材料科学技术学报 2004
Preparation and ASE Spectrum of a Single-Mode Erbium Doped Tellurite Glass Fiber with D-type Cladding GeometryKeywords: Preparation,ASE spectrum,Er3,Tellurite glass fiber Abstract: Based on the host of tellurite glasses, the glass formation, preform manufacture, and fiber fabrication are described. The characterization of amplified spontaneous emission (ASE) from this newly fabricated single-mode Er3 -dopedtellurite fibers is also presented. When pumped at 980 nm, a very broad erbium ASE around 1.53μm was observed. The variations of ASE with fiber length and pumping power are measured and discussed. The output of 2 mW from Er3 -doped tellurite fiber ASE source was obtained under the pump power of 660 mW.
|