Kolotyrkin Y M.Effects of anions on the dissolution kinetics of metals[J].Electrochem J.Corrosion Science,1961,108(3):209.[30]Dawson J L,Ferreira M G S.Electrochemical studies of the pitting of austenitic stainless steel[J].Corrosion Science,1986,26(12):1009.
[2]
Sedriks A J.Corrosion of Stainless Steels[M].New York: John Wiley and Sons,1979.64.
Kain R M,Phull B S,Pikul S J.1940′ til now-long term marine atmospheric corrosion resistance of stainless steel and other nickel containing alloys[A].Townsent H E,Outdoor atmospheric corrosion[C].ASTM STP 1421.Philadelphia:American Society for Testing and Materials,2002.343.
[5]
Wallinder D,Wallinder I O,Leygraf C.Influence of surface treatment of type 304 L stainless steel on atmospheric corrosion resistance in urban and marine environments[J].Corrosion,2003,59(3):220.
Lekie H P,Uhlig H H.Environmental factors affecting the critical potential for pitting in 18.8 stainless steel[J].Journal of The Electrochemical Society,1966,113(12):1262.
[8]
Hong T,Nagumo M.The effect of SO2-4 concentration in NaCl solution on the early stages of pitting corrosion of type 430 stainless steel[J].Corrosion Science,1997,39(5):961.
[9]
Pistorius P C,Burstein G T.Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate[J].Corrosion Science,1992,33(12):188
[10]
SSedriks A J.Corrosion of Stainless Steels[M].New York: John Wiley and Sons,1979.1.
[11]
徐徐增华.金属耐蚀材料,第六讲:奥氏体不锈钢[J].腐蚀与防护,2001,22(6):275.
[12]
AAsami K,Hashimoto K.Importance of initial surface film in the degradation of stainless steels by atmospheric exposure[J].Corros Sion.Science,2003,45(10):2263.〖CM2*4-3〗[4]崔忠圻.金属学与热处理[M].北京:机械工业出版社,2000.372.
[13]
DDegerbeck J,Karlsson A,Berglund G.Atmospheric corrosion of stainless steel of type 18Cr2MoTi[J].British Corrosion Journal,1979,14(4):220.
[14]
KKain R M,Wollenberg P.Atmospheric corrosion and weathering behavior of ternecoated stainless steel roofing[A].Townsent H E.Outdoor atmospheric corrosion[C].ASTM STP 1421.Philadelphia:American Society for Testing and Materials,2002.316.
[15]
LLaque F L,Copson H R.Corrosion Resistance of Metals and Alloys[M].2nd edition.New York:Reinhold Publishing Corp.,1963.410.
[16]
UUhlig H H.Effect of metal composition and structure on corrosion and oxidation[J].Corrosion,1963,19(7):231t.
[17]
OOsozawa K,Engell H J.The anodic polarization curves of iron-nickelchromium alloys[J].Corrosion.Science,1966,6(8):389.[10]张德康.不锈钢局部腐蚀[M].北京:科学出版社,1982.1.
[18]
Malik A U,Mayan Kutty P C,Siddiqi N A,et al.The influence of pH and chloride concentration on the corrosion behaviour of AISI 316L steel in aqueous solutions[J].Corrosion.Science,1992,33(11):1809.
[19]
Muto I,Sato E,Ito S.New electrochemical method to evaluate atmospheric corrosion resistance of stainless steels[A].Cragnolino G,Sridhar N.Application of accelerated corrosion tests to service life prediction of materials[C].ASTM STP 1194.Philadelphia:American Society for Testing and Materials,1994.382.
[20]
Klassen R D,Roberge P R,Lenard D R,et al.Corrosivity patterns near sources of salt aerosols[A].Townsent H E.Outdoor atmospheric corrosion[C].ASTM STP 1421.Philadelphia:American Society for Testing and Materials,2002.19.
[21]
Kolotyrkin Y M.Pitting corrosion of metals[J].Corrosion,1963,19(8):261t.
[22]
Schwenk W.Theory of stainless steel pitting[J].Corrosion,1964,20(4):129t.
[23]
Liang C F,Hou W T.Twelve year atmospheric exposure of stainless steels in China[A].Townsent H E.Outdoor atmospheric corrosion[C].ASTM STP 1421.Philadelphia:American Society for Testing and Materials,2002.358.
[24]
Tochihara M.Atmospheric corrosion of stainless steels used for the eaves of buildings[J].Materials.Performance,1996,35(12):58.
[25]
Tsutsumi Y,Nishikata A,Tsuru T.Initial stage of pitting corrosion of type 304 stainless steel under thin electrolyte layers containing chloride[J].Journal of The Electrochemical Society.,2005,152(9):B358.
[26]
Tsutsumi Y,Nishikata A,Tsuru T.Pitting corrosion mechanism of type 304 stainless steel under a droplet of chloride solutions[J].Corrosion Science,2007,49(3):1394.
[27]
Wang J H,Su C C,SzklarskaSmialowska Z.Effects of Cl- concentration and temperature on pitting of AISI 304 stainless steel[J].Corrosion,1988,44(10):732.
[28]
刘永辉,张佩芬.金属腐蚀学原理[M].北京:航空工业出版社,1993.103.
[29]
Cruz R P V,Nishikata A,Tsuru T.Pitting corrosion mechanism of stainless steels under wetdry exposure in chloridecontaining environments[J].Corrosion Science,1998,40(1):125.
Williams D E,Westcott C,Fleischmann M.Stochastic models of pitting corrosion of stainless steels[J].Journal of The Electrochemical Society,1985,132(8):1804.
[32]
Khatak H S,Raj Baldev.Corrosion of Austenitic Stainless Steels:Mechanism,Mitigation and Monitoring[M].New Delhi:Narosa publishing house,2002.74.
[33]
Lin L F,Chao C Y,Macdonald D D.A point defect model for anodic passive films[J].Electrochem J.Corrosion Science,1981,128(6):1194.
[34]
Sato N.A theory for breakdown of anodic oxide films on metals[J].Electrochimica Acta,1971,16(10):1683.[28]SzklarskaSmialowsk Z.Review of literature on pitting corrosion published since 1960[J].Corrosion,1971,27(6):223.