材料工程  2010 

采用BNi68CrWB钎料钎焊GH783的接头组织与性能

Keywords: 镍基高温合金,GH783,钎焊,接头,力学性能

Full-Text   Cite this paper   Add to My Lib

Abstract:

选用BNi68CrWB钎料,对低膨胀高温合金GH783的钎焊工艺及接头组织性能进行研究。研究表明,采取BNi68CrWB钎料、钎焊规范为1180℃/10min,钎焊试样焊后进行完全热处理,获得钎焊接头室温拉伸强度最高达到701MPa,接头650℃拉伸强度最高达到了696MPa;钎焊接头的组织由镍-钴基γ固溶体、共晶及其他脆性化合物相构成;钎焊间隙不同,接头中固溶体所占比例不同,0.05mm间隙中元素扩散较充分,接头以固溶体为主,共晶及其他脆性化合物相较少。钎焊间隙对接头性能影响较大,0.05mm钎焊间隙的接头强度明显高于0.1mm间隙接头。

References

[1]  贾新云,赵宇新.长期时效对低膨胀高温合金GH783组织与性能的影响[J].航空材料学报,2006,26(4):14-17.
[2]  贾新云,赵宇新,张绍维.热处理对GH783合金组织与性能的影响[J].材料工程,2006,(增刊1):165-171.
[3]  WU X W,CHANDEL R S.Induction brazing of Inconel 718 to Inconel X-750 using Ni-Cr-Si-B amorphous foil[J].Journal of Materials Processing Technology,2000,104(1):34-43.
[4]  李文.DD98镍基单晶高温合金的瞬态液相连接[D].中国科学院金属研究所博士论文.2002.
[5]  LI X H,MAO W,CHENG Y Y.Microstructures and properties of transient liquid phase diffusion bonded joints of Ni3Al-base superalloy[J].Transactions of Nonferrous Metals Society of China,2001,11(3):405-408.
[6]  郑运荣,张德堂.高温合金与钢的彩色金相研究[M].北京:国防工业出版社,1999.
[7]  HECK K A,SMITH D F,HOLDERBY M A,et al.Three phase controlled expansion superalloys with oxidation resistance[A].Superalloys 1992[C].PA:The Seven Springs International Symposium Committee,1992.217-226.
[8]  SMITH J S,HECK K A.Development of a low thermal expansion,crack growth resistant superalloy[A].Superalloys 1996[C].PA:The Seven Springs International Symposium Committee,1996.91-100.
[9]  HECK K A,SMITH J S,SMITH R.Inconel alloy 783:an oxidation-resistant,low expansion superalloy for gas turbine applications[J].Journal of Engineering for Gas Turbines and Power,1998,120(2):363-369.
[10]  MA L Z,CHANG K M,MANNAN S K,et al.Effects of NiAl-βprecipitates on fatigue crack propagation of Inconelalloy 783 under time-dependent condition with vallous load ratios[J].Scripta materialia,2003,48(5):551-557.
[11]  MA L Z,CHANG K M.Identification of SAGBO-induced damage zone ahead of crack tip to characterize sustained loading crack growth in alloy 783[J].Scripta materialia,2003,48(5):1271-1276.
[12]  MA L Z,CHANG K M,MANNAN S K.Effect of thermomechaincal processing on fatigue crack propagation in inconel alloy 783[A].SUPERALLOYS 2000[C].PA:The Seven Springs International Symposium Committee,2000.601-608.
[13]  郭绍庆,李晓红,毛唯,等.低膨胀高温合金焊接性的研究现状[J].宇航材料工艺,2000,(6):5-9.
[14]  邓继雄,潘辉,魏祚伟.低膨胀高温合金(GH907)钎焊接头力学性能研究[A].第九次全国焊接会议论文集[C].北京:中国机械工程学会焊接学会,1999.147-151.
[15]  毛唯,李晓红,叶雷.定向凝固Ni3Al基高温合金IC6A的真空钎焊[J].航空材料学报,2006,26(3):103-106.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133