材料工程  2014 

304不锈钢与Sn作用后腐蚀性能评价

DOI: 10.3969/j.issn.1001-4381.2014.03.007, PP. 41-45

Keywords: 低熔点金属Sn,不锈钢,电化学腐蚀

Full-Text   Cite this paper   Add to My Lib

Abstract:

通过动电位极化和恒电流恒电位极化测试研究了低熔点金属Sn对304不锈钢腐蚀性能的影响,并采用扫描电子显微镜观察样品的腐蚀形貌。动电位极化的实验结果表明黏附于304不锈钢表面的Sn加速了基体点蚀的形成,并且Sn的量越多点蚀越严重。不同时间的恒电位极化也说明在相同实验条件下Sn存在的304不锈钢,腐蚀坑多且深。恒电流极化测试表明Sn降低304不锈钢的腐蚀性能,源于电极电位较低的Sn容易点蚀,使腐蚀坑内酸性升高最终导致钢的破坏。

References

[1]  GARCIA-MAZARIO M, LANCHA A M, HERNANDEZ M, et al. Effect of lead on Inconel 600 and Incoloy 800 oxide layers formed in simulated steam generator secondary environments[J]. Nuclear Engineering and Design, 1996, 167 (2): 155-167.
[2]  LAURILA T, VUORINEN V, KIVILAHTI J K. Interfacial reactions between lead-free solders and common base materials[J]. Materials Science and Engineering: R: Reports, 2005, 49 (1-2): 1-60.
[3]  HUANG Y C, CHEN S W, GIERLOTKA W, et al. Dissolution and interfacial reactions of Fe in molten Sn-Cu and Sn-Pb solders[J]. Journal of Materials Research, 2007, 22 (10): 2924-2929.
[4]  赵艳, 程从前, 曹志远, 等. 钝化状态对Sn与304不锈钢交互作用的影响[J]. 稀有金属材料与工程, 2012, 41 (S2): 808-812.ZHAO Yan, CHENG Cong-qian, CAO Zhi-yuan, et al. The effect of passivity on the interaction between Sn and 304 type stainless steel[J]. Rare Materials and Engineering, 2012, 41 (Suppl2): 808-812.
[5]  LUO J, CHENG H, ASL K M, et al. The role of a bilayer interfacial phase on liquid metal embrittlement[J]. Science, 2011, 333 (6050): 1730-1735.
[6]  AUGER T, HAMOUCHE Z, MEDINA-ALMAZAN L, et al. Liquid metal embrittlement of T91 and 316L steels by heavy liquid metals: A fracture mechanics assessment[J]. Journal of Nuclear Materials, 2008, 377 (1): 253-260.
[7]  胡强, 黄安国, 李忠锁. 无铅钎料对不锈钢的腐蚀性研究[J].电子工业专用设备, 2005, 120 (1): 53-57.HU Qiang, HUANG An-guo, LI Zhong-suo. Stainless steel corrosion study for lead-free solder[J]. Equipment Electronic Products Manufacturing, 2005, 120 (1): 53-57.
[8]  ZHONG P, YAN H. A case study of Bi-Sn induced embrittlement[J]. Engineering Failure Analysis, 1996, 3 (4): 241-248.
[9]  韩恩厚, 王俭秋, 吴欣强, 等. 核电高温高压水中不锈钢和镍基合金的腐蚀机制[J].金属学报, 2010, 46 (11): 1379-1391.HAN En-hou, WANG Jian-qiu, WU Xin-qiang, et al. Corrosion mechanisms of stainless steel and nickel base alloys in high temperature high pressure water[J]. Acta Metallurgica Sinica, 2010, 46 (11): 1379-1391.
[10]  王永强, 李时磊, 杨滨, 等. 核电站一回路主管道铸造奥氏体不锈钢热老化研究现状与展望[J]. 材料导报, 2012, 26 (3): 101-105. WANG Yong-qiang, LI Shi-lei, YANG Bin, et al. Research status and outlook on thermal aging of cast austenitic stainless steels used in primary coolant pipes of nuclear power plant[J]. Materials Review, 2012, 26 (3): 101-105.
[11]  CLEGG R E, JONES D R H. Liquid metal embrittlement of tensile specimens of En19 steel by tin[J]. Engineering Failure Analysis, 2003, 10 (1): 119-130.
[12]  美国机械工程师学会. ASME核电规范与标准NQA-1, 核设施质量保证要求[S].上海核工程研究设计院译, 2004. 43.
[13]  French Association for Design. Construction and In-service Inspection Rules for Nuclear Island Components, RCC-M Design and construction rules for mechanical components of PWR nuclear island[S]. SectionⅤ-Fabrication, Pairs: AFCEN, 2000. 1.
[14]  DARWISH S M, AL-HABDAN S, AL-TAMIMI A. A knowledge-base for electronics soldering[J]. Journal of Materials Processing Technology, 2000, 97 (1-3): 1-9.
[15]  CHENG C Q, YANG F, ZHAO J, et al. Leaching of heavy metal elements in solder alloys[J]. Corrosion Science, 2011, 53 (5): 1738-1747.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133