EE Tal-Gutelmacher,D Eliezer,D Eylon.The effects of low fu-gacity hydrogen in duplex-and beta-annealed Ti-6Al-4V alloy[J].Materials Science and Engineering,2004,381:230.
[3]
CC F Clarke,D Hardie,B M Ikeda.Hydrogen-induced crackingof commercial purity titanium[J].Corrosion Science,1997,39(9):1545.
[4]
CC L Briant,Z F Wang,N Chollocoop.Hydrogen embrittlementof commercial purity titanium[J].Corrosion Science.2002,44(8):1875.
[5]
TTae Kyu Kim,Jong-Hyuk Baek,Byung-Seon,et al.Character-istics of hydriding and hydrogen embrittlement of the Ti-Al-Zralloy[J].Annals of Nuclear Energy,2002,29(17):2041.
[6]
DD F Teter,I M Robertson,H K Birnbaum,The effects of hy-drogen on the deformation and fracture of-βtitanium[J].ActaMaterial,2001,49(20):4313.
[7]
K R Morash,D F Bahr,The effects of hydrogen on deforma-tion and cross slip in BCC titanium alloy[J].Scripta Material,2001,45(7):839.
Menno Blaauw.Hydrogen precipitation in titanium observedwith neutron incoherent scattering and prompt gamma neutronactivation analysis[J].Nuclear Instruments and Methods inPhysics Research A,2003,505,20.
[10]
Matthew R Gibbons,Wade J Richards,Kevin Shields.Opti-mization of neutron tomography for rapid hydrogen concentra-tion inspection of metal castings[J].Nuclear Instruments andMethods in Physics Research Section A,1999,424:53.
[11]
Masakazu Yoshioka,Akira Ueno,Hidehiro Kishimoto.Analy-sis of hydrogen behaviour in crack growth tests of-γTiAl bymeans of the hydrogen microprint technique[J].Inter-metallics,2004,12(1):23.
Takumi Haruna,Toshio Shibata,Taku Iwata.Potential-pH re-gion for environment-assisted cracking of gamma titanium alu-minide[J].Intermetallics,2000,8:92.
[14]
A K Roya,M K Spraggeb,D L Flemingb et al.Cracking of ti-tanium alloys under cathodic applied potential.Micron,2001,32(2):211.
[15]
D Hardie,S Ouyang.Effect of hydrogen and strain rate uponthe ductility of mill-annealed Ti5Al4V[J].Corrosion Science,1999,41(1):155.
[16]
Peterson,Kenneth Allen.Electron channelling studies of hy-drogen embrittlement and cleavage fractures in BCC metals(titanium,molybdenum,iron,silicon)[D].University of min-nesota,PhD,,DAI-B,1984 44/09,2860.
[17]
NN E Paton,J C William.Effect of hydrogen on titanium and itsalloys.Hydrogen in metals[M].Oxford:Pergamon Press,1974.49.
Toshio Ogawaa,Ken’ichi Yokoyamab,Kenzo Asaoka,et al.Hydrogen absorption behavior of beta titanium alloy in acidfluoride solutions[J].Biomaterials,2004,25:2419.
[22]
Kenichi Yokoyamaa,Toshio Ogawa,Kenzo Asaoka,et al.Hy-drogen absorption of titanium in acidic fluoride solutions[J].Materials Science and Engineering A,2004,384:19.
[23]
Kazuyuki Kanekoa,Ken ichi Y,Keiji Moriyama,et al.Delayedfracture of beta titanium orthodontic wire in fluoride aqueoussolutions[J].Biomaterials,2003,24(12):2113.
[24]
Hollis A C,Scully J C.Stress corrosion cracking and hydrogenembrittlement of titanium in methanol-hydrochloric acid solu-tions[J].Corrosion Science,1993,34(5):821.
[25]
Hollis A C,Scully J C.Stress corrosion cracking and hydrogenembrittlement of titanium in methanol-iodine solutions[J].Corrosion Science,1993,34(5):837.
[26]
Brass A M,Chene J.Hydrogen absorption inα/βtitanium alu-minides during mechanical grinding[J].Scripta Materialia,1998,39(11):1569.
[27]
L C Covington.The influence of surface condition and environ-ment on the hydriding of titanium[J].Corrosion,1979,35(8):378.
[28]
余存烨.石化钛设备腐蚀氢脆检测与安全评定[J].石油化工腐蚀与防,1996,13(1):20.
[29]
Y Hirohata,D Motojima,T Hinoa,et.al.Suppression of hy-drogen absorption to V-4Cr-4Ti alloy by TiO2/TiC coating[J].Journal of Nuclear Materials,2003,313-316:172.
S K Yen.Retardation effects of thermally grown oxide filmson the hydrogen embrittlement of commercial pure titanium[J].Corrosion Science,1999,41(10):2031.
Manor E,Eliezer D.Hydrogen effects in titanium-aluminide al-loy stabilized by Nb,V,and Mo[J].Scripta Metallurgical&Materialia,1990,24(1):129.
[35]
Anand Durairajan.Synthesis and characterization of novel coat-ings for corrosion protection and hydrogen embrittlement inhi-bition[D].PhD,University of South Carolina,2001.
[36]
Lee S C,Ho W Y,Chen T M.Prevention of hydrogen degra-dation in titanium by deposition of TiN thin film[J].Journal ofMaterials Engineering and Performance,1994,3(6):740.
[37]
Lee S C,Ho W Y,Huang C C,et al.Hydrogen embrittlementand fracture toughness of a titanium alloy with surface modifi-cation by hard coatings[J].Journal of Materials Engineeringand Performance,1996,5(1):64.
[38]
Fu Y Yan,B Loh,N L,et al.Hydrogen embrittlement of tita-nium during microwave plasma assisted CVD diamond deposi-tion[J].Surface Engineering,2000,16(4):349.
[39]
Lee C T,Loutfy R O,Withers J C.Ceramic coatings for pro-tecting titanium alloys in high temperature hydrogen environ-ment[J].Ceramic Engineering and Science Proceedings,1995,16(5):1029.