al. Preparation and anti-oxidation behavior of Si-C-B self-healing coating on C/SiC composite [J]. Journal of Inorganic Materials, 2008, 23(4): 774-778.
[23]  成来飞. 1650℃长寿命碳/碳复合材料防氧化涂层研究 [D]. 西安: 西北工业大学, 1997: 99.
[24]  Cheng Laifei. Investigation of long life for anti-oxidation coating of carbon/carbon composites at 1650℃ [D]. Xi’an: Northwestern Polytechnical University, 1997: 99.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133