Mechanical activation and electrolysis of gold from goldsmith's wasteKeywords: waste , gold , mechanical activation , leaching , electrolysis Abstract: The intensification of the thiourea leaching of gold from goldsmith's waste (Ko ice, Slovakia) using mechanical activationas the pretreatment step. The leaching of “as-received“ sample in an acid thiourea solution resulted in 77 % Au dissolution, aftermechanical activation 98 % of the gold was leached during 120 min. The activation was performed in an attritor using variable millingtimes. The physico-chemical changes in the waste as a consequence of mechanical activation had a pronounced influenceon the subsequent gold extraction. Maximum recovery of gold was reached behind 60 minutes at optimum conditions of electrolysis.
|