SiC复相陶瓷内加热器套管的抗热震及抗氧化性能

DOI: 10.7521/j.issn.0454-5648.2014.06.02

Full-Text   Cite this paper   Add to My Lib

Abstract:

模拟内加热器服役环境,将具有复层结构的碳化硅(SiC)复相陶瓷内加热器套管置于金属铝液中,测试套管各部位材料的抗热震及抗氧化性能。通过X射线衍射和扫描电子显微镜研究材料成分和显微结构的变化,分析确定导致内加热器整体失效的原因及部位。结果表明SiC复相陶瓷套管内管材料在长效氧化条件下残余强度依然达到270MPa以上,不会导致套管整体失效;外管材料在氧化和热震双重作用下,液面至液面下100mm处的孔隙率明显增加,残余强度显著降低,这是导致内加热器整体失效的主要原因

References

[1]   耿刚强, 官磊, 李宁, 等. 铁硅金属间化合物耐熔铝腐蚀性研究[J]. 热加工工艺, 2006, 35(12): 14-16.
[2]  GENG Gangqiang, GUAN Lei, LI Ning, et. al. Hot Working Technol (in Chinese), 2006, 35(12): 14-16.
[3]   YANG W, SHI Z, LI H, et. al. Improvement of strength and oxidation resistance for SiC/graphite composites by SiC coating [J]. IOP Conf Series: Mater Sci Eng, 2011, 18(2): 1-4.
[4]   YANG W, SHI Z, JIN Z, et. al. Effects of impregnating and heat treatment on the oxidation and thermal shock properties of pressureless sintered SiC/graphite composites [J]. Mater Sci Forum, 2012, 724: 311-314.
[5]   史忠旗, 金志浩, 乔冠军. 可加工陶瓷的弱界面结构与性能优化研究进展[J]. 硅酸盐学报, 2007, 35(S1): 131-136.
[6]  SHI Zhongqi, JIN Zhihao, QIAO Guanjun. J Chin Ceram Soc, 2007, 35(S1): 131-136.
[7]  
[8]   杨万利,史忠旗,金志浩,等.SiC复相陶瓷内加热器套管的制备及性能[J].硅酸盐学报,2012, 40(3): 362-365.
[9]  YANG Wanli, SHI Zhongqi, JIN Zhihao, et. al. J Chin Ceram Soc, 2012, 40(3): 362-365.
[10]   陈冬.中国热镀锌行业现状与前景[J].河北冶金,2002(5): 7-10.
[11]  CHEN Dong. Hebei Metal(in Chinese), 2002(5): 7-10.
[12]   JOHNSTON M W, LITTLE J A. Degradation of oxidized SiC-Si3N4 in molten aluminum [J]. J Mater Sci, 1990, 25: 5284-5290.
[13]   高扩农,李守荣.抗液态锌腐蚀材料综述[J].金属制品,2001, 27(3): 50-52.
[14]  GAO Kuonong, LI Sourong. Metal Prod J (in Chinese), 2001, 27(3): 50-52.
[15]   PAWLIK T, SOPICKA-LIZER M, Mikuskiewicz M, et al. Corrosion resistance of alumina-SiAlON refractories for application in aluminium industry [J]. Adv Mater Forum, 2010, 636/637: 142-148.
[16]   JONES M I, ETZION R, DESMAISON J, et. al. Corrosion behavior of reaction bonded Si3N4-SiC and SiAlON-SiC composites in simulated aluminum smelting conditions [J]. J Ceram Soc Jpn, 2008, 116(1354): 712-716.
[17]   ROULET F, TRISTANT P, DESMAISON J, et. al. Corrosion behavior of aluminum nitride in liquid aluminium: influence of the microstructure [J]. J Eur Ceram Soc, 1997, 17(15/16): 1877-1883.
[18]  MOURADOFF L, LACHAUDURAND A, DESMAISON J, et. al. Study of the interaction between liquid aluminum and silicon-nitride [J]. J Eur Ceram Soc, 1994, 13(4): 323-328.
[19]   JOHNSTON M W, LITTLE J A. Oxidation and liquid aluminum degradation of a nitride-bonded silicon-carbide ceramic [J]. Corros Sci, 1993, 35(5/8): 931-938.
[20]   CHEN Hukui, LIU Jianrui, HUANG Weidong. Corrosion behavior of silicon nitride bonding silicon carbide in molten magnesium and AZ91 magnesium alloy [J]. Mater Sci Eng A, 2006, 415 (1/2): 291-296.
[21]   SIDHU M S, KRAL M V. Erosion of ferrous alloys by liquid aluminum [C]//Techical Session on Light Metals, Seattle, America, 2010: 325-330.

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133