Effect of Ultrasonic Wave on Leaching Manganese-containing Silver Orewith the Binary Ore Leaching Process
细粒嵌布锰银矿浸取中的超声强化作用

Keywords: manganese,silver ore,leaching,ultrasonic wave
锰银矿
,浸出,超声波,细粒嵌布

Full-Text   Cite this paper   Add to My Lib

Abstract:

The two-step leaching technique was used to extract silver from manganese-containing silver ore. In the first step the ore was leached with a binary ore process to resolve manganese oxide and expose the fresh silver ore, using pyrite as reductant. The manganese leaching reached 98% and the leaching conditions are: leaching temperature 95oC, leaching time 5 h, pyrite: manganese ore=0.28. When the ultrasonic wave at the rate of 40 kHz is applied to the reaction system, the leaching time can be reduced by 50% and the pyrite consumption amount is decreased by nearly 20%. Then, the leaching residue was treated to extract silver and the recovery was 95%.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133